马氏体相变的形核问题
孟庆平 戎咏华 徐祖耀
(上海交通大学材料科学与工程学院; 上海 200030)
Nucleation Of Martensitic Transformation[
MENG Qingping; RONG Yonghua; T.Y. Hsu (XU Zuyao)
School of Materials Science and Engineering; Shanghai Jiao Tong University; Shanghai 200030
引用本文:

孟庆平; 戎咏华; 徐祖耀 . 马氏体相变的形核问题[J]. 金属学报, 2004, 40(4): 337-341 .
, , . Nucleation Of Martensitic Transformation[[J]. Acta Metall Sin, 2004, 40(4): 337-341 .

全文: PDF(187 KB)  
摘要: 在对马氏体相变经典形核理论阐述的基础上, 仔细考察了Fisher等以统计物理对形核几率的原始推导, 指出一些学者近年来否定Cohen和Kaufman马氏体相变形核几率计算的错误, 确定形核几率计算中的形核能垒ΔG*应为临界核胚中所有原子的总自由能变化, 而不应为核胚中单个原子的自由能. 对他们佐证均匀形核观点所引用的实验给予了重新解释, 对他们提出的形核模型进行了评论. 最后简要提出研究马氏体相变形核问题的几个可能方向.
关键词 : 马氏体相变,  形核几率,  形核能垒    
Abstract:On the basis of describing the classical nucleation theory of martensitic transformation and considering in detail the original derivation of nucleation probability through statistical physics by Fisher $et~al$, the present work points out the mistakes appearing in the recent works of some authors who negated the calculation of the nucleation probability of martensitic transformation with Cohen and Kaufman. The nucleation barrier ΔG* in calculating the nucleation probability should be the free energy change of total atoms in an embryo, rather than that of an atom. The experiments cited by these scholars, supporting their viewpoint of homogeneous nucleation of martensitic transformation, are re--explained and the nucleation model suggested by them is critically reviewed by us with the basic concept of statistical physics. Finally, several research directions are briefly suggested for study of the nucleation of martensitic transformation.
Key words: martensitic transformation    nucleation probability    nucleation barrier
收稿日期: 2002-06-05     
ZTFLH:  TG151  
[1] , 1948;18:999Kurdjumov G V.J Met,1959;11:449
[2] Shih C H,Averbach B L,Cohen M.Trans AIME,1955 203: 183
[3] Wechsler M S, Lieberman D S, Read T A. Trans AIME,1953; 197: 1503
[4] Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129,224, 1957; 5: 137
[5] Hsu T Y(Xu Zuyao).Martensitic Transformation andMartensite.2nd ed.,Beijing:Science Press,1999:430(徐祖耀.马氏体相变与马氏体.第2版,科学出版社,1999:430)
[6] Pati S R, Cohen M. Acta Metall, 1969; 17: 189
[7] Pati S R, Cohen M. Acta Metall, 1971; 19: 1327
[8] Lin M, Olson G B, Cohen M. Metall Trans, 1992; 23A:2987
[9] Cohen M. Trans AIME, 1958; 212: 171
[10] Kaufman L, Cohen M. In: Chalmers B, King R eds.,Progress in Metal Physics. Vol.7, New York: PergamonPress, 1958: 165
[11] Owen W S, Gilbert A. JISJ, 1961; 196: 142
[12] Fisher J C, Hollomon J H, Turnbull D. J Appl Phys, 1948;19: 775
[13] Turnbull D. Trans AIME, 1948; 175: 774
[14] Turnbull D, Fisher J C. J Chem Phys, 1949; 17: 71
[15] Kulin S A, Cohen M. Trans AIME, 1950; 188: 1139
[16] Machlin E S, Cohen M. Trans AIME, 1951; 191: 746
