| 柱状晶Ni在冷轧过程中晶粒取向的演变及模拟 |
| 吴桂林;刘 伟;Andrew Godfrey;刘 庆 |
| (清华大学材料科学与工程系; 北京 100084) |
|
| EXPERIMENTAL OBSERVATION AND MODELLING OF THE ORIENTATION EVOLUTION OF INDIVIDUAL GRAINS IN COLUMNAR GRAIN Ni DURING COLD ROLLING |
引用本文:
吴桂林; 刘伟; Andrew Godfrey; 刘庆 . 柱状晶Ni在冷轧过程中晶粒取向的演变及模拟[J]. 金属学报, 2004, 40(8): 785-790 .
[1] Hansen N. Metali Mater Trans A, 2001; 32A: 2917 [2] Bay B, Hansen N, Hughes D A, Kuhlmann-Wilsdorf D.Acta Metali Mater, 1992; 40: 205 [3] Hughes D A, Hansen N. Metali Trans, 1993; 24A: 2021 [4] Hansen N, Juul Jensen D. Proc R Soc Lond A, 1999; 357:1447 [5] Liu Q, Juul Jensen D, Hansen N. Acta Mater, 1997; 46:5819 [6] Huang X, Hansen N. Scr Mater, 1997; 38: 1 [7] Huang X. Scr Mater, 1998; 38: 1697 [8] Delannay L, Mishin O V, Juul Jensen D, Van Houtte P.Acta Mater, 2001; 49: 2441 [9] Solas D E, Tome C N. Inter J Plast, 2001; 17: 737 [10] Hirsch J, Nes E, Lucke K. Acta Metali, 1987; 35: 427 [11] Skalli A, Fortunier R, Fillit R, Driver J H. Acta Metali,1985; 33: 997 [12] Panchanadeeswaran P, Doherty R D, Becker R. ActaMater, 1996; 44: 1233 [13] Raabe D, Sachtleber M, Weiland H, Scheele G, Zhao Z.Acta Mater, 2003; 51: 1539 [14] Bhattacharyya A, El-Danaf E, Kalidindi S R, Doherty RD. Inter J Plast, 2001; 17: 861 [15] Krieger Lassen N C, Juul Jensen D, Conradsen K. ActaCrystall, 1994; A50: 741 [16] Hartig C H, Feller-Kniepmeier M. Acta Metali, 1985; 33:743 [17] Taylor G J. J Ins Met, 1938; 62: 307 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|