Please wait a minute...
金属学报  2021, Vol. 57 Issue (8): 989-999    DOI: 10.11900/0412.1961.2020.00451
  研究论文 本期目录 | 过刊浏览 |
超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响
陈胜虎(), 戎利建
中国科学院金属研究所 中国科学院核用材料与安全评价重点实验室 沈阳 110016
Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic
CHEN Shenghu(), RONG Lijian
CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
引用本文:

陈胜虎, 戎利建. 超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响[J]. 金属学报, 2021, 57(8): 989-999.
Shenghu CHEN, Lijian RONG. Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic[J]. Acta Metall Sin, 2021, 57(8): 989-999.

全文: PDF(16689 KB)   HTML
摘要: 

利用SEM、XRD、EPMA和XPS等研究了冷旋锻变形对9Cr2WVTa铁素体-马氏体钢在650℃空气中氧化膜形成过程的影响,在此基础上考察了预氧化制备氧化膜对9Cr2WVTa铁素体-马氏体钢在饱和氧液态Pb-Bi共晶 (LBE)中腐蚀行为的影响。结果表明,冷旋锻变形量的增加可提高样品的抗氧化性能,63%变形处理使抗氧化性能略有提高,94%变形处理可显著提高抗氧化性能。相较于回火态样品,63%变形处理样品形成的氧化物仍主要为(Fe, Cr)2O3,只是氧化物颗粒尺寸略有下降;94%变形获得的超细晶样品中,不仅氧化物颗粒尺寸显著减小,而且促进了富Mn氧化物(MnCr2O4和Mn2O3)的形成。超细晶样品中大幅度提高的空位浓度和位错密度、以及增加的晶界数量,显著提高了元素的扩散速率,Mn的异常快速扩散促进了富Mn氧化物的形成,稳定性好的富Mn氧化物提高了氧化膜的致密性。650℃空气中预氧化处理20 h后,超细晶样品表面获得致密性良好的富Mn氧化膜,在550℃饱和氧LBE中腐蚀500 h后,预氧化制备氧化膜可有效阻止LBE对铁素体-马氏体钢的侵蚀,并抑制了Fe的外扩散。Mn在LBE中较高的溶解度会加快富Mn氧化膜的溶解,随着Mn的不断溶解和LBE的持续侵蚀,预制备氧化膜的致密性不断下降而最终破裂,腐蚀2000 h后,样品表面形成了连续的Pb-Bi腐蚀产物。

关键词 : 超细晶铁素体-马氏体钢,  冷旋锻变形,  预氧化,  Pb-Bi腐蚀,  扩散    
Abstract:

Liquid lead and lead-bismuth eutectic (LBE) are considered primary candidate materials for coolant in advanced lead fast reactors, and also, for coolant and spallation target in accelerator-driven systems because of their favorable thermal-physical and chemical properties. However, liquid lead and LBE exhibit substantial structural material corrosion, which is considered one of the critical challenges in the liquid lead or LBE application. Among the effective methods to reduce the corrosive effect, careful control of the oxygen content dissolved in the liquid introduces a protective oxide layer on the surface of the structural material. Ferritic-martensitic steels with (9%-12%)Cr (mass fraction) have been considered promising structural materials in the advanced lead fast reactor and accelerator-driven system. Oxide scale with duplex structure is formed on the (9%-12%)Cr ferritic-martensitic steels in oxygen-containing LBE, but the oxide scale grows rapidly enough to cause the substrate recession. Recently, pre-oxidation treatment was proposed to further improve the corrosion performance in LBE. As reported, grain refinement promoted the formation of oxide scale without chemical modification. However, grain refinement effects on the oxide scale formation of (9%-12%)Cr ferritic-martensitic steels are not clear, and the effect of oxide scale through pre-oxidation treatment on the corrosion performance in LBE is rarely reported. In this study, the oxide scale formation behavior during pre-oxidation in air at 650oC on the 9Cr2WVTa ferritic-martensitic steel after different cold rotary-swaging deformation rates was analyzed using SEM, XRD, EPMA, and XPS, and the effect of pre-oxide scale on the corrosion performance in stagnant oxygen-saturated LBE was further investigated. The results demonstrated that the high-temperature oxidation resistance in air was enhanced by increasing the diameter reduction. A slight improvement in oxidation resistance was observed after 63% deformation, while significant enhancement in oxidation resistance was present in ultrafine-grained sample fabricated by 94% deformation. The oxide particle size was slightly reduced in the sample produced after 63% deformation during air oxidation compared with the tempered sample, but (Fe, Cr)2O3 oxide particles were formed on both samples. The size of oxide particles was significantly reduced and Mn-riched oxide (MnCr2O4 and Mn2O3) was promoted in the ultrafine-grained sample. The presence of Mn-riched oxide with good stability improved the oxide scale compactness. The compact oxide scale on the ultrafine-grained sample using pre-oxidation treatment at 650oC for 20 h effectively suppressed the corrosive attack of LBE and the outward diffusion of Fe through the pre-oxide scale after exposure for 500 h to stagnant oxygen-saturated LBE at 550oC. The higher solubility of Mn in LBE promoted the dissolution of the Mn-riched pre-oxide scale. The gradual dissolution of Mn in pre-oxide scale and corrosive attack by LBE led to the breakdown of the pre-oxide scale, which was supported by the formation of a continuous corrosion product layer after exposure for 2000 h to stagnant oxygen-saturated LBE.

