流动海水中多重应力耦合作用下B10 Cu-Ni合金的微观结构演变与动态失效机制
李瑞雪1, 周晨曦1, 杨慧敏1, 雍兴跃2(), 刘景军1()
1 北京化工大学 材料科学与工程学院 北京 100029
2 北京化工大学 化学工程学院 北京 100029
Microstructural Evolution and Dynamic Failure Mechanism of B10 Cu-Ni Alloy Under Multiple Stress Coupling in Flowing Seawater
LI Ruixue1, ZHOU Chenxi1, YANG Huimin1, YONG Xingyue2(), LIU Jingjun1()
1 School of Materials Science and Engineering, Beijing University of Chemical Technology, Beijing 100029, China
2 School of Chemical Engineering, Beijing University of Chemical Technology, Beijing 100029, China
引用本文:

李瑞雪, 周晨曦, 杨慧敏, 雍兴跃, 刘景军. 流动海水中多重应力耦合作用下B10 Cu-Ni合金的微观结构演变与动态失效机制[J]. 金属学报, 2026, 62(7): 1273-1287.
Ruixue LI, Chenxi ZHOU, Huimin YANG, Xingyue YONG, Jingjun LIU. Microstructural Evolution and Dynamic Failure Mechanism of B10 Cu-Ni Alloy Under Multiple Stress Coupling in Flowing Seawater[J]. Acta Metall Sin, 2026, 62(7): 1273-1287.

全文: PDF(5218 KB)   HTML
摘要: 

针对Cu-Ni合金在流动海水中承受多重应力耦合作用时易发生微观结构劣化与动态失效的关键问题,本工作以管路系统广泛应用的B10 Cu-Ni合金为研究对象,研究了其在复杂服役环境下的微观结构演变规律与动态失效特征。采用实验与模拟计算相结合的研究策略,通过分子动力学(MD)方法构建了合金/海水溶剂化模型,重点研究了海水流速、压力及其耦合作用对B10 Cu-Ni合金微观结构演变及其腐蚀动力学过程的影响机制。结果表明,Cu-Ni合金的腐蚀过程受多步耦合的Cu原子迁移-溶解能垒控制。基于密度泛函理论(DFT)的计算分析表明,随着海水压力从0.1 MPa增至12 MPa,迁移-溶解能垒由1.76 eV降至1.54 eV,腐蚀速率显著提升。此外,随着海水流速的增加,合金(111)晶面产生原子级轴向弹性拉伸应变,迁移-溶解能垒进一步降低,存在使腐蚀加剧的临界流速(4 m/s)。在海水流速与压力耦合作用下,迁移-溶解能垒进一步减小,功函数降低,腐蚀动力学过程显著加快。模拟计算所得的腐蚀速率常数与实测腐蚀速率的变化趋势基本一致,有效实现了对B10 Cu-Ni合金在实际工况环境下动态失效过程中腐蚀倾向的评估与预测。

关键词 : B10 Cu-Ni合金,  流动海水,  微观结构,  流体力学,  腐蚀动力学    
Abstract:

To address the critical issue of microstructural degradation and dynamic failure of Cu-Ni alloys subjected to multiple stress couplings in flowing seawater, this study systematically investigates the microstructural evolution and failure characteristics of the alloy in a complex service environment. Focusing on the widely used B10 Cu-Ni alloy in pipeline systems, a combined experimental and computational simulation approach was employed. A molecular dynamics method was used to construct an alloy/seawater solvation model, with emphasis on the effects of seawater flow rate, pressure, and their coupled interactions on microstructural evolution and corrosion kinetics. In flowing seawater, the strain level of the alloy increases markedly, accompanied by a rise in microstructural defects. The results reveal that corrosion of Cu-Ni alloys proceeds through a multi-step coupled mechanism governed by the migration-dissolution energy barrier of Cu atoms. Density functional theory calculations show that as seawater pressure increases from 0.1 MPa to 12 MPa, the migration-dissolution energy barrier decreases from 1.76 eV to 1.54 eV, significantly accelerating the corrosion rate. Furthermore, increasing seawater flow rate induces atomic-level axial elastic tensile strain on the (111) crystal plane of the alloy, further reducing the migration-dissolution energy barrier. A critical flow rate of 4 m/s has been identified as exacerbating corrosion. Under the coupled influence of flow rate and pressure, the migration-dissolution energy barrier is further reduced, the work function decreases, and corrosion kinetics are significantly accelerated. The corrosion rate constants obtained from simulations exhibit highly consistent trends with experimentally measured corrosion rates, enabling reliable assessment and prediction of the corrosion tendency of the B10 Cu-Ni alloy during dynamic failure under real operational conditions.

