| 工业纯铁内部穿晶疲劳微裂纹的扩散愈合过程 |
| 张海龙 杨君刚 孙军 |
| 西安交通大学金属材料强度国家重点实验室;西安710049 |
|
引用本文:
张海龙; 杨君刚; 孙军 . 工业纯铁内部穿晶疲劳微裂纹的扩散愈合过程[J]. 金属学报, 2002, 38(10): 1015-1020 .
[1] Lange F F. Am Geram Soc Bull, 1969; 48: 893 [2] Yen C F, Coble R L. J Am Ceram Soc, 1972; 55: 507 [3] Evans A G, Charles E A. Ada Metall, 1977; 25: 919 [4] Gupta T K. J Am Ceram Soc, 1978; 61: 191 [5] Zhang Y H, Edwards L, Plumbridge W J. J Am CeramSoc, 1998; 81: 1861 [6] Smith D L, Evans B. Journal of Geophysical Research,1984; 89: 4125 [7] Ackler H D. J Am Ceram Soc, 1998; 81: 3093 [8] Davies P, Cantwell W, Kausch H H. J Mater Sci Lett,1989; 8: 1247 [9] Zhou Y Z, Zeng Y, He G H, Zhou B L. J Mater Res, 2001;16: 17 [10] Gittins A. Acta Metall, 1968; 16: 517 [11] Herring C. J Appl Phys, 1950; 21: 301 [12] Huang P Z, Li Z H, Sun J. Metall Mater Trans A, 2002;33: 1117 [13] Markworth A J. Scr Metall, 1972; 6: 957 |
|