Please wait a minute...
金属学报  2026, Vol. 62 Issue (7): 1246-1256    DOI: 10.11900/0412.1961.2024.00211
  研究论文 本期目录 | 过刊浏览 |
晶粒尺寸与晶体取向对CrCoNi中熵合金孪晶界疲劳开裂行为的影响
王玉洁1, 李琳琳1(), 张振军2,3(), 张哲峰2,3
1 东北大学 数字钢铁全国重点实验室 沈阳 110819
2 中国科学院金属研究所 沈阳材料科学国家研究中心 沈阳 110016
3 中国科学技术大学 材料科学与工程学院 沈阳 110016
Effects of Grain Size and Crystallographic Orientation on Fatigue Cracking at Twin Boundaries in CrCoNi Medium-Entropy Alloy
WANG Yujie1, LI Linlin1(), ZHANG Zhenjun2,3(), ZHANG Zhefeng2,3
1 State Key Laboratory of Digital Steel, Northeastern University, Shenyang 110819, China
2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
3 School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China
引用本文:

王玉洁, 李琳琳, 张振军, 张哲峰. 晶粒尺寸与晶体取向对CrCoNi中熵合金孪晶界疲劳开裂行为的影响[J]. 金属学报, 2026, 62(7): 1246-1256.
Yujie WANG, Linlin LI, Zhenjun ZHANG, Zhefeng ZHANG. Effects of Grain Size and Crystallographic Orientation on Fatigue Cracking at Twin Boundaries in CrCoNi Medium-Entropy Alloy[J]. Acta Metall Sin, 2026, 62(7): 1246-1256.

全文: PDF(3115 KB)   HTML
摘要: 

CrCoNi中熵合金拥有超越大多数fcc多主元合金和传统合金的优异综合力学性能,具有巨大的发展潜力以及广泛的应用前景。为确保该合金的长期稳定且安全使用,有必要充分探索其疲劳特性和损伤机理。细晶强化是该合金的主要强化方式,明确不同晶粒尺寸下孪晶界疲劳的开裂规律对减少沿晶疲劳开裂、提高材料疲劳性能具有重要意义。本工作采用滑移形貌法研究了两种晶粒尺寸CrCoNi中熵合金在低周疲劳条件下的孪晶界疲劳开裂行为。结果表明,对于任意给定的晶粒尺寸,CrCoNi中熵合金从滑移带开裂到孪晶界开裂之间的转变随着基体与孪晶之间Schmid因子差的增加而变化;随着孪晶界两侧滑移带Schmid因子差的增加,孪晶界面开裂变得更加容易。孪晶界开裂所需的Schmid因子差随晶粒尺寸增加而减小;随着晶粒尺寸增加,较小Schmid因子差使孪晶界附近产生较大的位错塞积,导致孪晶界损伤加剧而易疲劳开裂。

关键词 : CrCoNi中熵合金,  疲劳开裂,  孪晶界,  晶粒尺寸,  滑移带    
Abstract:

The CrCoNi medium-entropy alloy is known to demonstrate superior comprehensive mechanical properties relative to most fcc multiple-principal-elemental alloys. To ensure the long-term stability and safety of this alloy in practical applications, its fatigue characteristics and damage mechanisms must be thoroughly explored. Grain refinement is a crucial method for strengthening this alloy, and the effect of grain size on twin-boundary (TB) fatigue cracking must be clarified to reduce the intergranular fatigue cracks and improve fatigue performance. By conducting SEM measurements, the fatigue cracking behaviors at TBs in a CrCoNi medium-entropy alloy with two different grain sizes were systematically studied employing the slipping morphology method under low-cycle fatigue tests. The surface roughness around the TBs of the fatigued samples was characterized via laser confocal microscopy and white-light interference microscopy to quantify variations in the surface damage levels. Irrespective of grain size, the transition from slip-band cracking to TB cracking was observed to vary with the increasing difference in the Schmid factors (DSF) between the matrix and twin. Further, the propensity for TB cracking was facilitated by the escalation of DSF. Moreover, the magnitude of the required DSF for TB cracking was influenced by the grain size. The requirement of DSF for TB cracking decreased with increasing grain size. With the increase in grain size, even the minimal DSF is expected to result in the significant pilling up of dislocations near the TBs, thereby worsening the damage and rendering these boundaries favorable sites for fatigue cracking.

