| 铸造镍基合金K44的高温蠕变行为 |
| 侯介山 张玉龙 郭建亭 冀 光 周兰章 叶恒强 |
| 中国科学院金属研究所; 沈阳 110016 |
|
| High Temperature Creep Behavior Of Cast Ni Base Superalloy K44 |
| HOU Jieshan; ZHANG Yulong; GUO Jianting;JI Guang; ZHOU Lanzhang; YE Hengqiang |
| Institute of Metal Research; The Chinese Academy of Science; Shenyang 110016 |
引用本文:
侯介山; 张玉龙; 郭建亭; 冀; 光; 周兰章; 叶恒强 . 铸造镍基合金K44的高温蠕变行为[J]. 金属学报, 2004, 40(6): 579-.
,
,
,
,
,
,
.
High Temperature Creep Behavior Of Cast Ni Base Superalloy K44[J]. Acta Metall Sin, 2004, 40(6): 579-.
[1] Huang X Y. Superalloy. Beijing: Metallurgy Industry Press, 2000: 350(黄晓尧.高温合金.北京:冶金工业出版社,2000:350) [2] Mukherjee A K, Bird J E, Dorn J E. Trans ASM,1969;62: 155 [3] Mclean M. Acta Metall, 1998; 34: 692 [4] Nabarro F R N, de Villiers H L. Physics of Creep. London:Taylor & Francis Ltd, 1995: 241 [5] Mukherji D, Jiao F, Chen W, Wahi R P. Acta Metall,1991; 39(7) : 1515 [6] Tian S G, Zhou H H, Zhang J H, Yang H C, Xu Y B, Hu Z Q. Mater Sci Eng, 2000; 279A: 160 [7] Maldini M, Lupic V. Scr Metall, 1988; 22: 1737 [8] Hou J S, Guo J T, Zhou L Z, Li G S. J Iron Steel Res,2003; 15(7) : 614(侯介山, 郭建亭, 周兰章, 李谷松. 钢铁研究学报, 2005; 15(7) :614) [9] Dyson B F, Mclean M. Acta Metall, 1983; 31: 25 [10] Dyson B F, Mclean M. Acta Metall, 1983; 31: 18 [11] Link T, Epishin A, Bruckner U. Acta Metall, 2000; 48:1981 [12] Feng D. Metal Physics (Vol.3) . Beijing: Science Press,1988: 565(冯端. 金属物理学(第三卷)北京; 科学出版社, 1988:565) [13] Monkman F C, Grant J. Proc ASTM 1956; 56: 593 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|