| AZ31镁合金蠕变初期的变形特征 |
| 田素贵; 杨景红;于兴福;孙根荣; 金敬铉; 徐永波;胡壮麒 |
| 沈阳工业大学 材料科学与工程学院; 沈阳 110023 |
|
| Deformation~ Features Of AZ31 Mg--Alloy In Initial Period Of High Temperature Creep |
| TIAN Sugui; YANG Jinghong; YU Xingfu;SOHN Keunyong; KIM Kyunghyun;XU Yongbo; HU Zhuangqi |
| Department of Materials Science and Engineering; Shenyang University of Technology; Shenyang 110023 |
引用本文:
田素贵; 杨景红; 于兴福; 孙根荣; 金敬铉; 徐永波; 胡壮麒 . AZ31镁合金蠕变初期的变形特征[J]. 金属学报, 2005, 41(4): 375-379 .
,
,
,
,
,
,
.
Deformation~ Features Of AZ31 Mg--Alloy In Initial Period Of High Temperature Creep[J]. Acta Metall Sin, 2005, 41(4): 375-379 .
[1]Winandy C D. In: Smith S D, Winandy C D, eds., Automotive Sourcing Special Report, London: Automotive Sourcing UK Ltd., 1998: 1 [2]Robert S B. Magnesium Products Design. USA: The International Magnesium Association. 1987: 373 [3]Claude D W. In: Smith S D, Winandy C D, eds., Automotive Sourcing Special Report, London: Automotive Sourcing UK Ltd., 1998: 8 [4]McQueen H J, Bourell D L. J Met, 1987; 39: 28 [5]McQueen H J, Bourell D L. J Mater Shaping Technol, 1987; 5: 53 [6]McQueen H J, Pekguleryuz M, In: Mordike B L, Hehman F, eds., Magnesium Alloys and Their Applications, Oberursel: DGM, 1992: 101 [7]Sittner P, Paidar V. Acta Metall, 1989; 37: 1717 [8]Myshlyaev M M, McQueen H J, Mwembela A, Konopleva E. Mater Sci Eng, 2003; A337: 121 [9]Galiyev A, Kabyshev R, Gottstein G. Acta Mater, 2001; 49: 1199 [10]Sheerly W F, Nash R R. Trans Metall Soc AIME, 1960; 218: 416 [11]Obara T, Yoshinaga H, Morozumi S. Acta Metall, 1973; 21: 845 [12]Koike J, Kobayashi T, Mukai T, Watanabe H, Suzuki M, Maruyama K, Higashi K. Acta Mater, 2003; 51: 2055 [13]Loreth M, Morton J, Jacobson K, Katrak F, Agarwal J. In: MacEwan S, Gilardeau J P, eds., Recent Metallurgical Advances in Light Metals, Montreal: Met Soc CIM, 1995: 11R |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|