| 硼含量对Fe-Zr-B-Nb非晶合金的晶化、形成能力和磁性能的影响 |
| 肖 利 张 可 华 中 姚 斌 |
| 吉林师范大学物理学院; 四平 136000 |
|
引用本文:
肖利; 张可; 华中 ; 姚斌 . 硼含量对Fe-Zr-B-Nb非晶合金的晶化、形成能力和磁性能的影响[J]. 金属学报, 2005, 41(2): 203-208 .
[1] Suzuki K, Makino A, Kataoka N, Inoue A, Masumoto T.Mater Trans JIM, 1991; 32: 93 [2] Makino A, Suzuki K, Inoue A, Hirotsu Y, Masumoto T.J Magn Magn Mater, 1994; 133: 329 [3] Shen B G, Xu R F, Zhao J G, Zhan W S. Phys Rev B,1991; 43: 11005 [4] Slawaska-Waniewska A, Zuberek R. J Magn Magn Mater,1996; 160: 253 [5] Brzozka K, Slawaska-Waniewska A, Jezuita K. J MagnMagn Mater, 1996; 160: 255 [6] Kim K Y, Noh T H, Kang I K. Mater Sci Eng, 1994;A179/A180: 552 [7] Kemeny T, Kaptas D, Kiss L K, Pusztai T, Balogh J,Vincze I. J Magn Magn Mater, 2000; 215/216: 268 [8] Ohnuma S, Shirakawa K, Nose M, Masumoto T. IEEETrans Magn, 1980; 16: 1129 [9] Hasegawa R, Ray R. J Appl Phys, 1978; 49: 4174 [10] Chien C C, Musser D, Gyorgy E M, Sherwood R C, ChenH S, Lubersky F E, Walfer J L. Phys Rev B, 1979; 20:283 [11] Inoue A, Zhang T, Takeuchi A. Appl Phys Lett, 1997; 71:464 [12] Inoue A. Acta Mater, 2000; 48: 279 [13] Makino A, Bitoh T, Kojima A, Inoue A, Masumoto T. JAppl Phys, 2000; 87(9): 7100 [14] Muller M, Grahl H, Mattern N, Kuhm U. Mater Sci Eng,1997; A226-228: 565 [15] Ma L Q, Wang L M, Zhang T, Inoue A. J Mater Sci Lett,1998; 17: 1893 [16] Ma L Q, Wang L M, Zhang T, Inoue A. Mater Res Bull,1999; 34(6): 915 [17] Greer A L. Nature, 1993; 366: 303 [18] Wang W H, Yang H B. J Appl Phys, 1998; 84: 5961 [19] Kemeny T, Kaptas D, Kiss L, Pusztai T F, Balgh J, VinczeI. J Magn Magn Mater, 2000; 215-216: 268 [20] Kaptas D, Kemeny T, Balogh J, Bujdoso L, Kiss L F,Pusztai T, Vincze I. J Phys Condens Matter, 1999; 11:L179 [21] Hong R, Ryan D H. Phys Rev B, 1995; 51: 15885 [22] Saito N, Hiroyoshi H, Fukamuchi K, Nakagawa Y. J PhysF Met Phys, 1986; 16: 911 [23] Kaul S N, Siruguri V, Chandra G. Phys Rev B, 1992; 45:12343 [24] Jackson K A. Nucleation Phenomena, Washington:American Chem Soc, 1966: 37 [25] Turbull D. Contemp Phys, 1969; 10: 473 [26] Chen H S. Appl Phys Lett, 1976; 29(1): 12 [27] Luborsky F E, Liebermann H H, Becker J J, Walter JL. Amorphous Metallic Alloys. London Butterworths:Luborsky F E, 1983: 188 [28] Durand J. Amorphous Magnetism Ⅱ, New York PlenumPress: R A Levy and R Hasegawa, 1977: 275 [29] Becker J J. IEEE Trans' Magn, 1977; 13: 988 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|