| 马氏体相变的形核问题 |
| 孟庆平 戎咏华 徐祖耀 |
| (上海交通大学材料科学与工程学院; 上海 200030) |
|
| Nucleation Of Martensitic Transformation[ |
| MENG Qingping; RONG Yonghua; T.Y. Hsu (XU Zuyao) |
| School of Materials Science and Engineering; Shanghai Jiao Tong University; Shanghai 200030 |
引用本文:
孟庆平; 戎咏华; 徐祖耀 . 马氏体相变的形核问题[J]. 金属学报, 2004, 40(4): 337-341 .
,
,
.
Nucleation Of Martensitic Transformation[[J]. Acta Metall Sin, 2004, 40(4): 337-341 .
[1] , 1948;18:999Kurdjumov G V.J Met,1959;11:449 [2] Shih C H,Averbach B L,Cohen M.Trans AIME,1955 203: 183 [3] Wechsler M S, Lieberman D S, Read T A. Trans AIME,1953; 197: 1503 [4] Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129,224, 1957; 5: 137 [5] Hsu T Y(Xu Zuyao).Martensitic Transformation andMartensite.2nd ed.,Beijing:Science Press,1999:430(徐祖耀.马氏体相变与马氏体.第2版,科学出版社,1999:430) [6] Pati S R, Cohen M. Acta Metall, 1969; 17: 189 [7] Pati S R, Cohen M. Acta Metall, 1971; 19: 1327 [8] Lin M, Olson G B, Cohen M. Metall Trans, 1992; 23A:2987 [9] Cohen M. Trans AIME, 1958; 212: 171 [10] Kaufman L, Cohen M. In: Chalmers B, King R eds.,Progress in Metal Physics. Vol.7, New York: PergamonPress, 1958: 165 [11] Owen W S, Gilbert A. JISJ, 1961; 196: 142 [12] Fisher J C, Hollomon J H, Turnbull D. J Appl Phys, 1948;19: 775 [13] Turnbull D. Trans AIME, 1948; 175: 774 [14] Turnbull D, Fisher J C. J Chem Phys, 1949; 17: 71 [15] Kulin S A, Cohen M. Trans AIME, 1950; 188: 1139 [16] Machlin E S, Cohen M. Trans AIME, 1951; 191: 746 [17] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897 [18] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1905 [19] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1915 [20] Magee C L. In: Aaronson H I ed., Phase Transformation.Cleveland: ASM, 1970: [21] Suezawa M, Cook H E. Acta Metall, 1980; 28: 423 [22] Russell K C. Metall Trans, 1971; 2: 5 [23] Deng Y R.Rare Met Mater Eng,1991;(1) :17(邓永瑞.稀有金属材料与工程, 1991;(1) :17) [24] Deng Y R.Rare Met Mater Eng,1991;(2) :9(邓永瑞.稀有金属材料与工程, 1991;(2) :9) [25] Deng Y R.Rare Met Mater Eng,1991;(3) :16(邓永瑞.稀有金属材料与工程, 1991;(3) :16) [26] Deng Y R.Theory of Martensitic Transformation.Bei-jing:Science Press,1993:7(邓永瑞.马氏体相变理论.北京:科学出版社, 1993:7) [27] Xiao J M.Phases and Phase Transformations of Alloys.Beijing:Metallurgy Industry Press,1987:332(肖纪美.合金相与相变.北京:冶金工业出版社,1987:332) [28] Zhao X Q.Acta Metall Sin,2001;37:1153(赵新清.金属学报,2001;37:1153) [29] Zhao X Q.J Mater Eng,1999;(11) :3(赵新清.材料工程,1999;(11) :3) [30] Zhao X Q,Han Y F.J Mater Eng,2000;(3) :3(赵新清,韩雅芳.材料工程, 2000;(3) :3) [31] Zhao X Q, Liu B X. Scr Mater, 1998; 38: 1137 [32] Zhao X Q, Han Y F. Metall Mater Trans, 1999; 30A: 884 [33] Landau L D, Lifshitz E M. Statistical Physics, Part 1 (3rd ed). Butterworth-Heinemann, Division of Reed Educational and Professional Ltd., 1999: 533 [34] Feder J, Russell K C, Lothe J, Pound G M. Adv Phys,1966; 15: 111 [35] Gunton J D, Miguel M S, Sahni P S. In: Domb C, Green M S eds., Phase Transitions and Critical Phenomena, Vol.8. London: Academic Press, 1983: 267 [36] Gunton J D. J Stat Phys, 1999; 95: 903 [37] Turnbull D. J Chem Phys, 1952; 20: 411 [38] Trunbull D, Cohen M H. J Chem Phys, 1958; 29: 1049 [39] Landau L D, Lifshitz E M. Statistical Physics, Part 1 (3rd ed). Butterworth-Heinemann, Division of Reed Educational and Professional Ltd., 1999: 34 [40] Lin M, Olson G B, Cohen M. Ada Metall Mater, 1992; 41: 253 [41] Kajiwara S, Ohno S, Honma K. Philos Mag, 1991; 63A: 625 [42] Kaufman L, Cohen M. Trans AIME, 1956; 206: 1393 [43] Cech R E, Turnbull D. Trans AIME, 1956; 206: 124 [44] Cech R E. Trans AIME, 1956; 206: 585 [45] Kelly T F, Cohen M, Sande J B V. Metall Trans, 1984; 15A: 819 [46] Meng Q P.PhD Dissertation,Shanghai Jiao Tong Uni-versity,2002(孟庆平.上海交通大学博士学位论文, 2002) [47] Rong Y, Meng Q, Hsu T Y (Xu Zuyao). In: Hanada S, Zhong Z, Nam S W, Wright R N eds., The 4th Pacific Rim Int Conf on Advanced Materials and Processing (PRICM4) . The Japan Institute of Metals, 2001: 147 [48] Alexander S, Mctague J. Phys Rev Lett, 1978; 41: 702 [49] Auer S, Frenkel D. Nature, 2001; 409: 1020 [50] Hsu T Y(Xu Zuyao).Shanghai Met,2003;25(3) :1 and25(4) :1(徐祖耀.马氏体相变研究的进展.第8次全国热处理大会特邀报告,2003,见:上海金属,2003;25(3) :1和25(4) :1) [51] Patel J R, Cohen M. Acta Metall, 1953; 1: 531 [52] Meng Q P, Rong Y H, Hsu T Y (Xu Zuyao). to be published. [53] Offerman S E, Dijk N H, Sietsma J, Grigull S, LauridsenE M, Margulier L, Poulsen H F, Rekveldt M Th, ZwaagS. Science, 2002; 298: 1003 [54] Buff F P, Kirkwood J G. J Chem Phys, 1950; 18: 991 [55] Tolman R C. J Chem Phys, 1949; 17: 333 [56] Olson G B, Cohen M. Proc Int Conf Solid-Solid PhaseTransformations, New York: AIME, 1982: 1145 [57] Falk F. Acta Metall, 1980; 28: 1773 [58] Falk F. Z Phys B, Condens Matter, 1984; 54: 159 [59] Barsch G R, Krumhansl J A. Metall Trans, 1988; 19A:761 [60] Klein W, Lookman T, Saxena A, Hatch D M. Phys RevLett, 2002; 88: 085701 [61] Zhao Y, Zhang J, Hsu T Y (Xu Zuyao). J Appl Phys,2000; 88: 4022 [62] Tang M, Zhang J H, Hsu T Y (Xu Zuyao). Acta Mater,2002; 50: 467 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|