| 热轧硅钢表层动态再结晶区形成规律及剪切织构特征 |
姜伟宁1, 武晓龙1, 杨平1( ), 顾新福1, 解清阁2 |
1.北京科技大学 材料科学与工程学院 北京 100083 2.北京科技大学 钢铁共性技术协同创新中心 北京 100083 |
|
| Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel |
JIANG Weining1, WU Xiaolong1, YANG Ping1( ), GU Xinfu1, XIE Qingge2 |
1.School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China 2.Collaborative Innovation Center of Steel Technology, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
姜伟宁, 武晓龙, 杨平, 顾新福, 解清阁. 热轧硅钢表层动态再结晶区形成规律及剪切织构特征[J]. 金属学报, 2022, 58(12): 1545-1556.
Weining JIANG,
Xiaolong WU,
Ping YANG,
Xinfu GU,
Qingge XIE.
Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. Acta Metall Sin, 2022, 58(12): 1545-1556.
| 1 |
Calvillo P R, Salazar N, Schneider J, et al. Microstructure characterization by EBSD of hot rolled high-silicon steel [J]. Defect Diffus. Forum, 2008, 273-276: 69
doi: 10.4028/www.scientific.net/DDF.273-276.69
|
| 2 |
Stöcker A, Schmidtchen M, Kawalla R. Hot rolling simulation for non-oriented electrical steel [J]. AIP Conf. Proc., 2017, 1896: 190021
|
| 3 |
Wu X L, Yang P, Gu X F, et al. The influence of normalization temperatures on different texture components and magnetic properties of nonoriented electrical steels [J]. Steel. Res. Int., 2021, 92: 2000361
|
| 4 |
Inagaki H, Suda T. The development of rolling textures in low-carbon steels [J]. Texture, Stress, Microstr., 1972, 1: 612480
|
| 5 |
Koh P K, Dunn C G. Cold-rolled textures of silicon-iron crystals [J]. JOM, 1955, 7(2): 401
doi: 10.1007/BF03377518
|
| 6 |
Zhang N, Yang P, He C X, et al. Effect of {110}<229> and {110}<112> grains on texture evolution during cold rolling and annealing of electrical steel [J]. ISIJ Int., 2016, 56: 1462
doi: 10.2355/isijinternational.ISIJINT-2016-145
|
| 7 |
Shao Y Y, Yang P, Mao W M. Analysis on grain boundary effects of columnar grained electrical steel [J]. Acta Metall. Sin., 2014, 50: 259
doi: 10.3724/SP.J.1037.2013.00459
|
| 7 |
邵媛媛, 杨平, 毛卫民. 电工钢柱状晶热、冷轧时晶界作用分析 [J]. 金属学报, 2014, 50: 259
doi: 10.3724/SP.J.1037.2013.00459
|
| 8 |
Matsuo M, Sakai T, Suga Y. Origin and development of through-the-thickness variations of texture in the processing of grain-oriented silicon steel [J]. Metall. Trans., 1986, 17A: 1313
|
| 9 |
Yang P, Shao Y Y, Mao W M, et al. Orientation evolutions during hot rolling of electrical steel containing initial columnar grains [J]. Mater. Sci. Forum, 2012, 702-703: 754
doi: 10.4028/www.scientific.net/MSF.702-703.754
|
| 10 |
Shao Y Y, Yang P, Fu Y J, et al. Texture evolution of columnar grains in electrical steel during hot rolling [J]. J. Iron Steel Res. Int., 2013, 20: 99
|
| 11 |
Fedoseev A I, Raabe D, Gottstein G. Texture development and simulation of inhomogeneous deformation of FeCr during hot rolling [J]. Mater. Sci. Forum, 1994, 157-162: 1771
doi: 10.4028/www.scientific.net/MSF.157-162.1771
|
| 12 |
Shimizu Y, Ito Y, Iida Y. Formation of the Goss orientation near the surface of 3 pct silicon steel during hot rolling [J]. Metall. Trans., 1986, 17A: 1323
|
| 13 |
Cruz-Gandarilla F, Baudin T, Penelle R, et al. Study of local microstructure and texture heterogeneities in hot rolled CGO Fe-3%Si sheets [J]. Mater. Sci. Forum, 2004, 467-470: 123
doi: 10.4028/www.scientific.net/MSF.467-470.123
|
| 14 |