Key words: B10 Cu-Ni alloy    flowing seawater    microstructure    fluid dynamics    corrosion kinetics
收稿日期: 2024-09-11     
ZTFLH:  TG178  
通讯作者: 刘景军,liujingjun@mail.buct.edu.cn,主要从事金属材料微观结构与性能强化研究;
雍兴跃,yongxy@mail.buct.edu.cn,主要从事流动海水腐蚀与防护研究
作者简介: 李瑞雪,女,1998年生,博士生
图1  B10 Cu-Ni合金的结构表征及EDS分析
图2  B10 Cu-Ni合金不同晶面的快速Fourier变换(FFT)、逆快速Fourier变换(IFFT)及应变水平分析
图3  B10合金稳定结构模型的建立及迁移-溶解动力学过程分析
图4  不同海水压力下(海水流速为0) B10合金腐蚀10 h前后的SEM像、XRD谱、(111)晶面的微应变及位错密度
图5  不同海水压力下B10seg合金/海水界面溶剂化模型的建立,合金表面H2O分子的密度分布,模拟不同压力下H2O分子对合金中表面原子溶解影响的示意图模型,合金的表面能和功函数,海水压力对Helmboltz层影响的示意图,压力作用下原子的迁移-溶解过程及腐蚀速率常数与质量损失的对比
图6  常压条件下海水流速为1~5 m/s时B10合金表面腐蚀形貌的SEM像,XRD谱,(111)晶面的微应变和位错密度;B10seg合金的迁移-溶解过程,腐蚀速率常数与质量损失对比及腐蚀动力学参数分析
图7  4.0 MPa压力条件下,海水流速为1~5 m/s时B10seg合金的迁移-溶解过程,腐蚀速率常数与质量损失的对比;单一压力(4.0 MPa、0 m/s)/流速(0.1 MPa、4 m/s)及耦合因素(4.0 MPa、4 m/s)作用时B10合金表面腐蚀形貌的SEM像、XRD谱及(111)晶面的微应变和位错密度分析
图8  压力(4.0 MPa、0 m/s)/流速(0.1 MPa、4 m/s)单一因素与耦合因素作用(4.0 MPa、4 m/s)条件下B10seg合金的迁移-溶解过程、腐蚀动力学参数及电荷密度分布
图9  深海动态环境下B10 Cu-Ni合金的迁移-溶解动力学机制示意图
[1] Lin L Y, Liu S F, Liu Z C, et al. Surface and interface characteristics of Cu-Ni alloy corroded in seawater [J]. Corros. Sci. Prot. Technol., 1999, 11(1): 37
[1] 林乐耘, 刘少峰, 刘增才 等. 铜镍合金海水腐蚀的表面与界面特征研究 [J]. 腐蚀科学与防护技术, 1999, 11(1): 37
[2] Xia Q Q, Zhu T. Analysis and thinking of B10 material standard of ship sea pipeline [J]. Ship Stand. Eng., 2018, 51(4): 15
[2] 夏齐强, 朱 韬. 舰船海水管路B10材料标准分析与思考 [J]. 船舶标准化工程师, 2018, 51(4): 15
[3] Luo X, Xin X, Li Y, et al. Progress on corrosion and repair technology of marine seawater pipe [J]. China Elastom., 2022, 32(1): 80
[3] 罗 旭, 辛 颉, 李 瑜 等. 船舶海水管路腐蚀及修复技术研究进展 [J]. 弹性体, 2022, 32(1): 80
[4] Zhang Z Q, Guo Z L, Lei Z F. Applications of copper alloy in shipbuilding [J]. Dev. Appl. Mater., 2006, 21(5): 43
[4] 张智强, 郭泽亮, 雷竹芳. 铜合金在舰船上的应用 [J]. 材料开发与应用, 2006, 21(5): 43
[5] Tian F, Bai X Q, He X Y, et al. Research progress on microbiological induced corrosion of metallic materials under ocean environment [J]. Surf. Technol., 2018, 47(8): 182
[5] 田 丰, 白秀琴, 贺小燕 等. 海洋环境下金属材料微生物腐蚀研究进展 [J]. 表面技术, 2018, 47(8): 182
[6] Stack M M, Corlett N, Turgoose S. Some thoughts on modelling the effects of oxygen and particle concentration on the erosion-corrosion of steels in aqueous slurries [J]. Wear, 2003, 255: 225
doi: 10.1016/S0043-1648(03)00205-9
[7] Xu Y. Numerical simulation study on erosion-corrosion induced by liquid-solid two-phase flow [D]. Beijing: Beijing University of Chemical Technology, 2001
[7] 徐 姚. 液固两相流冲刷腐蚀数值模拟研究 [D]. 北京: 北京化工大学, 2001
[8] Leon A, Levy G K, Ron T, et al. The effect of strain rate on stress corrosion performance of Ti6Al4V alloy produced by additive manufacturing process [J]. J. Mater. Res. Technol., 2020, 9: 4097
doi: 10.1016/j.jmrt.2020.02.035
[9] Ren P W. Study of tribocorrosion of three different corrosion reisistance materials under deep-sea high pressure [D]. Beijing: University of Science and Technology Beijing, 2022
[9] 任鹏伟. 三类不同耐蚀性材料在深海高压下的磨蚀研究 [D]. 北京: 北京科技大学, 2022
[10] Liu R, Xie Y S, Jin Y, et al. Stress corrosion cracking of the titanium alloys under hydrostatic pressure resulting from the degradation of passive films [J]. Acta Mater., 2023, 252: 118946