Key words: ultrafine-grained ferritic-martensitic steel    cold rotary-swaging deformation    pre-oxidation    Pb-Bi corrosion    diffusion
收稿日期: 2020-11-09     
ZTFLH:  TG174  
基金资助:国家自然科学基金项目(51871218);中国科学院青年创新促进会项目(2018227);辽宁省自然科学基金项目(2020-);MS-010,以及国防科技工业核材料技术创新中心基金项目(ICNM-2020-ZH-18)
作者简介: 陈胜虎,男,1986年生,副研究员,博士
图1  9Cr2WVTa铁素体-马氏体钢经不同变形量冷旋锻变形后的微观组织
图2  不同变形量的冷旋锻9Cr2WVTa铁素体-马氏体钢在650℃空气中的氧化增重曲线
图3  不同变形量的冷旋锻9Cr2WVTa铁素体-马氏体钢经650℃空气氧化20、100和500 h后表面形成氧化膜的SEM像
图4  不同变形量的冷旋锻9Cr2WVTa铁素体-马氏体钢经650℃空气氧化500 h后的XRD谱
图5  不同变形量的冷旋锻9Cr2WVTa铁素体-马氏体钢经650℃空气氧化20 h后氧化膜中元素含量随深度方向的变化
图6  未预氧化处理与预氧化处理的94%变形量样品经550℃饱和氧LBE腐蚀500和2000 h后氧化膜截面形貌的BSE像
图7  预氧化处理的94%变形量样品经550℃饱和氧LBE腐蚀2000 h后氧化膜的EPMA元素分布
图8  不同变形量的冷旋锻9Cr2WVTa铁素体-马氏体钢(110)、(200)、(211)和(220)的XRD峰
图9  预氧化处理的94%变形量样品经550℃饱和氧LBE腐蚀500和2000 h后的表面SEM像
1 Yvon P. Structural Materials for Generation Ⅳ Nuclear Reactors [M]. Duxford: Woodhead Publishing, 2017: 24
2 OECD/NEA Nuclear Science Committee, translated by Rong L J, Zhang Y T, Lu S P, et al. Handbook on Lead-Bismuth Eutectic Alloy and Lead: Properties, Materials Compatibility, Thermal-hydraulics and Technologies [M]. Beijing: Science Press, 2007: 3
2 OECD/NEA Nuclear Science Committee著, 戎利建, 张玉妥, 陆善平等译. 铅与铅铋共晶合金手册——性能、材料相容性、热工水力学和技术 [M]. 北京: 科学出版社, 2007: 3
3 Han J S, Liu B, Li W Q. Summary of lead-cooled fast reactor research [J]. Nucl. Sci. Technol., 2018, 6(3): 87
3 韩金盛, 刘 滨, 李文强. 铅冷快堆研究概述 [J]. 核科学与技术, 2018, 6(3): 87
4 Zhang J S. A review of steel corrosion by liquid lead and lead-bismuth [J]. Corros. Sci., 2009, 51: 1207
5 Gorynin I V, Karzov G P, Markov V G, et al. Structural materials for atomic reactors with liquid metal heat-transfer agents in the form of lead or lead-bismuth alloy [J]. Met. Sci. Heat Treat., 1999, 41: 384
6 Gong X, Marmy P, Yin Y. The role of oxide films in preventing liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic [J]. J. Nucl. Mater., 2018, 509: 401
7 Tsisar V. Influence of rolling and preoxidation on the oxidation resistance of EP823 steel in static lead melt [J]. Probl. Atom. Sci. Technol., 2012, 78(2): 89
8 Lillard R S, Valot C, Hill M A, et al. Influence of preoxidation on the corrosion of steels in liquid lead-bismuth eutectic [J]. Corrosion, 2004, 60: 1031
9 Yaskiv O I, Kukhar I S, Fedirko V M. Effect of preliminary diffusion oxidation on mechanical properties of ferritic steel in oxygen-containing lead [J]. Fusion Eng. Des., 2015, 101: 134
10 Klueh R L, Harries D R. High-Chromium Ferritic and Martensitic Steels for Nuclear Applications [M]. West Conshohocken: American Society for Testing and Materials, 2001: 5
11 Tan L, Hoelzer D T, Busby J T, et al. Microstructure control for high strength 9Cr ferritic-martensitic steels [J]. J. Nucl. Mater., 2012, 422: 45
