| Zr替代稀土对RE(NiCoMnTi)5贮氢合金相结构和性能的影响 |
| 任可 雷永泉 |
| 浙江大学材料科学与工程系; 杭州 310027 |
|
引用本文:
任可; 雷永泉 . Zr替代稀土对RE(NiCoMnTi)5贮氢合金相结构和性能的影响[J]. 金属学报, 2000, 36(8): 854-858 .
[1] Lei Y Q, Li Z P, Chen C P, Wu J, Wang Q D. J LessCommon Met, 1991; 172: 1265 [2] Jiang J J, Lei Y Q, Sun D L. Rare Met Mater Eng, 1993;22: 68(江建军,雷永泉,孙大林.稀有金属材料与工程,1993;22:68) [3] Chen L X. Rare Met Mater Eng, 1999; 28: 302(陈立新.稀有金属材料与工程,1999;28:302) [4]Sakai T, Miyamura H, Oguro K, Kato A, Kuriyama H,Ishikawa H. Denki Kagaku, 1989; 57: 612 [5] Sakai T, Miyamura H, Kuriyama N, Kato A, Oguro K,Ishikawa H. J Electrochem Soc, 1990; 37: 795 [6] Gachon J C, Dirand M, Hertz H. i Less-Common Met,1983; 92: 307 [7] Buschow K H J, Mal H H Van. J Less-Common Met,1972; 29: 203 [8] Mishima R. J Alloys Comp, 1993; 192: 176` |
|