doi: 10.1016/j.actamat.2023.118946
[11] Dai J W, Zhang X G, Zhang L, et al. In vitro corrosion behavior of biodegradable WE43 alloy under various physiological flow velocities [J]. J. Mater. Sci., 2024, 59: 7854
doi: 10.1007/s10853-024-09617-1
[12] Du J, Wang H R, Du M, et al. Electrochemical corrosion behavior of 90/10 Cu-Ni alloy in flowing seawater [J]. Corros. Sci. Prot. Technol., 2008, 20: 12
[12] 杜 娟, 王洪仁, 杜 敏 等. B10铜镍合金流动海水冲刷腐蚀电化学行为 [J]. 腐蚀科学与防护技术, 2008, 20: 12
[13] Li X M, Zhang Y M, Guo X H, et al. Erosion corrosion behavior of copper-nickel alloy pipe in flowing seawater [J]. J. Henan Univ. Sci. Technol. (Nat. Sci.), 2017, 38(3): 10
[13] 李晓孟, 张彦敏, 国秀花 等. 流动海水中铜镍合金管材的冲刷腐蚀行为 [J]. 河南科技大学学报(自然科学版), 2017, 38(3): 10
[14] Islam M A, Farhat Z N, Ahmed E M, et al. Erosion enhanced corrosion and corrosion enhanced erosion of API X-70 pipeline steel [J]. Wear, 2013, 302: 1592
doi: 10.1016/j.wear.2013.01.041
[15] Ren P W. Study on erosion-corrosion behavior of X70 steel in simulated deep sea environment [D]. Nanning: Guangxi University, 2023
[15] 任鹏炜. X70钢在模拟深海环境下的冲刷腐蚀行为研究 [D]. 南宁: 广西大学, 2023
[16] Yuan S J, Pehkonen S O. Surface characterization and corrosion behavior of 70/30 Cu-Ni alloy in pristine and sulfide-containing simulated seawater [J]. Corros. Sci., 2007, 49: 1276
doi: 10.1016/j.corsci.2006.07.003
[17] Zhang R W. Effect of iron and manganese on corrosion resistance of B10 copper-nickel alloy and its mechanism [D]. Ganzhou: Jiangxi University of Science and Technology, 2019
[17] 张荣伟. 铁、锰对B10白铜合金耐蚀性能的影响及机理研究 [D]. 赣州: 江西理工大学, 2019
[18] Wang Y Q, Shao Y W, Meng G Z, et al. Study on passivating treatment of Cu-Ni alloy in compound passivant containing benzotriazole [J]. Acta Metall. Sin., 2012, 48: 744
doi: 10.3724/SP.J.1037.2012.00032
[18] 王艳秋, 邵亚薇, 孟国哲 等. Cu-Ni合金BTA复配体系钝化处理工艺研究 [J]. 金属学报, 2012, 48: 744
doi: 10.3724/SP.J.1037.2012.00032
[19] Aigbodion V S, Ozor P O, Eke M N, et al. Explicit microstructure, corrosion, and stress analysis of value-added Al-3.7%Cu-1.4%Mg/1.5% rice husk ash nanoparticles for pump impeller application [J]. Chem. Data Collect., 2021, 33: 100675
doi: 10.1016/j.cdc.2021.100675
[20] Yan Y J, Huang J, Pan L, et al. A comparative study of methods for calculating the dislocation density in GaN-on-Si epitaxial wafers [J]. Micromachines, 2024, 15: 954
doi: 10.3390/mi15080954
[21] Zak A K, Majid W H A, Abrishami M E, et al. X-ray analysis of ZnO nanoparticles by Williamson-Hall and size-strain plot methods [J]. Solid State Sci., 2011, 13: 251
doi: 10.1016/j.solidstatesciences.2010.11.024
[22] Delley B. An all-electron numerical method for solving the local density functional for polyatomic molecules [J]. J. Chem. Phys., 1990, 92: 508
[23] Chen Z M, Jin C, Ji X Y, et al. Atomistic understanding of Pt-based medium entropy alloys for oxygen reduction electrocatalysis based on first principles [J]. Int. J. Hydrogen Energy, 2023, 48: 160
doi: 10.1016/j.ijhydene.2022.09.247
[24] Baker M D, Baker A D, Belanger J, et al. Linear relationship between weighted-average madelung constants and density functional theory energies for MgO nanotubes [J]. J. Phys. Chem., 2012, 116C: 25588