[17] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897
[18] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1905
[19] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1915
[20] Magee C L. In: Aaronson H I ed., Phase Transformation.Cleveland: ASM, 1970:
[21] Suezawa M, Cook H E. Acta Metall, 1980; 28: 423
[22] Russell K C. Metall Trans, 1971; 2: 5
[23] Deng Y R.Rare Met Mater Eng,1991;(1) :17(邓永瑞.稀有金属材料与工程, 1991;(1) :17)
[24] Deng Y R.Rare Met Mater Eng,1991;(2) :9(邓永瑞.稀有金属材料与工程, 1991;(2) :9)
[25] Deng Y R.Rare Met Mater Eng,1991;(3) :16(邓永瑞.稀有金属材料与工程, 1991;(3) :16)
[26] Deng Y R.Theory of Martensitic Transformation.Bei-jing:Science Press,1993:7(邓永瑞.马氏体相变理论.北京:科学出版社, 1993:7)
[27] Xiao J M.Phases and Phase Transformations of Alloys.Beijing:Metallurgy Industry Press,1987:332(肖纪美.合金相与相变.北京:冶金工业出版社,1987:332)
[28] Zhao X Q.Acta Metall Sin,2001;37:1153(赵新清.金属学报,2001;37:1153)
[29] Zhao X Q.J Mater Eng,1999;(11) :3(赵新清.材料工程,1999;(11) :3)
[30] Zhao X Q,Han Y F.J Mater Eng,2000;(3) :3(赵新清,韩雅芳.材料工程, 2000;(3) :3)
[31] Zhao X Q, Liu B X. Scr Mater, 1998; 38: 1137
[32] Zhao X Q, Han Y F. Metall Mater Trans, 1999; 30A: 884
[33] Landau L D, Lifshitz E M. Statistical Physics, Part 1 (3rd ed). Butterworth-Heinemann, Division of Reed Educational and Professional Ltd., 1999: 533
[34] Feder J, Russell K C, Lothe J, Pound G M. Adv Phys,1966; 15: 111
[35] Gunton J D, Miguel M S, Sahni P S. In: Domb C, Green M S eds., Phase Transitions and Critical Phenomena, Vol.8. London: Academic Press, 1983: 267
[36] Gunton J D. J Stat Phys, 1999; 95: 903
[37] Turnbull D. J Chem Phys, 1952; 20: 411
[38] Trunbull D, Cohen M H. J Chem Phys, 1958; 29: 1049
[39] Landau L D, Lifshitz E M. Statistical Physics, Part 1 (3rd ed). Butterworth-Heinemann, Division of Reed Educational and Professional Ltd., 1999: 34
[40] Lin M, Olson G B, Cohen M. Ada Metall Mater, 1992; 41: 253
[41] Kajiwara S, Ohno S, Honma K. Philos Mag, 1991; 63A: 625
[42] Kaufman L, Cohen M. Trans AIME, 1956; 206: 1393
[43] Cech R E, Turnbull D. Trans AIME, 1956; 206: 124
[44] Cech R E. Trans AIME, 1956; 206: 585
[45] Kelly T F, Cohen M, Sande J B V. Metall Trans, 1984; 15A: 819
[46] Meng Q P.PhD Dissertation,Shanghai Jiao Tong Uni-versity,2002(孟庆平.上海交通大学博士学位论文, 2002)
[47] Rong Y, Meng Q, Hsu T Y (Xu Zuyao). In: Hanada S, Zhong Z, Nam S W, Wright R N eds., The 4th Pacific Rim Int Conf on Advanced Materials and Processing (PRICM4) . The Japan Institute of Metals, 2001: 147
[48] Alexander S, Mctague J. Phys Rev Lett, 1978; 41: 702
[49] Auer S, Frenkel D. Nature, 2001; 409: 1020
[50] Hsu T Y(Xu Zuyao).Shanghai Met,2003;25(3) :1 and25(4) :1(徐祖耀.马氏体相变研究的进展.第8次全国热处理大会特邀报告,2003,见:上海金属,2003;25(3) :1和25(4) :1)
[51] Patel J R, Cohen M. Acta Metall, 1953; 1: 531
[52] Meng Q P, Rong Y H, Hsu T Y (Xu Zuyao). to be published.
