| Ti53Cu15Ni18.5Al7M3Si3B0.5(M=Zr, Hf, Sc)高强度块体金属玻璃的制备及其性能 |
| 夏明许 郑红星 马朝利 李建国 |
| (上海交通大学 材料科学与工程学院; 上海 200030) |
|
引用本文:
夏明许; 郑红星; 马朝利; 李建国 . Ti53Cu15Ni18.5Al7M3Si3B0.5(M=Zr, Hf, Sc)高强度块体金属玻璃的制备及其性能[J]. 金属学报, 2005, 41(2): 199-202 .
[1] Perepezko J H. Smith J S. .J Non Cryst Solids,1981;44:65 [2] Inoue A, Othera K L, Masumoto T. .J Appl Phys,1988;27: L2248 [3] Inoue A, Zhang T. Mater Trans, 1989;30:965 [4] Inoue A, Zhang T, Masumoto T. Mater Trans,1990;31:177 [5] Inoue A, Nishiyama N, Matsuda T. Mater Trans,1996;37: 181 [6] Zhang T, Inoue A. Mater Trans,1998;39:1001 [7] Inoue A, Zhang T. Mater Trans. 1997;38:577 [8] Itoi T, Inoue A. Mater Trans. JIM, 1999; 41:1256 [9] Chiriac H. Lupu N. J Magn Magn Mater, 1999; 196-197:235 [10] Javazaki H. Kaih U,Izemiya K. Mater Sci Eng,2001;A318: 77 [11] Kim Y C, Kim W T. Kirn D H. Mater Trans 2002;43:1243 [12] Zhang T, Inoue A. Mater Trans,1998;39:1001 [13] Inoue A. Mater Sci Forum, 1995: 179/191: 691 [14] Egami T. J Non Cryst Solids, 1996;205-207:575 [15] Nagel S R, Tauc J. Phys Rev Lett,1975;35:380 [16] Zhang T, Inoue A, Masumoto T. Mater Sci Eng,1994;A181/A182: 1423 [17] Hahn T. International Tables for Crystallography,VolumeA, Kluwer Acadmic Publishers, Boston,1995:681 [18] de Boer F R, Boom R,Mattens W C M,Miedema A R,Niesterdam A K. Cohesion in Metals. North-Holland:El-sevier Science Pubilishers, 1989: 1X |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|