| Ni3Al中B和Mg的非平衡晶界共偏聚 |
| 胡静 张云 林栋梁 |
| 上海交通大学材料科学及工程学院;上海200030 |
|
引用本文:
胡静; 张云; 林栋梁 . Ni3Al中B和Mg的非平衡晶界共偏聚[J]. 金属学报, 2002, 38(8): 829-834 .
[1] Liu C T, White C L, Horton J A. Acta Metall, 1985; 33:213 [2] Choudhury A, White C L, Brooks C R. Scr Metall, 1986;20: 1061 [3] Lin D L, Chen D. Acta Metall Mater, 1990; 38: 523 [4] Choudhury A, White C L, Brooks C R. Acta Metall Mater,1992; 40: 57 [5] Zhang Y, Lin D L.Trans Met Heat Treat, 1996;17(Suppl.): 32(张云,林栋梁.金属热处理学报,1996;17(增刊):32) [6] Wang Y M, Lin D L, Zhang Y. Mater Res Soc Symp Proc,1997; 460: 511 [7] Zhang Y, Lin D L. Phys Test Chem Anal, Part A: Physical Testing, 1997; 33(1); 22(张云,林栋梁.理化检验(物理分册),1997;33(1):22) [8] Williams T M, Stoneham A M, Harries D K. Met Sci J,1976; 10: 14 [9] He X L, Chu Y Y. J Phys D: J Appl Phys, 1983; 16: 1145 [10] Chapman M A V, Faulkner R G. Acta Metall, 1983; 31:677 [11] Karsson L. Acta Metall, 1988; 36: 35 [12] Lin D L, Zhang Y. In: Ishida Y, Morita M, Suga T, Ichimose H, Ohashi O, Echigoya J eds., Interface Science and Materials Interconnection, Proc 8th Int Conf on Intergranular and Interphase Boundaries in Materials, Toyama, Japan, Tokyo: The Japan Institute of Metals, 1997: 53 [13] Lin D L, Zhang Y. Mater Sci Eng, 1998; 256A: 39 [14] Wang T M, Shimotomai M, Doyama M. J Phys F: MetPhys, 1984; 14: 37 [15] Swalin R A, Martin A, Olsen R. Trans AIME, 1957; 209:936 [16] Schewmon P G. Diffusion in Solids. New York: McGraw-Hill Book Company Inc, 1990: 115 [17] Yu Z S, Chen N. Sci Chin, 1992; (10)A: 1114(余宗森,陈宁.中国科学,1992;(10)A:1114) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|