[53] Offerman S E, Dijk N H, Sietsma J, Grigull S, LauridsenE M, Margulier L, Poulsen H F, Rekveldt M Th, ZwaagS. Science, 2002; 298: 1003
[54] Buff F P, Kirkwood J G. J Chem Phys, 1950; 18: 991
[55] Tolman R C. J Chem Phys, 1949; 17: 333
[56] Olson G B, Cohen M. Proc Int Conf Solid-Solid PhaseTransformations, New York: AIME, 1982: 1145
[57] Falk F. Acta Metall, 1980; 28: 1773
[58] Falk F. Z Phys B, Condens Matter, 1984; 54: 159
[59] Barsch G R, Krumhansl J A. Metall Trans, 1988; 19A:761
[60] Klein W, Lookman T, Saxena A, Hatch D M. Phys RevLett, 2002; 88: 085701
[61] Zhao Y, Zhang J, Hsu T Y (Xu Zuyao). J Appl Phys,2000; 88: 4022
[62] Tang M, Zhang J H, Hsu T Y (Xu Zuyao). Acta Mater,2002; 50: 467
[1] 姜江, 郝世杰, 姜大强, 郭方敏, 任洋, 崔立山. NiTi-Nb原位复合材料的准线性超弹性变形[J]. 金属学报, 2023, 59(11): 1419-1427.
[2] 李伟, 贾兴祺, 金学军. 高强韧QPT工艺的先进钢组织调控和强韧化研究进展[J]. 金属学报, 2022, 58(4): 444-456.
[3] 原家华, 张秋红, 王金亮, 王灵禺, 王晨充, 徐伟. 磁场与晶粒尺寸协同作用对马氏体形核及变体选择的影响[J]. 金属学报, 2022, 58(12): 1570-1580.
[4] 王金亮, 王晨充, 黄明浩, 胡军, 徐伟. 低应变预变形对变温马氏体相变行为的影响规律及作用机制[J]. 金属学报, 2021, 57(5): 575-585.
[5] 左良, 李宗宾, 闫海乐, 杨波, 赵骧. 多晶Ni-Mn-X相变合金的织构化与功能行为[J]. 金属学报, 2021, 57(11): 1396-1415.
[6] 肖飞, 陈宏, 金学军. 形状记忆合金弹热制冷效应的研究现状[J]. 金属学报, 2021, 57(1): 29-41.
[7] 王世宏,李健,葛昕,柴锋,罗小兵,杨才福,苏航. γ/ε双相Fe-19Mn合金在拉伸变形过程中的组织演变和加工硬化行为[J]. 金属学报, 2020, 56(3): 311-320.
[8] 郑晓航, 宁睿, 段佳彤, 蔡伟. Ti70-xTa15Zr15Fex (x=0.3、0.6、1.0)形状记忆合金薄膜的马氏体相变与阻尼行为[J]. 金属学报, 2020, 56(12): 1690-1696.
[9] 陈雷, 郝硕, 梅瑞雪, 贾伟, 李文权, 郭宝峰. 节约型双相不锈钢TRIP效应致塑性增量及其固溶温度依赖性[J]. 金属学报, 2019, 55(11): 1359-1366.
[10] 崔立山, 姜大强. 基于应变匹配的高性能金属纳米复合材料研究进展[J]. 金属学报, 2019, 55(1): 45-58.
[11] 魏铖, 柯常波, 马海涛, 张新平. 基于序参量梯度的改进相场模型及对大尺度体系马氏体相变的模拟研究[J]. 金属学报, 2018, 54(8): 1204-1214.
[12] 韦昭召, 马骁, 张新平. NiTi合金B2-B19′马氏体相变晶体学的拓扑模拟研究[J]. 金属学报, 2018, 54(10): 1461-1470.
[13] 杨继兰, 蒋元凯, 顾剑锋, 郭正洪, 陈海龑. 奥氏体化温度对中碳淬火-配分钢干滑动摩擦磨损性能的影响[J]. 金属学报, 2018, 54(1): 21-30.
[14] 王学,胡磊,陈东旭,孙松涛,李立全. 马氏体相变对9%Cr热强钢管道多道焊接头残余应力演化的影响[J]. 金属学报, 2017, 53(7): 888-896.
[15] 张晓嵩,徐勇,张士宏,程明,赵永好,唐巧生,丁月霞. 塑性变形及固溶处理对奥氏体不锈钢晶间腐蚀性能的协同作用研究[J]. 金属学报, 2017, 53(3): 335-344.