| 钢中fcc/bcc(bct)马氏体形核与长大的一种晶体学模型 |
| 杨金波;杨志刚;邱冬;张文征;张弛;白秉哲;方鸿生 |
| 清华大学材料科学与工程系; 北京 100084 |
|
| A general crystallographic model of fcc/bcc(bct) martensitic nucleation and growth in steels |
| YANG Jinbo; YANG Zhigang; QIU Dong; ZHANG Wenzheng; ZHANG Chi; BAI Bingzhe; FANG Hongsheng |
| Department of Materials Science and Engineering; Tsinghua University; Beijing 100084 |
引用本文:
杨金波; 杨志刚; 邱冬; 张文征; 张弛; 白秉哲; 方鸿生 . 钢中fcc/bcc(bct)马氏体形核与长大的一种晶体学模型[J]. 金属学报, 2005, 41(3): 225-230 .
,
,
,
,
,
,
.
A general crystallographic model of fcc/bcc(bct) martensitic nucleation and growth in steels[J]. Acta Metall Sin, 2005, 41(3): 225-230 .
[1] Cohen M, Olson G B, Clapp P C. In: Owen W S, Cohen M, Wayman C M, eds., Proc Int Conf on Martensitic Transformations, ICOMAT 79, Cambridge, Mass: MIT Press, 1979: 1 [2] Christian J W. Mater Sci Eng, 1990; A127: 215 [3] Aaronson H I, Hall M G. Metall Mater Trans, 1994; 25A: 1797 [4] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1905 [5] Olson G B, Cohen M. Metall Trans, 1976; 7A: 1915 [6] Bogers A J, Burgers W G. Acta Metall, 1964; 12: 255 [7] Roytburd A L, Khachaturyan A G. Phys Met Metall, 1970; 30: 68 [8] Kurdjumov G V, Khachaturyan A G. Acta Metall, 1975; 23: 1077 [9] Wechsler M S, Lieberman D S, Read T A. Trans AIME, 1953; 197: 1503 [10] Bowles J S, Mackenzie J K. Acta Metall, 1954; 2: 129 [11] Dahmen U, Westmacott K H. In: Aaronson H I, et al, eds., Proc Int Conf on Solid-Solid Phase Transformation, Warrendale, Pa: The Metallurgical Society of AIME, 1981: 433 [12] Dahmen U. Acta Metall, 1982; 30: 63 [13] Luo C P, Weatherly G C. Acta Metall, 1987; 35: 1963 [14] Zhang W Z, Purdy G R. Philos Mag, 1993; 68A: 291 [15] Zhang W Z, Weatherly G C. Acta Mater, 1998; 46: 1837 [16] Qiu D, Zhang W Z. Philos Mag, 2003; 83: 3093 [17] Frank F C. Acta Metall, 1953; 1: 15 [18] Srinivasan G R, Wayman C M. Acta Metall, 1968; 16: 621 [19] Hirth J P, Spanos G, Hall M G, Aaronson H I. Acta Mater, 1998; 46: 857 [20] Liu X, Zhong F, Zhang J X, Zhang M X, Kang M K, Guo Z Q. Phys Rev, 1995; 52B: 9970 [21] Ridley N, Stuart H, Zwell L. TMS AIME, 1969; 245: 1834 [22] Wayman C M. Introduction to the Crystallography of Martensitic Transformations. New York: The MacMil-lan Co., 1964: 146 [23] Greninger A B, Troiano A R. Trans AIME, 1940; 140: 307 [24] Greninger A B, Troiano A R. Trans AIME, 1949; 185: 590 [25] Otte H M, Read T A. Trans AIME, 1957; 209: 412 [26] Johnson K A, Wayman C M. Acta Crystallogr, 1963; 16: 480 [27] Read R P. Acta Metall, 1962; 10: 865 [28] Moritani T, Miyajima N, Furuhara T, Maki T. Scr Mater, 2002; 47: 193 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|