|
|
|
| 低碳钢低温变形γ→α相变行为的预测模型 |
| 许云波 王国栋 刘相华 |
| 东北大学轧制技术及连轧自动化国家重点实验室;沈阳110004 |
|
引用本文:
许云波; 王国栋; 刘相华 . 低碳钢低温变形γ→α相变行为的预测模型[J]. 金属学报, 2002, 38(10): 1021-1026 .
[1] Matsumura Y, Yada H. Transaction ISIJ, 1987; 27: 492 [2] Mintz B, Abu-Shosha R, Shaker M. Mater Sci Technol, 1993; 9: 907 [3] Yang W Y, Hu A M, Sun Z Q. Acta Metall Sin, 2000; 36: 1057(杨王(王月),胡安民,孙祖庆.金属学报,2000;36:1057) [4] Yang P, Fu Y Y, Cui F E, Yun Z Q. Acta Metall Sin, 2001; 37: 617(杨 平,傅云义,崔凤娥,孙祖庆.金属学报,2001;37:617) [5] Du L X, Liu X H, Wang G D. Acta Metall Sin, 2002; in press(杜林秀,刘相华,王国栋.金属学报,2002;待发表) [6] Xu Y B, Liu X H, Wang G D. Acta Metall Sin, 2002; inpress [7] Li W J. Ph D Thesis, Northestern University, 2001(李维娟.东北大学博士论文,2001) [8] Umemmto M. Acta Metall, 1986; 34: 1377 [9] Cahn J W. Acta Metall, 1956; 4: 449 [10] Cahn K S, Lee J K, Shiflet G J, Aaronson H I. MetallTrans A, 1978; 9A: 1016 [11] Imao T, Hiroshi S, Tomo T. Thermomechanical Processing of High Strength Low Alloy Steels. Tokyo: Butter-worths, 1988: 30 [12] Xu Z Y. The Theory of Transformation. Beijing: Science Press, 2000: 422(徐祖耀.相变原理.北京:科学出版社,2000:422) [13] Christian J W. The Theory of Transformations in Metal and Alloys. Oxford: Pergamon Press, 1965: 471 [14] Pham T T, Hawbolt E B, Brimacombe J K. Metall Mater Trans, 1995; 26A: 1987 [15] Yoshie A, Fujita T, Fujioka M, Okamoto K, Morikawa H. ISIJ Int, 1996; 36: 474 [16] Dutta B, Palmiere E J, Sellars C M. Acta Mater, 2001; 49: 785 [17] Umemoto M, Ohtsuka H, Tamura I. THERMEC-88, ISIJ, Tokyo, 1988; 2: 769 [18] Kaufman L, Radcliffe S V, Cohen M. Decomposition of Austenite by Diffusional Process. New York: Inter Science, 1962: 387 [19] Hillert M. Metall Trans, 1975; 6A: 5 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|