| 热塑性变形条件下钢内部裂纹愈合的实验研究 |
| 韦东滨 韩静涛 |
| 北京科技大学材料科学与工程学院; 北京 100083 |
|
引用本文:
韦东滨; 韩静涛 . 热塑性变形条件下钢内部裂纹愈合的实验研究[J]. 金属学报, 2000, 36(6): 622-625 .
[1] Giffith A A Phil Trans Roy Soc,19202 221A 163 [2] Shapiro E Dieter G E Metal Trans, 1970;1: 1711 [3] Cao Q X Han J T, Ma Q X Zheng T Xie Y X, Li F L.J Plasticity Eng,1994;1:14(曹起襄,韩静涛,马庆贤,郑涛,谢云蛐,李福利塑性工程学报,1994;1:14) [4] Wang Z X.Physical Metallurgy.Beliing:MetallurgicalIndustry Press, 1991: 143(王占学,塑性加工金属学北京:冶金工业出版社,1991:143) [5] Zhao Z Y. Plastic Deformation of Metals and Rolling Theory.Bening:Metallurgical Industry Press.1991:124(赵志业 金属塑性变形与轧制理论 北京:冶金工业出版社,1991:124) [6] Kymanin V Y, Kawaliajowa L A Kakaolaowa M P Metalland Thermo-Mech Treat Met,1995;4:7 [7] An J Z Heat Treat Met Abroad 1996: 17 2(安敬竹 国外金属热处理,19962 17:2) [8] Han J T, Zhao G, Cao Q X、 Set Chin, 1997: 27E 23(韩静涛,赵钢,曹起骧 中国科学,19972 27E:23) [9] Han J T、Zhao G,Cao Q X,Acta Metall Sin,1996:32:723(韩静待,赵钢,曹起骧,金属学报.1996;32:723) [10] Zhong Z P Ph D Thesis Tsinghua University,1998:97(钟志平,清华大学博士学位论文,1998:97)_ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|