Key words: CrCoNi medium-entropy alloy    fatigue cracking    twin boundary    grain size    slip band
收稿日期: 2024-06-24     
ZTFLH:  TG144  
基金资助:国家自然科学基金项目(52371101);辽宁省兴辽英才计划项目(XLYC2203105)
通讯作者: 李琳琳,lill@ral.neu.edu.cn,主要从事金属材料疲劳损伤微观机制研究;
张振军,zjzhang@imr.ac.cn,主要从事金属材料疲劳与断裂机制、力学性能预测研究
作者简介: 王玉洁,女,满族,1994年生,博士生
图1  疲劳样品示意图
图2  不同晶粒尺寸的CoCrNi中熵合金(MEA)的微观组织与晶粒尺寸分布
T / oCd / μmYS / MPaUTS / MPaUE / %TE / %Nf / cyc
9005.0395.6862.458.684.557883
110033.5231.3686.183.5107.723208
表1  不同晶粒尺寸CrCoNi MEA样品在室温下的力学性能
图3  CrCoNi MEA样品在0.4%总应变幅下的晶界开裂和滑移带开裂表面形貌
图4  不同晶粒尺寸CrCoNi MEA样品在0.4%总应变幅下的表面疲劳形貌及高低起伏特征
图5  不同晶粒尺寸CrCoNi MEA样品在0.4%应变幅下疲劳后孪晶界开裂表面形貌
图6  不同晶粒尺寸CrCoNi MEA样品在0.4%总应变幅下疲劳后孪晶界两侧疲劳形貌特征
图7  总应变幅0.4%条件下不同晶粒尺寸CoCrNi MEA样品疲劳位错结构的明场TEM像
图8  利用滑移形貌法确定取向的原理示意图
Grain typeΔΩ
0-0.050.05-0.100.10-0.150.15-0.30
FG0, 74, 34, 15, 0
CG2, 47, 48, 09, 0
表2  晶粒尺寸与晶体取向对孪晶界/滑移带疲劳开裂行为影响统计数据
图9  晶体取向和晶粒尺寸对CrCoNi MEA孪晶界疲劳开裂趋势的影响
图10  不同晶粒尺寸样品中孪晶界两侧位错塞积导致孪晶界开裂的示意图
[1] Yeh J W, Chen S K, Lin S J, et al. Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes [J]. Adv. Eng. Mater., 2004, 6: 299
doi: 10.1002/adem.v6:5
[2] George E P, Raabe D, Ritchie R O. High-entropy alloys [J]. Nat. Rev. Mater., 2019, 4: 515
doi: 10.1038/s41578-019-0121-4
[3] Cantor B, Chang I T H, Knight P, et al. Microstructural development in equiatomic multicomponent alloys [J]. Mater. Sci. Eng., 2004, A375-377: 213
[4] Cantor B. Multicomponent and high entropy alloys [J]. Entropy, 2014, 16: 4749
doi: 10.3390/e16094749
[5] Otto F, Dlouhý A, Somsen C, et al. The influences of temperature and microstructure on the tensile properties of a CoCrFeMnNi high-entropy alloy [J]. Acta Mater., 2013, 61: 5743
doi: 10.1016/j.actamat.2013.06.018
[6] Gali A, George E P. Tensile properties of high- and medium-entropy alloys [J]. Intermetallics, 2013, 39: 74
doi: 10.1016/j.intermet.2013.03.018
[7] Gludovatz B, Hohenwarter A, Catoor D, et al. A fracture-resistant high-entropy alloy for cryogenic applications [J]. Science, 2014, 345: 1153
doi: 10.1126/science.1254581 pmid: 25190791
[8] Gludovatz B, Hohenwarter A, Thurston K V S, et al. Exceptional damage-tolerance of a medium-entropy alloy CrCoNi at cryogenic temperatures [J]. Nat. Commun., 2016, 7: 10602
doi: 10.1038/ncomms10602 pmid: 26830651
[9] Laplanche G, Kostka A, Reinhart C, et al. Reasons for the superior mechanical properties of medium-entropy CrCoNi compared to high-entropy CrMnFeCoNi [J]. Acta Mater., 2017, 128: 292
doi: 10.1016/j.actamat.2017.02.036
[10] Zhang Z J, Sheng H W, Wang Z J, et al. Dislocation mechanisms and 3D twin architectures generate exceptional strength-ductility-toughness combination in CrCoNi medium-entropy alloy [J]. Nat. Commun., 2017, 8: 14390
doi: 10.1038/ncomms14390 pmid: 28218267
[11] Heczko M, Mazánová V, Slone C E, et al. Role of deformation twinning in fatigue of CrCoNi medium-entropy alloy at room temperature [J]. Scr. Mater., 2021, 202: 113985
doi: 10.1016/j.scriptamat.2021.113985
[12] Miao J, Slone C E, Smith T M, et al. The evolution of the deformation substructure in a Ni-Co-Cr equiatomic solid solution alloy [J]. Acta Mater., 2017, 132: 35
