| Ag对β-NiAl 的高温氧化膜Al2O3形貌的影响 |
| 张学军; 吴维弢;牛 焱 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳 110016 |
|
| Effect Of Silver Addition On Surface Morphology Of Al2O3 Scales During Oxidation Of β-NiAl |
| ZHANG Xuejun; WU Weitao; NIU Yan |
| State Key Laboratory for Corrosion and Protection; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
引用本文:
张学军; 吴维弢; 牛焱 . Ag对β-NiAl 的高温氧化膜Al2O3形貌的影响[J]. 金属学报, 2005, 41(4): 369-374 .
,
,
.
Effect Of Silver Addition On Surface Morphology Of Al2O3 Scales During Oxidation Of β-NiAl[J]. Acta Metall Sin, 2005, 41(4): 369-374 .
[1]Zhou J, Guo J T. Mater Sci Eng, 2003; A339: 166 [2]Rybicki G C, Smialek J L. Oxid Met, 1989; 31: 275 [3]Doychak J, Smialek J L, Mitchell T E. Metall Trans, 1989; 20A: 499 [4]Mosely P T, Hyde K R, Bellany B A, Tappin G. Carros Sci, 1984; 24: 547 [5]Doychak J, Ruhle M. Oxid Met, 1989; 31: 431 [6]Hagel W C. Corrosion, 1965; 21: 316 [7]Wood G C, Ghattopadhay B. Garros Sci, 1970; 10: 471 [8]Wood G C, Chattopadhay B. Oxid Met, 1970; 2: 373 [9]Smialek J L, Gibala R. Metall Trans, 1983; A10: 2143 [10]Brumm M W, Grabke H J. Corros Sci, 1992; 33: 1677 [11]Brumm M W, Grabke H J. Corros Sci, 1993; 34: 547 [12]Brumm M W, Grabke H J, Wagemann B. Corros Sci, 1994; 36: 37 [13]Grabke H J, Meier G H. Oxid Met, 1995; 44: 147 [14]Grabke H J, Wiemer D, Viefhaus H. Appl Surf Sci, 1997; 47: 243 [15]Grabke H J, Brumm M W, Wagemann B. Mater Corros, 1996; 47: 675 [16]Pint B A, Treska M, Hobbs L W. Oxid Met, 1997; 47: 1 [17]Yang S L, Wang F H, Niu Y, Wu W T. Mater Sci Forum, 2001; 369-372: 361 [18]Li M J, Sun X F, Guan H R, Jiang X X, Hu Z Q. Oxid Met, 2003; 59: 483 [19]Li M J, Sun X F, Guan H R, Jiang X X, Hu Z Q. Acta Metall Sin, 2003; 39: 755 (李猛进,孙晓峰,管恒荣,姜晓霞,胡壮麒.金属学报,2003; 39:755) [20]Zhang X J, Wu W T, Guo J T, Niu Y. High Temp Mater Proc, in press [21]Grabke H J. Intermetallics, 1999; 7: 1153 |
|