[25] Luo Z L, Gao W, Jiang Q. Determinants of vacancy formation and migration in high-entropy alloys [J]. Sci. Adv., 2025, 11: eadr4697
doi: 10.1126/sciadv.adr4697
[26] Schultz P A. First-principles calculations of metal surfaces. I. Slab-consistent bulk reference for convergent surface properties [J]. Phys. Rev., 2021, 103B: 195426
[27] Canneaux S, Bohr F, Henon E. KiSThelP: A program to predict thermodynamic properties and rate constants from quantum chemistry results [J]. J. Comput. Chem., 2014, 35: 82
pmid: 24190715
[28] Halgren T A, Lipscomb W N. The synchronous-transit method for determining reaction pathways and locating molecular transition states [J]. Chem. Phys. Lett., 1977, 49: 225
doi: 10.1016/0009-2614(77)80574-5
[29] Zhang W Q, Han S J, Zhang D W, et al. Variations in dissolved oxygen and aquatic biological responses in China’s coastal seas [J]. Environ. Res., 2023, 223: 115418
doi: 10.1016/j.envres.2023.115418
[30] Jarvis B M, Greene R M, Wan Y S, et al. Contiguous low oxygen waters between the continental shelf hypoxia zone and nearshore coastal waters of Louisiana, USA: Interpreting 30 years of profiling data and three-dimensional ecosystem modeling [J]. Environ. Sci. Technol., 2021, 55: 4709
doi: 10.1021/acs.est.0c05973
[31] Rouf M A, Islam M J, Roknuzzaman M, et al. Vertical profile of dissolved oxygen and associated water variables in the Pasur-Rupsha estuary of Bangladesh [J]. Heliyon, 2022, 8: e10935
doi: 10.1016/j.heliyon.2022.e10935
[32] Li B, Zhang L, Yan T Y, et al. Effects of heat treatment processes and W wire properties on residual stress in W wire reinforced Zr-based metallic glass composites [J]. Acta Metall. Sin., 2024, 60: 1055
doi: 10.11900/0412.1961.2024.00066
[32] 李 彪, 张 龙, 颜廷毅 等. 热处理工艺和W丝特性对W丝增强锆基非晶复合材料残余应力的影响 [J]. 金属学报, 2024, 60: 1055
[33] Chakrahari K K, Liao J H, Kahlal S, et al. [Cu13{S2CN n Bu2}6-(acetylide)4]+: A two-electron superatom [J]. Angew. Chem. Int. Ed., 2016, 55: 14704
doi: 10.1002/anie.v55.47
[34] Zhang J M, Ma F, Xu K W. Calculation of the surface energy of FCC metals with modified embedded-atom method [J]. Appl. Surf. Sci., 2004, 229: 34
doi: 10.1016/j.apsusc.2003.09.050
[35] Han Y, Lai K C, Lii-Rosales A, et al. Surface energies, adhesion energies, and exfoliation energies relevant to copper-graphene and copper-graphite systems [J]. Surf. Sci., 2019, 685: 48
doi: 10.1016/j.susc.2019.01.009
[36] Deng J, Wang C, Guan G Z, et al. The deformations of carbon nanotubes under cutting [J]. ACS Nano, 2017, 11: 8464
doi: 10.1021/acsnano.7b04130 pmid: 28767215
[37] Davis H L, Faulkner J S, Joy H W. Calculation of the band structure for copper as a function of lattice spacing [J]. Phys. Rev., 1968, 167: 601
doi: 10.1103/PhysRev.167.601
[38] Zhu J, Li Z, Yang S T, et al. Characterization of strain field distribution in carbon fiber reinforced resin matrix composites using electron beam moiré and geometric phase analysis [J]. Opt. Lasers Eng., 2023, 163: 107457
doi: 10.1016/j.optlaseng.2022.107457
[39] Meng Z K, Meng Z C, Gao C Y, et al. Molecular dynamics simulation of creep mechanism in nanocrystalline α-zirconium under various conditions [J]. Acta Metall. Sin., 2024, 60: 699
