Please wait a minute...
金属学报  2026, Vol. 62 Issue (7): 1288-1296    DOI: 10.11900/0412.1961.2024.00304
  研究论文 本期目录 | 过刊浏览 |
钢包静置过程夹杂物去除的工业试验与数值模拟
段豪剑1, 谢忠研1, 李占魁1, 徐学军1, 黄财德2, 温瀚2, 张立峰3()
1 北京科技大学 冶金与生态工程学院 北京 100083
2 首钢京唐钢铁联合有限责任公司 炼钢部 唐山 063200
3 北方工业大学 机械与材料工程学院 北京 100144
Industrial Trial and Numerical Simulation of Inclusion Removal During Ladle Holding Period
DUAN Haojian1, XIE Zhongyan1, LI Zhankui1, XU Xuejun1, HUANG Caide2, WEN Han2, ZHANG Lifeng3()
1 School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China
2 Steelmaking Department, Shougang Jingtang United Iron and Steel Co. Ltd., Tangshan 063200, China
3 School of Mechanical and Materials Engineering, North China University of Technology, Beijing 100144, China
引用本文:

段豪剑, 谢忠研, 李占魁, 徐学军, 黄财德, 温瀚, 张立峰. 钢包静置过程夹杂物去除的工业试验与数值模拟[J]. 金属学报, 2026, 62(7): 1288-1296.
Haojian DUAN, Zhongyan XIE, Zhankui LI, Xuejun XU, Caide HUANG, Han WEN, Lifeng ZHANG. Industrial Trial and Numerical Simulation of Inclusion Removal During Ladle Holding Period[J]. Acta Metall Sin, 2026, 62(7): 1288-1296.

全文: PDF(3244 KB)   HTML
摘要: 

在高品质钢的生产过程中,二次精炼的最后阶段通常是钢包静置过程,以促进夹杂物的上浮去除,从而提高钢液的洁净度。本工作首先通过工业试验调研了钢包吹氩密封成分调整(CAS)精炼生产商用热轧低碳钢(SPHC低碳钢)时,钢包静置过程中夹杂物数密度和面积分数的演变。随后采用离散相模型建立了钢包静置过程中夹杂物运动和去除的数值模型。实验结果表明,随着静置时间的增加,夹杂物逐渐上浮并被去除,其数密度和面积分数分别从静置开始时的52.8 mm-2和279 × 10-6下降至静置15 min后的22.1 mm-2和148 × 10-6。计算结果表明,在钢包静置过程中,直径小于10 μm的夹杂物主要跟随钢液流动,钢包静置900和1800 s后的夹杂物去除率分别为51.6%和66.7%;直径为100 μm夹杂物的运动受到钢液流动和自身上浮的双重作用,钢包静置900和1800 s后其去除率分别为70.2%和89.2%;直径为1000 μm的夹杂物主要是自身上浮运动,在钢包静置120 s后其去除率已接近100%。

关键词 : 钢包静置过程,  夹杂物,  工业试验,  数值模拟    
Abstract:

In high-quality steel production, the final stage of secondary refining typically involves a ladle holding period to facilitate the flotation and removal of inclusions. This improves the cleanliness of the molten steel. This study investigated the evolution of inclusion number density and area fraction during the ladle holding period by conducting industrial trial on composition adjustment via the sealed argon bubbling refining process of steel plate hot rolled commercial (SPHC) low-carbon steel. The results indicated that inclusions would be removed by floating during the ladle holding period. The inclusion number density and area fraction decreased from 52.8 mm-2 and 279 × 10-6 at the start of the holding period to 22.1 mm-2 and 148 × 10-6 after 15 min, respectively. To clarify the movement and removal of inclusions, a numerical model was developed based on a discrete phase model, incorporating multiphase flow and heat transfer during the ladle holding period. The calculations revealed the following conclusions: (1) inclusions smaller than 10 μm primarily followed the molten steel's fluid flow, with removal rates of 51.6% and 66.7% after 900 and 1800 s, respectively; (2) inclusions with a diameter of 100 μm were influenced by the molten steel's fluid flow and their buoyancy, achieving removal rates of 70.2% and 89.2% after 900 and 1800 s, respectively; (3) inclusions with a diameter of 1000 μm primarily underwent self-floating, reaching an approximately 100% removal rate after 120 s.

