| Fe--0.3C--3Mn--2Ni--2Si中贝氏体表面浮突效应的原子力显微镜研究 |
| 杨金波 杨志刚 白秉哲 方鸿生 |
| 清华大学材料科学与工程系; 北京 100084 |
|
| Atomic Force Microscope Investigation of the Surface Relief Effect of Bainite in An Fe--C--Mn--Ni--Si Alloy |
| YANG Jinbo; YANG Zhigang; BAI Bingzhe; FANG Hongsheng |
| Department of Materials Science and Engineering; Tsinghua University; Beijing 100084 |
引用本文:
杨金波; 杨志刚; 白秉哲; 方鸿生 . Fe--0.3C--3Mn--2Ni--2Si中贝氏体表面浮突效应的原子力显微镜研究[J]. 金属学报, 2004, 40(6): 574-.
,
,
,
.
Atomic Force Microscope Investigation of the Surface Relief Effect of Bainite in An Fe--C--Mn--Ni--Si Alloy[J]. Acta Metall Sin, 2004, 40(6): 574-.
[1] Aaronson H I, Rigsbee J M, Muddle B C, Nie J F. Scr Mater, 2002; 47: 207 [2] Bowles J S, Mackenzie J K. Acta Met, 1954; 2: 129 [3] Srinivasan G R, Wayman C M. Acta Met, 1968; 16: 621 [4] Kinsman K R, Eichen E, Aaronson H I. Metall Trans,1975; 6A: 303 [5] Hall M G, Aaronson H I. Metall Mater Trans A, 1994;25A: 1923 [6] Bo X Z, Fang H S, Wang J J, Huang W G. Mater Trans JIM,1997; 38: 965 [7] Hirth J P, Spanos G, Hall M G, Aaronson H I. Acta Mater,1998; 46: 857 [8] Hehemann R F, Kinsman K R, Aaronson H I. Metall Trans, 1972; 3: 1077 [9] Fang H S, Wang J J, Yang Z G, Li C M, Deng X R, Zheng Y K. Prog Natur Sci, 1994; 4: 182 [10] Swallow E, Bhadeshia H K D H. Mater Sci Technol, 1996;12: 121 [11] Yang Z G, Fang H S, Wang J J, Zheng Y K. J Mater Sci Lett, 1996; 15: 721 [12] Yang Z G, Zhang C, Bai B Z, Fang H S. Mater Lett, 2001;48: 292 [13] Srinivasan G R, Wayman C M. The Mechanism of Phase Transformations in Crystalline Solids. London: Institute of Metals, 1969: 310 |
|