| Fe-Mn-Si形状记忆合金低温松弛机理 |
| 林成新 谷南驹 刘庆锁 温春生 赵连城 |
| 河北工业大学材料科学与工程学院;天津300130 |
|
引用本文:
林成新; 谷南驹; 刘庆锁; 温春生; 赵连城 . Fe-Mn-Si形状记忆合金低温松弛机理[J]. 金属学报, 2002, 38(8): 825-828 .
[1] Aato A, Chisima E, Soma K, Mori T. Ada Metall, 1982;30: 1177 [2] Kajiwara S. Mater Sci Eng, 1999; 273-275 : 67 [3] Tanahashi H, Maruyama T, Kubo H. Trans Mater ResSoc Jpn,1994; 18B: 1149 [4] Liu D Z, Liu W X, Gong F Y. J Phys IV Colloq, 1995;5(C8): 1241 [5] Duerig T W. Mater Sci Forum, 1990; 56-58: 679 [6] Yang J H, Chen H, Wayman C M. Metall Trans, 1992;23A: 1431q |
|