Key words: ladle holding period    inclusion    industrial experiment    numerical simulation
收稿日期: 2024-09-03     
ZTFLH:  TF769  
基金资助:国家重点研发计划项目(2023YFB3709900);国家自然科学基金项目(U22A20171);国家自然科学基金项目(52474341)
通讯作者: 张立峰,zhanglifeng@ncut.edu.cn,主要从事洁净钢与非金属夹杂物研究
Corresponding author: ZHANG Lifeng, professor, Tel: (010)88801689, E-mail: zhanglifeng@ncut.edu.cn
作者简介: 段豪剑,男,1990年生,博士
图1  钢包吹氩密封成分调整(CAS)精炼的工艺操作和取样记录示意图
图2  钢包静置过程钢中夹杂物数密度和面积分数的演变
图3  钢包静置过程钢液中总O含量的演变
图4  钢包静置过程中夹杂物形貌演变的SEM像
图5  钢包静置过程中夹杂物在钢液中的初始位置分布
图6  钢包静置过程中直径为1 μm的夹杂物在钢液中的运动和去除
图7  钢包静置过程中直径为10 μm的夹杂物在钢液中的运动和去除
图8  钢包静置过程中直径为100 μm的夹杂物在钢液中的运动和去除
图9  钢包静置过程中直径为1000 μm的夹杂物在钢液中的运动和去除
图10  钢包静置过程中钢液平均流速和夹杂物上浮速率的对比
图11  由工业试验测量的钢包静置过程中钢液的总O含量、夹杂物数密度以及基于夹杂物面积分数计算得到的夹杂物去除率
[1] Zhang L F, Thomas B G. State of the art in evaluation and control of steel cleanliness [J]. ISIJ Int., 2003, 43: 271
doi: 10.2355/isijinternational.43.271
[2] Zhang L F. Nucleation, growth, transport, and entrapment of inclusions during steel casting [J]. JOM, 2013, 65: 1138
doi: 10.1007/s11837-013-0688-y
[3] Zhang L F, Ren Q, Duan H J, et al. Modelling of non-metallic inclusions in steel [J]. Min. Proc. Ext. Metall., 2020, 129: 184
[4] Zhang L F. Non-Metallic Inclusions in Steel: Fundmentals [M]. Beijing: Metallurgical Industry Press, 2019: 1
[4] 张立峰. 钢中非金属夹杂物 [M]. 北京: 冶金工业出版社, 2019: 1
[5] Zhang L F. Non-Metallic Inclusions in Steel: Industrial Practice [M]. Beijing: Metallurgical Industry Press, 2019: 1
[5] 张立峰. 钢中非金属夹杂物: 工业实践 [M]. 北京: 冶金工业出版社, 2019: 1
[6] Ilegbusi O J, Szekely J. Melt stratification in ladles [J]. ISIJ Int., 1987, 27: 563
doi: 10.2355/isijinternational1966.27.563
[7] Austin P R, Camplin J M, Herbertson J, et al. Mathematical modelling of thermal stratification and drainage of steel ladles [J]. ISIJ Int., 1992, 32: 196
doi: 10.2355/isijinternational.32.196
[8] Chakraborty S, Sahai Y. Effect of holding time and surface cover in ladles on liquid steel flow in continuous casting tundishes [J]. Metall. Trans., 1992, 23B: 153
[9] Chakraborty S, Sahai Y. Effect of slag cover on heat loss and liquid steel flow in ladles before and during teeming to a continuous casting tundish [J]. Metall. Trans., 1992, 23B: 135
[10] Olika B, Pan Y H, Björkman B, et al. Numerical simulation and industrial investigation on the melt stratification phenomena in ladles holding molten steel [J]. Scand. J. of Metall., 1996, 25(1): 18
[11] Grip C E, Jonsson L, Jönsson P, et al. Numerical prediction and experimental verification of thermal stratification during holding in pilot plant and production ladles [J]. ISIJ Int., 1999, 39: 715
doi: 10.2355/isijinternational.39.715
[12] Xia J L, Ahokainen T. Transient flow and heat transfer in a steelmaking ladle during the holding period [J]. Metall. Mater. Trans., 2001, 32B: 733
