| 超高压烧结制备14Cr-ODS钢及微观组织与力学性能 |
王韬1, 龙弟均2, 余黎明1( ), 刘永长1, 李会军1, 王祖敏1 |
1.天津大学 材料科学与工程学院 水利工程仿真与安全国家重点实验室 天津 300354 2.中国核动力研究设计院 成都 610041 |
|
| Microstructure and Mechanical Properties of 14Cr-ODS Steel Fabricated by Ultra-High Pressure Sintering |
WANG Tao1, LONG Dijun2, YU Liming1( ), LIU Yongchang1, LI Huijun1, WANG Zumin1 |
1.State Key Laboratory of Hydraulic Engineering Simulation and Safety, School of Materials Science and Engineering, Tianjin University, Tianjin 300354, China 2.Nuclear Power Institute of China, Chengdu 610041, China |
引用本文:
王韬, 龙弟均, 余黎明, 刘永长, 李会军, 王祖敏. 超高压烧结制备14Cr-ODS钢及微观组织与力学性能[J]. 金属学报, 2022, 58(2): 184-192.
Tao WANG,
Dijun LONG,
Liming YU,
Yongchang LIU,
Huijun LI,
Zumin WANG.
Microstructure and Mechanical Properties of 14Cr-ODS Steel Fabricated by Ultra-High Pressure Sintering[J]. Acta Metall Sin, 2022, 58(2): 184-192.
| 1 |
Yan P Y , Yu L M , Liu Y C , et al . Effects of Hf addition on the thermal stability of 16Cr-ODS steels at elevated aging temperatures [J]. J. Alloys Compd., 2018, 739: 368
|
| 2 |
Dai L , Liu Z , Yu L M , et al . Microstructural characterization of Mg-Al-O rich nanophase strengthened Fe-Cr alloys [J]. Mater. Sci. Eng., 2020, A771: 138664
|
| 3 |
Mukhopadhyay D . Development of low activation oxide-dispersion strengthened ferritic steels for fusion reactors [D]. Ann Arbor: University of Idaho, 1996
|
| 4 |
Hosemann P , Frazer D , Fratoni M , et al . Materials selection for nuclear applications: Challenges and opportunities [J]. Scr. Mater., 2018, 143: 181
|
| 5 |
Odette G R , Alinger M J , Wirth B D . Recent developments in irradiation-resistant steels [J]. Annu. Rev. Mater. Res., 2008, 38: 471
|
| 6 |
Lescoat M L , Ribis J , Gentils A , et al . In situ TEM study of the stability of nano-oxides in ODS steels under ion-irradiation [J]. J. Nucl. Mater., 2012, 428: 176
|
| 7 |
Shao Y , Yu L M , Liu Y C , et al . Hot deformation behaviors of a 9Cr oxide dispersion-strengthened steel and its microstructure characterization [J]. Int. J. Min. Met. Mater., 2019, 26: 597
|
| 8 |
Ren J , Yu L M , Liu Y C , et al . Microstructure evolution and tensile properties of an Al added high-Cr ODS steel during thermal aging at 650℃ [J]. Fusion Eng. Des., 2020, 157: 111700
|
| 9 |
Abe F . Precipitate design for creep strengthening of 9% Cr tempered martensitic steel for ultra-supercritical power plants [J]. Sci. Technol. Adv. Mater., 2008, 9: 013002
|
| 10 |
Capdevila C , Miller M K , Russell K F , et al . Phase separation in PM 2000TM Fe-base ODS alloy: Experimental study at the atomic level [J]. Mater. Sci. Eng., 2008, A490: 277
|
| 11 |
Kobayashi S , Takasugi T . Mapping of 475℃ embrittlement in ferritic Fe-Cr-Al alloys [J]. Scr. Mater., 2010, 63: 1104
|
| 12 |
Capdevila C , Miller M K , Toda I , et al . Influence of the α-α' phase separation on the tensile properties of Fe-base ODS PM 2000 alloy [J]. Mater. Sci. Eng., 2010, A527: 7931
|
| 13 |
Kim I S , Choi B Y , Kang C Y , et al . Effect of Ti and W on the mechanical properties and microstructure of 12% Cr base mechanical-alloyed nano-sized ODS ferritic alloys [J]. ISIJ Int., 2003, 43: 1640
|
| 14 |
Kim I S , Okuda T , Kang C Y , et al . Effect of oxide species and thermomechanical treatments on the strength properties of mechanically alloyed Fe-17%Cr ferritic ODS materials [J]. Met. Mater., 2000, 6: 513
|
| 15 |
Li Z Y , Lu Z , Xie R , et al . Effects of Y2O3, La2O3 and CeO2 additions on microstructure and mechanical properties of 14Cr-ODS ferrite alloys produced by spark plasma sintering [J]. Fusion Eng. Des., 2017, 121: 159
|
| 16 |
Li S F . Study on oxide strengthened dispersion alloys for generation IV advanced nuclear systems [D]. Beijing: University of Science and Technology Beijing, 2016
|
| 16 |
李少夫 . 用于第四代先进核能系统的氧化物弥散强化合金的研究 [D]. 北京: 北京科技大学, 2016
|
| 17 |