12 Chen S H, Jin X J, Rong L J. Microstructural evolution and mechanical properties of ultrafine-grained ferritic-martensitic steel during thermal aging [J]. Metall. Mater. Trans., 2020, 51A: 5154
13 Zinkle S J, Was G S. Materials challenges in nuclear energy [J]. Acta Mater., 2013, 61: 735
14 Martinelli L, Balbaud-Célérier F, Terlain A, et al. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part I) [J]. Corros. Sci., 2008, 50: 2523
15 Martinelli L, Balbaud-Célérier F, Terlain A, et al. Oxidation mechanism of an Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy at 470oC (Part II) [J]. Corros. Sci., 2008, 50: 2537
16 Martinelli L, Balbaud-Célérier F, Picard G, et al. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part III) [J]. Corros. Sci., 2008, 50: 2549
17 Wang J, Lu S P, Rong L J, et al. Effect of silicon on the oxidation resistance of 9wt.% Cr heat resistance steels in 550oC lead-bismuth eutectic [J]. Corros. Sci., 2016, 111: 13
18 Yang K, Yan W, Wang Z G, et al. Development of a novel structural material (SIMP steel) for nuclear equipment with balanced resistances to high temperature, radiation and liquid metal corrosion [J]. Acta Metall. Sin., 2016, 52: 1207
18 杨 柯, 严 伟, 王志光等. 核用新型耐高温、抗辐照、耐液态金属腐蚀结构材料——SIMP钢的研究进展 [J]. 金属学报, 2016, 52: 1207
19 Lu Y H, Song Y Y, Chen S H, et al. Effects of Al and Si on mechanical properties and corrosion resistance in liquid Pb-Bi eutectic of 9Cr2WVTa steel [J]. Acta Metall. Sin., 2016, 52: 298
19 鲁艳红, 宋元元, 陈胜虎等. Al和Si对9Cr2WVTa钢力学性能及耐Pb-Bi腐蚀性能的影响 [J]. 金属学报, 2016, 52: 298
20 Chen S H, Rong L J. Effect of silicon on the microstructure and mechanical properties of reduced activation ferritic/martensitic steel [J]. J. Nucl. Mater., 2015, 459: 13
21 Peng X, Wang F H. High temperature corrosion of nanocrystalline metallic materials [J]. Acta Metall. Sin., 2014, 50: 202
21 彭 晓, 王福会. 纳米晶金属材料的高温腐蚀行为 [J]. 金属学报, 2014, 50: 202
22 Singh Raman R K, Khanna A S, Tiwari R K. et al. Influence of grain size on the oxidation resistance of 2.25Cr-1Mo steel [J]. Oxid. Met., 1992, 37: 1
23 Trindade V, Christ H J, Krupp U. Grain-size effects on the high-temperature oxidation behaviour of chromium Steels [J]. Oxid. Met., 2010, 73: 551
24 Chen S H, Jin X J, Rong L J. Improvement in high temperature oxidation resistance of 9%Cr ferritic-martensitic steel by enhanced diffusion of Mn [J]. Oxid. Met., 2016, 85: 189
25 Chen S H, Rong L J. Roles of Mn in the high-temperature air oxidation of 9Cr ferritic-martensitic steel after severe plastic deformation [J]. Oxid. Met., 2018, 89: 415
26 Lu Y H, Wang Z B, Song Y Y, et al. Effects of pre-formed nanostructured surface layer on oxidation behaviour of 9Cr2WVTa steel in air and liquid Pb-Bi eutectic alloy [J]. Corros. Sci., 2016, 102: 301
27 Ungár T. Dislocation densities, arrangements and character from X-ray diffraction experiments [J]. Mater. Sci. Eng., 2001, A309-310: 14