doi: 10.1016/j.actamat.2017.04.033
[13] Chu S F, Zhang F, Chen D K, et al. Atomic-scale in situ observations of reversible phase transformation assisted twinning in a CrCoNi medium-entropy alloy [J]. Nano Lett., 2024, 24: 3624
doi: 10.1021/acs.nanolett.3c04516
[14] Wu Z, Bei H, Pharr G M, et al. Temperature dependence of the mechanical properties of equiatomic solid solution alloys with face-centered cubic crystal structures [J]. Acta Mater., 2014, 81: 428
doi: 10.1016/j.actamat.2014.08.026
[15] Suresh S. Fatigue of Materials [M]. 2nd Ed., Cambridge: Cambridge University Press, 1998: 156
[16] Zhang Z F, Wang Z G. Grain boundary effects on cyclic deformation and fatigue damage [J]. Prog. Mater. Sci., 2008, 53: 1025
doi: 10.1016/j.pmatsci.2008.06.001
[17] Liu W, Wang Z G, Xia Y B. Mechanism of initiation and propagation of intergranular cracks during fatigue process [J]. Ordnance Mater. Sci. Eng., 1990, (5): 1
[17] 刘 蔚, 王中光, 夏月波. 疲劳过程中沿晶裂纹萌生与扩展的机理 [J]. 兵器材料科学与工程, 1990, (5): 1
[18] Mughrabi H. Microstructural mechanisms of cyclic deformation, fatigue crack initiation and early crack growth [J]. Philos. Trans. Roy. Soc., 2015, 373A: 20140132
[19] Zhang Z J, Li L L, Zhang P, et al. Fatigue cracking at twin boundary: Effect of dislocation reactions [J]. Appl. Phys. Lett., 2012, 101: 011907
[20] Lu L, Shen Y F, Chen X H, et al. Ultrahigh strength and high electrical conductivity in copper [J]. Science, 2004, 304: 422
pmid: 15031435
[21] Lu K, Lu L, Suresh S. Strengthening materials by engineering coherent internal boundaries at the nanoscale [J]. Science, 2009, 324: 349
doi: 10.1126/science.1159610 pmid: 19372422
[22] Li L L, Zhang Z J, Zhang P, et al. Higher fatigue cracking resistance of twin boundaries than grain boundaries in Cu bicrystals [J]. Scr. Mater., 2011, 65: 505
doi: 10.1016/j.scriptamat.2011.06.009
[23] Sangid M D, Maier H J, Sehitoglu H. A physically based fatigue model for prediction of crack initiation from persistent slip bands in polycrystals [J]. Acta Mater., 2011, 59: 328
doi: 10.1016/j.actamat.2010.09.036
[24] Li L L, Zhang Z J, Zhang P, et al. Controllable fatigue cracking mechanisms of copper bicrystals with a coherent twin boundary [J]. Nat. Commun., 2014, 5: 3536
doi: 10.1038/ncomms4536 pmid: 24667520
[25] Wang A G, An X H, Gu J, et al. Effect of grain size on fatigue cracking at twin boundaries in a CoCrFeMnNi high-entropy alloy [J]. J. Mater. Sci. Technol., 2020, 39: 1
doi: 10.1016/j.jmst.2019.09.010
[26] Zhang Z J, Zhang P, Li L L, et al. Fatigue cracking at twin boundaries: Effects of crystallographic orientation and stacking fault energy [J]. Acta Mater., 2012, 60: 3113
doi: 10.1016/j.actamat.2012.02.016
[27] Zhang P, Zhang Z J, Li L L, et al. Twin boundary: Stronger or weaker interface to resist fatigue cracking? [J]. Scr. Mater., 2012, 66: 854
doi: 10.1016/j.scriptamat.2012.01.028
[28] Li L L, Zhang Z J, Zhang P, et al. A review on the fatigue cracking of twin boundaries: Crystallographic orientation and stacking fault energy [J]. Prog. Mater. Sci., 2023, 131: 101011
doi: 10.1016/j.pmatsci.2022.101011