[13] Xia J L, Ahokainen T. Thermal stratification in a steel ladle [J]. Can. Metall. Quart., 2001, 40: 479
doi: 10.1179/cmq.2001.40.4.479
[14] Pan Y H, Björkman B. Numerical analysis on the similarity between steel ladles and hot-water models regarding natural convection phenomena [J]. ISIJ Int., 2002, 42: 53
doi: 10.2355/isijinternational.42.53
[15] Pan Y H, Björkman B. Physical and mathematical modelling of thermal stratification phenomena in steel ladles [J]. ISIJ Int., 2002, 42: 614
doi: 10.2355/isijinternational.42.614
[16] Pan Y H, Grip C E, Björkman B. Numerical studies on the parameters influencing steel ladle heat loss rate, thermal stratification during holding and steel stream temperature during teeming [J]. Scand. J. Metall., 2003, 32: 71
doi: 10.1034/j.1600-0692.2003.10608.x
[17] Zhang C J, Wang A, Li Q X, et al. Analysis of temperture drop during 80 t ladle standing [J]. Henan Metall., 2013, 21: 20
[17] 张彩军, 王 昂, 李庆效 等. 80 t钢包静置过程温降分析 [J]. 河南冶金, 2013, 21: 20
[18] Lu B Y, Meng X N, Zhu M Y. Numerical analysis for the heat transfer behavior of steel ladle as the thermoelectric waste-heat source [J]. Catal. Today, 2018, 318: 180
doi: 10.1016/j.cattod.2017.10.038
[19] Duan H J, Ren Y, Zhang L F. Fluid flow, thermal stratification, and inclusion motion during holding period in steel ladles [J]. Metall. Mater. Trans., 2019, 50B: 1476
[20] Gopala Krishna E D, Shamshoddin S, Ande R. Numerical simulation of fluid flow and heat transfer in a ductile iron ladle during holding and teeming [J]. J. Thermal. Sci. Eng. Appl., 2019, 11: 011007
[21] Yan H, Conejo A N, Zhang H, et al. Numerical simulation of heat transfer during ladle holding period [J]. Cont. Cast., 2022, (1): 31
[21] 颜 晗, Conejo A N, 张 晗 等. 钢包静置过程中传热现象的数值模拟 [J]. 连铸, 2022, (1): 31
[22] Huang C D, Duan H J, Zhang L F. Modeling of motion of inclusions in argon-stirred steel ladles [J]. Steel Res. Int., 2024, 95: 2300537
doi: 10.1002/srin.v95.11
[23] Morsi S A, Alexander A J. An investigation of particle trajectories in two-phase flow systems [J]. J. Fluid Mech., 1972, 55: 193
doi: 10.1017/S0022112072001806
[24] Pearson K. The problem of the random walk [J]. Nature, 1905, 72: 294
[25] Duan H J, Huang C D, Zhang L F. Numerical simulation of transient flow and heat transfer in a steel ladle during holding period [J]. Metall. Mater. Trans., 2024, 55B: 2273
[26] Duan H J, Ren Y, Zhang L F. Effects of interphase forces on fluid flow in gas-stirred steel ladles using the Eulerian-Lagrangian multiphase approach [J]. JOM, 2018, 70: 2128
doi: 10.1007/s11837-018-3045-3
[27] Duan H J, Zhang L F, Thomas B G, et al. Fluid flow, dissolution, and mixing phenomena in argon-stirred steel ladles [J]. Metall. Mater. Trans., 2018, 49B: 2722
[1] 董洪标, 郝文硕. 综述:定向凝固枝晶生长的数值模拟[J]. 金属学报, 2026, 62(5): 756-769.
