| 铁基块状非晶合金的制备及性能 |
| 刘冬艳 王 成 张海峰 胡壮麒 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
引用本文:
刘冬艳; 王成; 张海峰; 胡壮麒 . 铁基块状非晶合金的制备及性能[J]. 金属学报, 2005, 41(2): 209-213 .
[1] Rraskin D, Smith C H. In: Luborsky F E ed., AmorphousMetallic Alloys. London: Butterworths, 1983: 381 [2] Smith C H. In: Liebermann H H ed., Rapid Solidified Alloys. New York: Marcel Dekker, 1993: 617 [3] Inoue A, Shinohara Y, Gook J S. Mater Trans JIM, 1995;36: 1427 [4] Inoue A, Zhang T, Koshiba H, Makino A. J Appl Phys,1999; 85: 5136 [5] Zhang W, Inoue A. Mater Trans JIM, 2000; 41: 1679 [6] Zhang T, Inoue A. Mater Trans JIM, 2001; 42: 1015 [7] Inoue A, Shen B L. Mater Trans JIM, 2002; 43: 2350 [8] Inoue A, Zhang T, Takeuchi A. Appl Phys Lett, 1997;7 1:464 [9] Shen T D, Schwarz R B. Appl Phys Lett, 1999; 75: 49 [10] Shen T D, Schwarz R B. Ada Mater, 2001; 49: 837 [11] Inoue A, Takeuchi A, Zhang T. Metall Mater Trans, 1998;29A: 177 [12] Greer A L. Nature, 1993; 336: 303 [13] Xiao G, Chien C L. Phys Rev, 1987; B35: 8763 [14] Grabias A, Kopcewicz M, Oleszak D. J Alloy Compd,2002; 339: 221 [15] Aubertin F, Gonser U, Campbell S, Wagner H G. Z Met-allkunde Bd, 1985; 76: 237 [16] Fries S M, Chien C L, Crummenauer J, Wagner H G,Gonser U. Hyperfine Interact, 1986; 27: 405 [17] Novakova A A, Kiselmnd T Y, Sidorova G V. Nuc InstMethod, Phys Res, 1993; B76: 107 [18] Cao C N. Corrosion Electrochemistry. Beijing: Chemistry Industry Press, 1985: 215(曹楚南.腐蚀电化学原理.北京:化学工业出版社,1985:215) [19] Xu X J, Ma H Y, Chen S H, Xu Z Y, Sui A F. J Elec-trochem Soc, 1999; 146: 1847 [20] Pourbaix M. Atlas of Electrochemical Equilibrim in Aqueous Solution (2nd edition). Pergamon, Houston, TX, 1974 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|