| Nb合金化γ-TiAl的氧化热力学理论分析 |
| 王兴军 常海威 雷明凯 |
| 大连理工大学材料工程系表面工程研究室;大连116024 |
|
引用本文:
王兴军; 常海威; 雷明凯 . Nb合金化γ-TiAl的氧化热力学理论分析[J]. 金属学报, 2001, 37(8): 810-814 .
[1]Becker S, Rahmel A, Schorr M, Schutze M. Oxid Met, 1992; 38: 425 [2] Shida Y, Anada H. Corros Sci, 1993; 35: 945 [3]Lei M K, Zhu X P, Tang Z, Wang F. J Mater Sci Lett, 2000; 19: 1839 [4]Stroosnijder M F, Zheng N, Quadakkers W J, Hofman R, Gil A, Lanza F. Oxid Met, 1996; 46: 19 [5] Luthra K L. Oxid Met, 1991; 36: 475 [6] Rahmel A, Spencer P J. Oxid Met, 1991; 35: 53 [7] Eckert M, Bencze L, Kath D, Nickel H, Hilpert K. Bar Bunsenges Phys Chem, 1996; 100: 418 [8] Kattner U R, Lin J C, Chang Y A. Metall Trans 1992; 23A: 2081 [9] Kattner U R, Boettinger W .J. Mater Sci Eng, 1992; 152A:9 [10] Zhang F, Chen S L, Chang Y A, Kattner U R. Inter-metallics, 1997; 5: 471 [11] Ohnuma I, Fujita Y, Mitsui H, Ishikawa K, Kainuma R, Ishida K. Acta Mater, 2000; 48: 3113 [12] Li J T. Ph D. Thesis, Northeastern University, Shenyang, 1997: 103(李俊涛.东北大学博士学位论文,沈阳,1997:103) [13] Eckert M, Kath D, Hilpert K. Metal Mater Trans, 1999; 30A: 1315 [14] Dinsdale A T. CALPHAD, 1991; 15: 317 [15] Eckert M, Hilpert K. Mater Corros, 1997; 48: 10 [16] Jacobson N 5, Brady M P Mehrotra G M. Oxid Met, 1999; 52: 537 [17] Hao Y L, Xu D 5, Cui Y Y, Yang R, Li D. Acta Mater, 1999; 47: 1129 [18] Lei M K, Zhu X P, Han S Q, Wang D Y, Wang F C, Wang F. Mater Chem Phys, 2000; 65: 249 [19] Schmitz-Niederau M, Schutze M. Oxid Met, 1999; 52: 225 [20] Nickel H, Zheng N, Elschner A, Quadakkers W J. Microchim Acta, 1995; 119: 23M |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|