28 Chen S H, Jin X J, Rong L J. Improving the strength and ductility of reduced activation ferritic/martensitic steel by cold-swaging and post-annealing [J]. Mater. Sci. Eng., 2015, A631: 139
29 Jin X J, Chen S H, Rong L J. Microstructure modification and mechanical property improvement of reduced activation ferritic/martensitic steel by severe plastic deformation [J]. Mater. Sci. Eng., 2018, A712: 97
30 Gupta R K, Birbilis N. The influence of nanocrystalline structure and processing route on corrosion of stainless steel: A review [J]. Corros. Sci., 2015, 92: 1
31 Mehrer H. Diffusion in Solids: Fundamentals, Methods, Materials, Diffusion-Controlled Processes [M]. Berlin Heidelberg: Springer, 2007: 117
32 Bakaev A, Terentyev D, He X, et al. Interaction of carbon-vacancy complex with minor alloying elements of ferritic steels [J]. J. Nucl. Mater., 2014, 451: 82
33 Feltham P. On the formation of point defects in metals by plastic deformation [J]. Phys. Stat. Sol., 1964, 6: 235
34 Young D J. High Temperature Oxidation and Corrosion of Metals [M]. Amsterdam: Elsevier, 2008: 37
35 Jin X J, Chen S H, Rong L J. Effects of Mn on the mechanical properties and high temperature oxidation of 9Cr2WVTa steel [J]. J. Nucl. Mater., 2017, 494: 103
36 International Atomic Energy Agency. Comparative Assessment of Thermophysical and Thermohydraulic Characteristics of Lead, Lead-Bismuth and Sodium Coolants for Fast Reactors [M]. Vienna: IAEA, 2002: 24
[1] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] 徐文国, 郝文江, 李应举, 赵庆彬, 卢炳聿, 郭和一, 刘天宇, 冯小辉, 杨院生. 微量Al、Ti对Inconel 690合金高温氧化行为的影响[J]. 金属学报, 2023, 59(12): 1547-1558.
[3] 刘路军, 刘政, 刘仁辉, 刘永. Nd90Al10 晶界调控对晶界扩散磁体磁性能和微观结构的影响[J]. 金属学报, 2023, 59(11): 1457-1465.
[4] 李赛, 杨泽南, 张弛, 杨志刚. 珠光体-奥氏体相变中扩散通道的相场法研究[J]. 金属学报, 2023, 59(10): 1376-1388.
[5] 沈莹莹, 张国兴, 贾清, 王玉敏, 崔玉友, 杨锐. SiCf/TiAl复合材料界面反应及热稳定性[J]. 金属学报, 2022, 58(9): 1150-1158.
[6] 李细锋, 李天乐, 安大勇, 吴会平, 陈劼实, 陈军. 钛合金及其扩散焊疲劳特性研究进展[J]. 金属学报, 2022, 58(4): 473-485.
[7] 化雨, 陈建国, 余黎明, 司永宏, 刘晨曦, 李会军, 刘永长. 高Cr铁素体耐热钢与奥氏体耐热钢的异种材料扩散连接接头组织演变及力学性能[J]. 金属学报, 2022, 58(2): 141-154.
[8] 刘仲武, 何家毅. 钕铁硼永磁晶界扩散技术和理论发展的几个问题[J]. 金属学报, 2021, 57(9): 1155-1170.
[9] 李娟, 赵宏龙, 周念, 张英哲, 秦庆东, 苏向东. CoCrFeNiCu高熵合金与304不锈钢真空扩散焊[J]. 金属学报, 2021, 57(12): 1567-1578.
[10] 刘晨曦, 毛春亮, 崔雷, 周晓胜, 余黎明, 刘永长. 低活化铁素体/马氏体钢组织调控及其固相连接研究进展[J]. 金属学报, 2021, 57(11): 1521-1538.
[11] 孙正阳, 杨超, 柳文波. UO2烧结过程的相场模拟[J]. 金属学报, 2020, 56(9): 1295-1303.
[12] 王超, 张旭, 王玉敏, 杨青, 杨丽娜, 张国兴, 吴颖, 孔旭, 杨锐. SiCf/Ti65复合材料界面反应与基体相变机理[J]. 金属学报, 2020, 56(9): 1275-1285.
[13] 丁文, 王小京, 刘宁, 秦亮. CoCrFeMnNi高熵合金作为中间层的Cu/304不锈钢扩散连接研究[J]. 金属学报, 2020, 56(8): 1084-1090.
[14] 孙正阳, 王昱天, 柳文波. 气孔与晶界相互作用的相场模拟[J]. 金属学报, 2020, 56(12): 1643-1653.
[15] 姜霖, 张亮, 刘志权. Al中间层和Ni(V)过渡层对Co/Al/Cu三明治结构靶材背板组件焊接残余应力的影响[J]. 金属学报, 2020, 56(10): 1433-1440.