Cruz-Gandarilla F, Penelle R, León H M, et al. A study of local microstructure and texture heterogeneities in a CGO Fe3%Si alloy from hot rolling to primary recrystallization [J]. Mater. Sci. Forum, 2005, 495-497: 483
doi: 10.4028/www.scientific.net/MSF.495-497.483
|
| 15 |
Cruz-Gandarilla F, Baudin T, Mathon M H, et al. Characterization of global and local textures in hot rolled CGO Fe3%Si [J]. Mater. Sci. Forum, 2006, 509: 25
doi: 10.4028/www.scientific.net/MSF.509.25
|
| 16 |
Lobanov M L, Redikul'tsev A A, Rusakov G M, et al. Effect of carbon on texture formation in electrical steel Fe-3% Si under hot rolling [J]. Metal Sci. Heat Treat., 2015, 56: 646
doi: 10.1007/s11041-015-9815-4
|
| 17 |
Mehdi M, He Y L, Hilinski E J, et al. The origins of the Goss orientation in non-oriented electrical steel and the evolution of the Goss texture during thermomechanical processing [J]. Steel Res. Int., 2019, 90: 1800582
|
| 18 |
Yan M Q, Qian H, Yang P, et al. Behaviors of brass texture and its influence on Goss texture in grain oriented electrical steels [J]. Acta Metall. Sin., 2012, 48: 16
doi: 10.3724/SP.J.1037.2011.00421
|
| 18 |
颜孟奇, 钱浩, 杨平 等. 电工钢中黄铜织构行为及其对Goss织构的影响 [J]. 金属学报, 2012, 48: 16
doi: 10.3724/SP.J.1037.2011.00421
|
| 19 |
Mukhopadhyay A, Howard I C, Sellars C M. Finite element modelling of effects of roll gap geometry in hot rolling [J]. Mater. Sci. Technol., 2005, 21: 901
doi: 10.1179/174328405X47546
|
| 20 |
Jia M X, Lü Y P, Xu L F, et al. The influence of friction on the texture formation of a IF steel during hot rolling in the ferrite region [J]. Steel Res. Int., 2013, 84: 761
doi: 10.1002/srin.201200260
|
| 21 |
Jiang W N, Wu X L, Yang P, et al. Relationship between the initial {100} textures and the shear textures developed in sheet surface during hot rolling of non-oriented silicon steel [J]. Mater. Charact., 2021, 182: 111534
|
| 22 |
Calvillo P R, Reis A C C, Kestens L, et al. Grain refinement by high temperature plane-strain compression of Fe-2%Si steel [J]. Mater. Sci. Forum, 2006, 503-504: 977
doi: 10.4028/www.scientific.net/MSF.503-504.977
|
| 23 |
Tsuji N, Tsuzaki K, Maki T. Effects of rolling reduction and annealing temperature on the recrystallization structure of solidified columnar crystals in a 19% Cr ferritic stainless steel [J]. ISIJ Int., 1994, 34: 1008
doi: 10.2355/isijinternational.34.1008
|
| 24 |
Hsun H. Microbands in a rolled Si-Fe crystal and their role in recrystallization [J]. Acta Metall., 1962, 10: 1112
doi: 10.1016/0001-6160(62)90083-4
|
| 25 |
Yan M Q, Yang P, Jiang Q W, et al. Influence of rolling direction on the texture evolution of Fe-3%Si alloy [J]. Acta Metall. Sin., 2011, 47: 25
|
| 25 |
颜孟奇, 杨平, 蒋奇武 等. 轧制方向对Fe-3%Si合金织构演变规律的影响 [J]. 金属学报, 2011, 47: 25
doi: 10.3724/SP.J.1037.2010.00432
|
| 26 |
Wada T, Matsumoto F, Kuroki K. On the recrystallization of 3%Si-Fe (001)[110] single crystal [J]. J. Jpn. Inst. Met., 1968, 32: 767
doi: 10.2320/jinstmet1952.32.8_767
|
| 27 |
Li Z C, Yang P, Yan M Q, et al. Evolution of microstructure and textures of {100} initial texture in an electrical steel [J]. Chin. J. Stereol. Image. Anal., 2009, 14: 237
|
| 27 |
李志超, 杨平, 颜孟奇 等. 电工钢中{100}织构的演变规律 [J]. 中国体视学与图像分析, 2009, 14: 237
|
| 28 |
Park J T, Szpunar J A. Evolution of recrystallization texture in nonoriented electrical steels [J]. Acta. Mater., 2003, 51: 3037
doi: 10.1016/S1359-6454(03)00115-0
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|