[39] 孟子凯, 孟智超, 高长源 等. 不同条件下纳米晶α-Zr蠕变行为的分子动力学模拟 [J]. 金属学报, 2024, 60: 699
doi: 10.11900/0412.1961.2022.00444
[40] Yi X N, Ma A L, Zhang L M, et al. Crystallographic anisotropy of corrosion rate and surface faceting of polycrystalline 90Cu-10Ni in acidic NaCl solution [J]. Mater. Des., 2022, 215: 110429
doi: 10.1016/j.matdes.2022.110429
[41] Yi X N, Zhang L J, Ma A L, et al. Study on anisotropic oxide formation rate in the initial corrosion stage of 90Cu-10Ni alloy in alkaline NaCl solution by experiments and first-principles calculation [J]. Corros. Sci., 2022, 209: 110768
doi: 10.1016/j.corsci.2022.110768
[42] Kong M, Wu J J, Han T R, et al. Corrosion mechanism of T1 phase in Al-Cu-Li alloy: First-principles calculations [J]. Acta Phys. Sin., 2020, 69: 027101
[42] 孔 敏, 吴静静, 韩天茹 等. 第一性原理研究Al-Cu-Li合金中T1相的腐蚀机理 [J]. 物理学报, 2020, 69: 027101
[43] Shin D Y, Lim D H. DFT approach for predicting the pH-potential-dependent durabilities of Pt-skinned Pt-M (M = Ni, Co, and Ir) alloys for fuel cell cathodes [J]. Appl. Surf. Sci., 2023, 616: 156449
doi: 10.1016/j.apsusc.2023.156449
[44] Hu S B, Liu L, Cui Y, et al. Influence of hydrostatic pressure on the corrosion behavior of 90/10 copper-nickel alloy tube under alternating dry and wet condition [J]. Corros. Sci., 2019, 146: 202
doi: 10.1016/j.corsci.2018.10.036
[45] Oktavian R, Taha M, Lee M J. Experimental and computational study of CO2 storage and sequestration with aqueous 2-amino-2-hydroxymethyl-1,3-propanediol (TRIS) solutions [J]. J. Phys. Chem., 2014, 118A: 11572
[46] Liu B Y, Xi H X, Li Z, et al. Adsorption and corrosion-inhibiting effect of 2-(2-{[2-(4-Pyridylcarbonyl)hydrazono]methyl}phenoxy)acetic acid on mild steel surface in seawater [J]. Appl. Surf. Sci., 2012, 258: 6679
doi: 10.1016/j.apsusc.2012.03.115
[47] Liu R, Cui Y, Liu L, et al. Study on the mechanism of hydrostatic pressure promoting electrochemical corrosion of pure iron in 3.5% NaCl solution [J]. Acta Mater., 2021, 203: 116467
doi: 10.1016/j.actamat.2020.11.009
[48] Du J. Erosion-corrosion behavior of copper and 90/10 Cu-Ni alloy in flowing seawater [D]. Qingdao: Ocean University of China, 2007
[48] 杜 娟. TUP紫铜及B10铜镍合金流动海水冲刷腐蚀行为研究 [D]. 青岛: 中国海洋大学, 2007
[49] Yi X N, Ma A L, Zheng Y G, et al. Elucidating different selective corrosion behavior of two typical marine aluminum bronze alloys from the perspective of constituent phases [J]. Corros. Sci., 2024, 235: 112167
doi: 10.1016/j.corsci.2024.112167
[50] Tan Z W, Yang L Y, Zhang D L, et al. Development mechanism of internal local corrosion of X80 pipeline steel [J]. J. Mater. Sci. Technol., 2020, 49: 186
doi: 10.1016/j.jmst.2019.10.023
[51] Yang L Y, Zhang D L, Fan H M, et al. In-situ electrochemical testing and fluid dynamics simulation of pipeline defects under flow accelerated corrosion [J]. Exp. Therm. Fluid Sci., 2024, 150: 111048
doi: 10.1016/j.expthermflusci.2023.111048
[52] Liu Q, Zhao W N, Ao Z M, et al. Photo-piezoelectric synergistic degradation of typical volatile organic compounds on BaTiO3 [J]. Chin. Chem. Lett., 2022, 33: 410
doi: 10.1016/j.cclet.2021.06.059
[1] 朱思瑛, 易敏, 郭万林. 金属材料晶界结构的拓扑性质与表征[J]. 金属学报, 2026, 62(5): 705-720.