[2] 梁雨雨, 倪培远, 刘麒麟, 厉英. 稀土合金化石油套管钢精炼-连铸-轧制过程夹杂物演变行为[J]. 金属学报, 2026, 62(4): 611-626.
[3] 贾玉亮, 张勇佳, 史泽楷, 沈旭, 殷亚军, 施长坤, 周建新, 吕志刚. 高温合金定向凝固雀斑形成机理及控制技术研究进展[J]. 金属学报, 2026, 62(2): 309-327.
[4] 韩鸿华, 史清宇, 杨诚乐, 孔德帅, 陈高强. 铝合金搅拌摩擦焊热-力-流耦合仿真及材料迁移轨迹解析[J]. 金属学报, 2026, 62(1): 148-158.
[5] 瞿铁, 谢杨, 王重阳, 李利霞, 徐侠剑, 毛峙溆, 骆文泽, 黄智泉, 邓德安. 34CrNi1Mo/Q355B异种钢对接接头残余应力及焊后热处理对残余应力的影响[J]. 金属学报, 2026, 62(1): 203-216.
[6] 王博辰, 任英, 邝霜, 单庆林, 潘宏伟, 路博勋, 石晓伟, 王举金, 张立峰. 铝脱氧钢与CaO-MgO-Al2O3 精炼渣反应动力学研究[J]. 金属学报, 2025, 61(9): 1335-1343.
[7] 邹建新, 张嘉祺, 赵颖燕, 林羲, 丁文江. 高容量镁基储氢合金材料研究与应用进展[J]. 金属学报, 2025, 61(3): 420-436.
[8] 徐涛, 邓安元, 李阳, 王恩刚. 连铸结晶器内Ar气泡破碎-聚合和捕获行为的数值模拟[J]. 金属学报, 2025, 61(12): 1895-1910.
[9] 段生朝, 刘珍童, 康君, 白乘风, 文健, 刘刚, 张立峰. 综述:中间包钢液二次氧化对钢中非金属夹杂物的影响[J]. 金属学报, 2025, 61(10): 1485-1501.
[10] 李俊杰, 李盼悦, 黄立清, 郭杰, 吴京洋, 樊凯, 王锦程. 真空自耗电弧熔炼铸锭凝固行为多尺度模拟研究进展[J]. 金属学报, 2025, 61(1): 12-28.
[11] 余东, 马威龙, 王亚莉, 王锦程. Au-Pt合金凝固-固态相变微观组织演化相场法模拟[J]. 金属学报, 2025, 61(1): 109-116.
[12] 孟泽, 李光强, 李腾飞, 郑庆, 曾斌, 刘昱. Ce对75Cr1钢洁净度、组织与耐点蚀性能的影响[J]. 金属学报, 2024, 60(9): 1229-1238.
[13] 王霖, 魏晨, 王雷, 王军, 李金山. Cu-Co系难混溶合金核壳结构演化过程模拟[J]. 金属学报, 2024, 60(9): 1239-1249.
[14] 任松, 吴家柱, 张屹, 张大斌, 曹阳, 尹存宏. 激光束空域形态对激光定向能量沉积316L不锈钢热输运影响的数值模拟[J]. 金属学报, 2024, 60(12): 1678-1690.
[15] 郭杰, 黄立清, 吴京洋, 李俊杰, 王锦程, 樊凯. 钛合金三次真空自耗电弧熔炼过程中的宏观偏析传递行为[J]. 金属学报, 2024, 60(11): 1531-1544.