Dadé M , Malaplate J , Garnier J , et al . Influence of microstructural parameters on the mechanical properties of oxide dispersion strengthened Fe-14Cr steels [J]. Acta Mater., 2017, 127: 165
|
| 18 |
Zhao Q , Ma Z Q , Yu L M , et al . Tailoring the secondary phases and mechanical properties of ODS steel by heat treatment [J]. J. Mater. Sci. Technol., 2019, 35: 1064
|
| 19 |
Gong M Q , Zhou Z J , Hu H L , et al . Effects of aluminum on microstructure and mechanical behavior of 14Cr-ODS steels [J]. J. Nucl. Mater., 2015, 462: 502
|
| 20 |
Peng Y Y , Yu L M , Liu Y C , et al . Effect of ageing treatment at 650oC on microstructure and properties of 9Cr-ODS steel [J]. Acta Metall. Sin., 2020, 56: 1075
|
| 20 |
彭艳艳, 余黎明, 刘永长 等 . 650℃时效对9Cr-ODS钢显微组织和性能的影响 [J]. 金属学报, 2020, 56: 1075
|
| 21 |
Zhao Q , Yu L M , Liu Y C , et al . Effects of aluminum and titanium on the microstructure of ODS steels fabricated by hot pressing [J]. Int. J. Min. Met. Mater., 2018, 25: 1156
|
| 22 |
Oksiuta Z , Ozieblo A , Perkowski K , et al . Influence of HIP pressure on tensile properties of a 14Cr ODS ferritic steel [J]. Fusion Eng. Des., 2014, 89: 137
|
| 23 |
Zhao Q , Yu L M , Liu Y C , et al . Microstructure and tensile properties of a 14Cr ODS ferritic steel [J]. Mater. Sci. Eng., 2017, A680: 347
|
| 24 |
Ma F K . Isostatic Pressing Technology [M]. Beijing: Metallurgical Industry Press, 1992: 158
|
| 24 |
马福康 . 等静压技术 [M]. 北京: 冶金工业出版社, 1992: 158
|
| 25 |
Pazos D , Suárez M , Fernández A , et al . Microstructural comparison of oxide dispersion strengthened Fe-14Cr steels produced by HIP and SPS [J]. Fusion Eng. Des., 2019, 146: 2328
|
| 26 |
Zhang Y Z , Li Y G , Han B , et al . Microstructural characteristics of Hadfield steel solidified under high pressure [J]. High Press. Res., 2011, 31: 634
|
| 27 |
Gu T , Xu F Q , Zhao Y H , et al . Effects of high pressure heat treatment on microstructure and mechanical properties of aluminum bronze [J]. Mater. Res. Express, 2019, 6: 096508
|
| 28 |
Du C C , Jin S B , Fang Y , et al . Ultrastrong nanocrystalline steel with exceptional thermal stability and radiation tolerance [J]. Nat. Commun., 2018, 9: 5389
|
| 29 |
Porter D A , Easterling K E , translated by Li C H , Yu Y N . Phase Transformations in Metals and Alloys [M]. Beijing: Metallurgical Industry Press, 1981: 286
|
| 29 |
Porter D A, Easterling K E 著, 李长海, 余永宁译. 金属和合金中的相变 [M]. 北京: 冶金工业出版社, 1981: 286
|
| 30 |
Xia L F , Zhang Z X . Diffusion in Metals [M]. Harbin: Harbin Institute of Technology Press, 1989: 74
|
| 30 |
夏立芳, 张振信 . 金属中的扩散 [M]. 哈尔滨: 哈尔滨工业大学出版社, 1989: 74
|
| 31 |
Sakasegawa H , Chaffron L , Legendre F , et al . Correlation between chemical composition and size of very small oxide particles in the MA957 ODS ferritic alloy [J]. J. Nucl. Mater., 2009, 384: 115
|
| 32 |
Seol J B , Haley D , Hoelzer D T , et al . Influences of interstitial and extrusion temperature on grain boundary segregation, Y-Ti-O nanofeatures, and mechanical properties of ferritic steels [J]. Acta Mater., 2018, 153: 71
|
| 33 |
Jiang Y , Smith J R , Odette G R . Formation of Y-Ti-O nanoclusters in nanostructured ferritic alloys: A first-principles study [J]. Phys. Rev., 2009, 79B: 064103
|
| 34 |
Qian Q , Wang Y R , Jiang Y , et al . Nucleation of Y-X-O (X = Al, Ti, or Zr) NCs in nano-structured ferritic alloys: A first principles comparative study [J]. J. Nucl. Mater., 2019, 518: 140
|
| 35 |
Williams C A , Unifantowicz P , Baluc N , et al . The formation and evolution of oxide particles in oxide-dispersion-strengthened ferritic steels during processing [J]. Acta Mater., 2013, 61: 2219
|
| 36 |
Zhang W Q . Phase Transformations in Solid Metals and Alloys [M]. Beijing: National Defense Industry Press, 2016: 70
|
| 36 |
张伟强 . 固态金属及合金中的相变 [M]. 北京: 国防工业出版社, 2016: 70
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|