| 近液相线半连续铸造A356铝合金显微组织 |
| 王平 路贵民 崔建忠 |
| 东北大学材料电磁过程教育部重点实验室;沈阳110004 |
|
引用本文:
王平; 路贵民; 崔建忠 . 近液相线半连续铸造A356铝合金显微组织[J]. 金属学报, 2002, 38(4): 389-392 .
[1] Fleming M C. Metall Tans, 1991; 22B: 269 [2] Kenney M P, Courtois J A, Evans R D. Metals Handbook.Vol.15, 9th ed., Metals Park, Ohio: ASM, 1988: 327 [3] Kiuchi M, Sugiyama S. J Mater Shaping Technol, 1990;8: 39 [4] Chiarmetta G. In: Kirkwood D H, Kapranos P eds., Proc4th Int Conf on Semi-Solid Processing of Alloy and Com-posites. Sheffield: The University of Sheffield, 1996: 204 [5] Nakada M, Shiohara Y, Flemings M C. ISLI Int, 1990;30(1): 27 [6] Lu G M, Cui J Z, Dong J, Xia K. Conference Semi-SolidProcessing of Alloys and Composites, Iurin, Italy Sept.,2000: 373 [7] Cui J Z, Lu G M, Liu D, Dong J. J Harbin Inst Technol,(崔建忠,路贵民,刘 丹,董 杰.哈尔滨工业大学学报,2000;32(4):110) [8] Lu G M, Dong J, Cui J Z. Chin J Nonferrous Met, 2001;(路贵民,董 杰,崔建忠 中国有色金属学报,2001;11:211) [9] Chen C P, Tsao C Y A. J Mater Sci, 1995; 30: 4019 |
|