[29] Zhang Z J. Investigations on the effects of stacking fault energy (SFE) on the strength-ductility cooperation and fatigue behaviors of single phase Cu-Zn alloys [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2013
[29] 张振军. 层错能对单相铜锌合金强度塑性匹配及疲劳行为影响研究 [D]. 沈阳: 中国科学院金属研究所, 2013
[30] Thompson A W, Backofen W A. The effect of grain size on fatigue [J]. Acta Metall., 1971, 19: 597
doi: 10.1016/0001-6160(71)90012-5
[31] Wang Y J, Yu T, Wang Z G, et al. Low cycle fatigue behaviors of CrCoNi medium-entropy alloy with different grain sizes [J]. Int. J. Fatigue, 2024, 180: 108105
doi: 10.1016/j.ijfatigue.2023.108105
[32] Lu K J, Chauhan A, Walter M, et al. Superior low-cycle fatigue properties of CoCrNi compared to CoCrFeMnNi [J]. Scr. Mater., 2021, 194: 113667
doi: 10.1016/j.scriptamat.2020.113667
[33] Zhang P. Investigations on tension, fatigue, fracture, strength and hardness of single-phase Cu-Zn alloys [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2011
[33] 张 鹏. 单相铜锌合金的拉伸、疲劳、断裂、强度与硬度研究 [D]. 沈阳: 中国科学院金属研究所, 2011
[34] Antolovich S D, Armstrong R W. Plastic strain localization in metals: Origins and consequences [J]. Prog. Mater. Sci., 2014, 59: 1
doi: 10.1016/j.pmatsci.2013.06.001
[35] Figueroa J C, Laird C. Crack initiation mechanisms in copper polycrystals cycled under constant strain amplitudes and in step tests [J]. Mater. Sci. Eng., 1983, 60: 45
[36] Tanaka K, Mura T. A dislocation model for fatigue crack initiation [J]. J. Appl. Mech., 1981, 48: 97
doi: 10.1115/1.3157599
[37] Sangid M D, Maier H J, Sehitoglu H. The role of grain boundaries on fatigue crack initiation—An energy approach [J]. Int. J. Plast., 2011, 27: 801
doi: 10.1016/j.ijplas.2010.09.009
[38] Essmann U, Gösele U, Mughrabi H. A model of extrusions and intrusions in fatigued metals I. Point-defect production and the growth of extrusions [J]. Philos. Mag., 1981, 44A: 405
[39] Dörr G, Blochwitz C. Microcracks in fatigued FCC polycrystals by interaction between persistent slip bands and grain boundaries [J]. Cryst. Res. Technol., 1987, 22: 113
doi: 10.1002/crat.v22:1
[40] Kobayashi S, Inomata T, Kobayashi H, et al. Effects of grain boundary- and triple junction-character on intergranular fatigue crack nucleation in polycrystalline aluminum [J]. J. Mater. Sci., 2008, 43: 3792
doi: 10.1007/s10853-007-2236-z
[41] Zhang Z F, Wang Z G. Comparison of fatigue cracking possibility along large- and low-angle grain boundaries [J]. Mater. Sci. Eng., 2000, A284: 285
[42] Thompson A L. The influence of grain and tlin boundaries in fatigue cracking [J]. Acta Metall., 1972, 20: 1085
doi: 10.1016/0001-6160(72)90172-1
[43] Liang F L, Laird C. Control of intergranular fatigue cracking by slip homogeneity in copper ii: Effect of loading mode [J]. Mater. Sci. Eng., 1989, A117: 103
[44] Hall E O. The deformation and ageing of mild steel: III Discussion of results [J]. Proc. Phys. Soc., 1951, 64B: 747
[45] Petch N J. The cleavage strengh of polycrystals [J]. J. Iron Steel Int., 1953, 174: 25
[1] 王洪瑛, 姚志浩, 李大禹, 郭婧, 姚凯俊, 董建新. 高 γ' 相含量粉末及变形高温合金组织和力学性能的异同性[J]. 金属学报, 2025, 61(9): 1364-1374.
