热变形条件下C-Mn钢奥氏体——铁素体相变模拟 |
兰勇军 黄成江 李殿中 |
中国科学院金属研究所 110016 |
|
引用本文:
兰勇军; 黄成江; 李殿中 . 热变形条件下C-Mn钢奥氏体——铁素体相变模拟[J]. 金属学报, 2003, 39(3): 242-248 .
[1] Tanaka T. Int Met Rev, 1981; 20: 185 [2] Zener C. J Appl Phys, 1949; 20: 950 [3] Enomoto M. Proc Int Conf on Physical Metallurgy of Thermo-Mechanical Processing of Steels and Other Metals (THERMEC 88) , Tokyo: Iron Steel Inst Japan, 1988: 360 [4] Christian J W. The Theory of Transformations in Metals and Alloys, 2nd ed., Oxford: Pergamon Press, 1981: 324 [5] Krielaart G P, Sietsma J, van der Zwaag S. Mater Sci Eng, 1997; 237A:216 [6] Agawal P K, Brimacombe J K. Metall Trans, 1981: 12B: 121 [7] de Ardo A .J. In: Southwick P, ed., Proc Conf Accelerated Cooling of Steels, Pittsburgh, PA: AIME, 1986: 97 [8] Umemoto M, Hiramatsu A, Moriya A, Watamabe T, Nanba S, Nakajima N, Anan G, Higo Y. 1SIJ Int. 1992; 32: 306 [9] Liu X, Karjalainen L P, Pertulla ,1 S. In: Beynon .J H, In-gham P, Teichert H, Waterson K, eds., Proc 2nd Int Conf on Modeling of Metal Rolling Processes, London: The Institute of Metals, 1996: 489 [10] Crooks M J, Garrat-Reed A J, Vander Saride J B, Owen W S. Metall Trans, 1982; 13A: 1347 [11] Torizuka S, Umezawa O, Tsuzaki K, Nagai K. Tetsu Ha-gane, 2000; 86: 26(长尾 彰英,仓本 繁,菅野进(?)宏,白神 哲夫,铁钢.2000;86:26) [12] Umenoto M, Ohtsuka H, Kato H, Tamura I, In: Dunne D P, Chandra T, eds., Proc Conf on High Strength Low Alloy Steels, Wollongong: University of Wollongong Press, 1984: 107 [13] David H, Sietsma J, van der Zwaag S. ISIJ hit, 2001; 41: 1028 [14] Yoshie A, Fujita T, Fujioka M, Okamoto K, Morikawa H, ISIJ Int, 1996; 36: 467 [15] Yoshie A, Fujita T, Fujioka M, Okamoto K, Morikawa H. ISIJ Int, 1996; 36: 474 [16] Roters F, Raabe D, Gottstein G. Acta Mater, 2000; 48: 4181 [17] Luce R, Wolske M, Kopp R, Roters F, Gottstein G. Com-put Mater Sci, 2001; 21: 1 [18] Aaronson H I, Domian H A, Pound G M. TMS A1MB, 1966; 236:768 [19] Bhadeshia H K D H. Met Sci, 1981; 15: 178 [20] Clemm P J, Fisher J C. Acta Metall, 1955; 3: 70 [21] Qu J B. PhD Thesis, Northeastern University, Shenyang, 1998: 58(曲锦波.东北大学博士学位论文,沈阳, 1998:58) [22] Xu z Y The Theory of Phase Transformation,Beijing:Science Press,2000:90(徐租耀.相变原理,北京:科学出版社, 2000:90) [23] Kaufman L,Clougherty E V,Weiss R T.Acta Matall,1963;11:323 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|