[2] 王启勇, 李晓博, 刘小超, 王心成, 张泰瑞, 倪中华, 陈彪. 低碳钢预制涡流搅拌摩擦焊工艺研究[J]. 金属学报, 2026, 62(1): 217-234.
[3] 赵今涛, 孙利芳, 何竹风, 刘玉杰, 马小柏, 申勇峰, 贾楠. 基于深冷轧制备的高强韧高氮奥氏体不锈钢的力学行为[J]. 金属学报, 2025, 61(12): 1884-1894.
[4] 刘仲武, 周帮, 廖雪峰, 何家毅. 全高丰度稀土(Ce, La, Y)-Fe-B永磁的研究现状和未来发展[J]. 金属学报, 2024, 60(5): 585-604.
[5] 王郑, 王振玉, 汪爱英, 杨巍, 柯培玲. 微弧氧化时间对锆合金表面MAO/Cr复合涂层结构与性能的影响[J]. 金属学报, 2024, 60(5): 691-698.
[6] 杜银, 李涛, 裴旭辉, 周青, 王海丰. TiZrHfCuBe高熵非晶合金的纳米划痕力学行为[J]. 金属学报, 2024, 60(11): 1451-1460.
[7] 张德印, 郝旭, 贾宝瑞, 吴昊阳, 秦明礼, 曲选辉. Y2O3 含量对燃烧合成Fe-Y2O3 纳米复合粉末性能的影响[J]. 金属学报, 2023, 59(6): 757-766.
[8] 刘满平, 薛周磊, 彭振, 陈昱林, 丁立鹏, 贾志宏. 后时效对超细晶6061铝合金微观结构与力学性能的影响[J]. 金属学报, 2023, 59(5): 657-667.
[9] 杨超, 卢海洲, 马宏伟, 蔡潍锶. 选区激光熔化NiTi形状记忆合金研究进展[J]. 金属学报, 2023, 59(1): 55-74.
[10] 解磊鹏, 孙文瑶, 陈明辉, 王金龙, 王福会. 制备工艺对FGH4097高温合金微观组织与性能的影响[J]. 金属学报, 2022, 58(8): 992-1002.
[11] 李金富, 李伟. 铝基非晶合金的结构与非晶形成能力[J]. 金属学报, 2022, 58(4): 457-472.
[12] 张显程, 张勇, 李晓, 王梓萌, 贺琛贇, 陆体文, 王晓坤, 贾云飞, 涂善东. 异构金属材料的设计与制造[J]. 金属学报, 2022, 58(11): 1399-1415.
[13] 马敏静, 屈银虎, 王哲, 王军, 杜丹. Ag-CuO触点材料侵蚀过程的演化动力学及力学性能[J]. 金属学报, 2022, 58(10): 1305-1315.
[14] 王洪伟, 何竹风, 贾楠. 非均匀组织FeMnCoCr高熵合金的微观结构和力学性能[J]. 金属学报, 2021, 57(5): 632-640.
[15] 潘杰, 段峰辉. 非晶合金的回春行为[J]. 金属学报, 2021, 57(4): 439-452.