[2] 屈小波, 安金敏, 王林, 李喜. 汽车用齿轮钢16MnCrS5热处理变形机理[J]. 金属学报, 2025, 61(4): 597-607.
[3] 韩婧, 邵琛玮, 邱子浩, 张振军, 张哲峰. 晶粒尺寸对Fe-Mn-Al-C系第三代TWIP钢低周疲劳性能的影响[J]. 金属学报, 2025, 61(12): 1873-1883.
[4] 李福林, 付锐, 白云瑞, 孟令超, 谭海兵, 钟燕, 田伟, 杜金辉, 田志凌. 初始晶粒尺寸和强化相对GH4096高温合金热变形行为和再结晶的影响[J]. 金属学报, 2023, 59(7): 855-870.
[5] 原家华, 张秋红, 王金亮, 王灵禺, 王晨充, 徐伟. 磁场与晶粒尺寸协同作用对马氏体形核及变体选择的影响[J]. 金属学报, 2022, 58(12): 1570-1580.
[6] 李晓倩, 王富国, 梁爱民. 喷涂工艺对Ta2O5原位复合钽基纳米晶涂层微观结构及摩擦磨损性能的影响[J]. 金属学报, 2021, 57(2): 237-246.
[7] 张守清, 胡小锋, 杜瑜宾, 姜海昌, 庞辉勇, 戎利建. 海洋平台用Ni-Cr-Mo-B超厚钢板的截面效应[J]. 金属学报, 2020, 56(9): 1227-1238.
[8] 许占一, 沙玉辉, 张芳, 章华兵, 李国保, 储双杰, 左良. 取向硅钢二次再结晶过程中的取向选择行为[J]. 金属学报, 2020, 56(8): 1067-1074.
[9] 和淑文, 王鸣华, 白琴, 夏爽, 周邦新. WC-TiC-TaC-Co硬质合金中TaC含量对其显微组织和力学性能的影响[J]. 金属学报, 2020, 56(7): 1015-1024.
[10] 华涵钰,谢君,舒德龙,侯桂臣,盛乃成,于金江,崔传勇,孙晓峰,周亦胄. W含量对一种高W镍基高温合金显微组织的影响[J]. 金属学报, 2020, 56(2): 161-170.
[11] 李鑫,董月成,淡振华,常辉,方志刚,郭艳华. 等通道角挤压制备超细晶纯Ti的腐蚀性能研究[J]. 金属学报, 2019, 55(8): 967-975.
[12] 万志鹏, 王涛, 孙宇, 胡连喜, 李钊, 李佩桓, 张勇. GH4720Li合金热变形过程动态软化机制[J]. 金属学报, 2019, 55(2): 213-222.
[13] 冯浩,李花兵,路鹏冲,杨纯田,姜周华,武晓雷. 铜绿假单胞菌对CrCoNi中熵合金微生物腐蚀行为的影响[J]. 金属学报, 2019, 55(11): 1457-1468.
[14] 钟茜婷, 王磊, 刘峰. Incoloy 028合金不连续动态再结晶中链状组织形成机理研究[J]. 金属学报, 2018, 54(7): 969-980.
[15] 刘廷光, 夏爽, 白琴, 周邦新, 陆永浩. 孪晶界在316L不锈钢三维晶界网络中的分布特征[J]. 金属学报, 2018, 54(10): 1377-1386.