| 一种Monte Carlo仿真新算法及其对三维个体晶粒长大速率拓扑依赖?… |
| 刘国权 宋晓艳 |
| 北京科技大学材料科学与工程系;北京 100083 |
|
引用本文:
刘国权; 宋晓艳 . 一种Monte Carlo仿真新算法及其对三维个体晶粒长大速率拓扑依赖?…[J]. 金属学报, 1999, 35(3): 245-248 .
[1] Anderson M P, Grest G S, Srolovitz D J. Philo Mag, 1989:59B: 293 [2] Atkinson H V. Acta Metall, 1988; 36: 469 [3] Yu H B, Liu G Q. Sci Bull, 1996; 41: 2000(于海波,刘国权、科学通报,1996;41:2000) [4] Fortes M A. Scr Mater, 1997; 37: 679 [5] Song X Y, Liu G Q, He Y Z. Prog Nat Sci, 1998; 8: 92 [6] Song X Y, Liu G Q. Scr Mater, 1998; 38: 1691 [7] Zhang X Z. Application of Monte Cacao Method in StatisticsPhysics. Zhengzhou: Henan Sci & Technol Press, 1991: 62(张孝泽.蒙特卡罗方法在统计物理中的应用.郑州:河南科学技术出版社, 1991: 62) [8] Smith C S. Met Rev, 1964; 9(33): 1-48 [9] Liu Guoquan. J Univ Sci Beijing, 1987; 9: 29(刘国权.北京科技大学学报,1987;9:29) [10] Hull F C. Mater Sci Technol, 1988; 4: 778 [11] Rhines F N, Craig K R. Metall Trans, 1974; 5: 417 [12] Liu G Q, Yu H B, Li W Q. Acta Stereologica, 1994, 13: 281 [13] Kurzydlowski K J, Ralph B. The Quantitative Description ofthe Microstructure of Materials. London: CRC Press, 1995:107, 256, 294 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|