| 一种测算镍基合金r'相亚点阵元素浓度及点阵常数的方法 |
| 彭志方 刘 攀 |
| 武汉大学动力与机械学院; 武汉 430072 |
|
| A Simulating Approach to Elemental Concentration of Sublattices and Lattice Parameter of r', Phase in Ni Base Superalloys |
| PENG Zhifang;LIU Pan |
| College of Power and Mechanical Engineering; Wuhan University; Wuhan 430072 |
引用本文:
彭志方; 刘攀 . 一种测算镍基合金r'相亚点阵元素浓度及点阵常数的方法[J]. 金属学报, 2004, 40(6): 569-.
,
.
A Simulating Approach to Elemental Concentration of Sublattices and Lattice Parameter of r', Phase in Ni Base Superalloys[J]. Acta Metall Sin, 2004, 40(6): 569-.
[1] Volkl R, Glatzel U, Feller-Kniepmeier M. Acta Mater,1998; 46(12) : 4395 [2] Watanabe R, Kuno T. Tetsu-to-Hagane, 1975; 61: 2274(渡边力藏, 九重常男. 铁钢,1975; 61: 2274) [3] Bhadeshia H K D H, Sree Harsha Lalam, University of Cambridge, http://www.msm.cam.ac.uk/map/nickel/programs/lattice.htm, Feb, 2000 [4] Yoshitake S, Narayan V, Harada H, Bhadeshia H K D H,Mackay D J C. ISIJ Int, 1998; 38(5) : 495 [5] Enomoto M, Harada H, Yamazaki M. CALPHAD, 1991;15(2) : 143 [6] Ikeda Y. Mater Trans JIM, 1997; 38(9) : 761 [7] Harada H, Ohno K, Yamagata T, Yokokawa T, Yamazaki M. In: Reichmann S, Duhl D N, Maurer G, Antolovic S,Lunds C eds, Superalloys 1988, Warrendale, PA: TMSAIME 1988; 733 [8] Peng Z F, Ren Y Y, Zhang W, Yan P, Zhao J C, Wang Y Q. Acta Metall Sin, 2001; 37(4) : 345(彭志方, 任遥遥, 张伟, 燕平, 赵京晨, 王延庆. 金属学报, 2001; 37(4) : 345) [9] Peng Z F, Ren Y Y. Metall Mater Trans, 2002; 33A: 3065 [10] Blavette D, Bostel A. Acta Metall, 1984; 32 (5) : 811 [11] Schmidt R, Feller-Kniepmeier M. Metall Trans, 1992;23A: 745 [12] Caron P, Khan T. Mater Sci Eng, 1983; 61: 173 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|