| 超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响 |
陈胜虎( ), 戎利建 |
| 中国科学院金属研究所 中国科学院核用材料与安全评价重点实验室 沈阳 110016 |
|
| Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic |
CHEN Shenghu( ), RONG Lijian |
| CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
陈胜虎, 戎利建. 超细晶铁素体-马氏体钢的高温氧化成膜特性及其对Pb-Bi腐蚀行为的影响[J]. 金属学报, 2021, 57(8): 989-999.
Shenghu CHEN,
Lijian RONG.
Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic[J]. Acta Metall Sin, 2021, 57(8): 989-999.
| 1 |
Yvon P. Structural Materials for Generation Ⅳ Nuclear Reactors [M]. Duxford: Woodhead Publishing, 2017: 24
|
| 2 |
OECD/NEA Nuclear Science Committee, translated by Rong L J, Zhang Y T, Lu S P, et al. Handbook on Lead-Bismuth Eutectic Alloy and Lead: Properties, Materials Compatibility, Thermal-hydraulics and Technologies [M]. Beijing: Science Press, 2007: 3
|
| 2 |
OECD/NEA Nuclear Science Committee著, 戎利建, 张玉妥, 陆善平等译. 铅与铅铋共晶合金手册——性能、材料相容性、热工水力学和技术 [M]. 北京: 科学出版社, 2007: 3
|
| 3 |
Han J S, Liu B, Li W Q. Summary of lead-cooled fast reactor research [J]. Nucl. Sci. Technol., 2018, 6(3): 87
|
| 3 |
韩金盛, 刘 滨, 李文强. 铅冷快堆研究概述 [J]. 核科学与技术, 2018, 6(3): 87
|
| 4 |
Zhang J S. A review of steel corrosion by liquid lead and lead-bismuth [J]. Corros. Sci., 2009, 51: 1207
|
| 5 |
Gorynin I V, Karzov G P, Markov V G, et al. Structural materials for atomic reactors with liquid metal heat-transfer agents in the form of lead or lead-bismuth alloy [J]. Met. Sci. Heat Treat., 1999, 41: 384
|
| 6 |
Gong X, Marmy P, Yin Y. The role of oxide films in preventing liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic [J]. J. Nucl. Mater., 2018, 509: 401
|
| 7 |
Tsisar V. Influence of rolling and preoxidation on the oxidation resistance of EP823 steel in static lead melt [J]. Probl. Atom. Sci. Technol., 2012, 78(2): 89
|
| 8 |
Lillard R S, Valot C, Hill M A, et al. Influence of preoxidation on the corrosion of steels in liquid lead-bismuth eutectic [J]. Corrosion, 2004, 60: 1031
|
| 9 |
Yaskiv O I, Kukhar I S, Fedirko V M. Effect of preliminary diffusion oxidation on mechanical properties of ferritic steel in oxygen-containing lead [J]. Fusion Eng. Des., 2015, 101: 134
|
| 10 |
Klueh R L, Harries D R. High-Chromium Ferritic and Martensitic Steels for Nuclear Applications [M]. West Conshohocken: American Society for Testing and Materials, 2001: 5
|
| 11 |
Tan L, Hoelzer D T, Busby J T, et al. Microstructure control for high strength 9Cr ferritic-martensitic steels [J]. J. Nucl. Mater., 2012, 422: 45
|
| 12 |
Chen S H, Jin X J, Rong L J. Microstructural evolution and mechanical properties of ultrafine-grained ferritic-martensitic steel during thermal aging [J]. Metall. Mater. Trans., 2020, 51A: 5154
|
| 13 |
Zinkle S J, Was G S. Materials challenges in nuclear energy [J]. Acta Mater., 2013, 61: 735
|
| 14 |
Martinelli L, Balbaud-Célérier F, Terlain A, et al. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part I) [J]. Corros. Sci., 2008, 50: 2523
|
| 15 |
Martinelli L, Balbaud-Célérier F, Terlain A, et al. Oxidation mechanism of an Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy at 470oC (Part II) [J]. Corros. Sci., 2008, 50: 2537
|
| 16 |
Martinelli L, Balbaud-Célérier F, Picard G, et al. Oxidation mechanism of a Fe-9Cr-1Mo steel by liquid Pb-Bi eutectic alloy (Part III) [J]. Corros. Sci., 2008, 50: 2549
|
| 17 |
Wang J, Lu S P, Rong L J, et al. Effect of silicon on the oxidation resistance of 9wt.% Cr heat resistance steels in 550oC lead-bismuth eutectic [J]. Corros. Sci., 2016, 111: 13
|
| 18 |
Yang K, Yan W, Wang Z G, et al. Development of a novel structural material (SIMP steel) for nuclear equipment with balanced resistances to high temperature, radiation and liquid metal corrosion [J]. Acta Metall. Sin., 2016, 52: 1207
|
| 18 |
杨 柯, 严 伟, 王志光等. 核用新型耐高温、抗辐照、耐液态金属腐蚀结构材料——SIMP钢的研究进展 [J]. 金属学报, 2016, 52: 1207
|
| 19 |
Lu Y H, Song Y Y, Chen S H, et al. Effects of Al and Si on mechanical properties and corrosion resistance in liquid Pb-Bi eutectic of 9Cr2WVTa steel [J]. Acta Metall. Sin., 2016, 52: 298
|
| 19 |
鲁艳红, 宋元元, 陈胜虎等. Al和Si对9Cr2WVTa钢力学性能及耐Pb-Bi腐蚀性能的影响 [J]. 金属学报, 2016, 52: 298
|
| 20 |
Chen S H, Rong L J. Effect of silicon on the microstructure and mechanical properties of reduced activation ferritic/martensitic steel [J]. J. Nucl. Mater., 2015, 459: 13
|
| 21 |
Peng X, Wang F H. High temperature corrosion of nanocrystalline metallic materials [J]. Acta Metall. Sin., 2014, 50: 202
|
| 21 |
彭 晓, 王福会. 纳米晶金属材料的高温腐蚀行为 [J]. 金属学报, 2014, 50: 202
|
| 22 |
Singh Raman R K, Khanna A S, Tiwari R K. et al. Influence of grain size on the oxidation resistance of 2.25Cr-1Mo steel [J]. Oxid. Met., 1992, 37: 1
|
| 23 |
Trindade V, Christ H J, Krupp U. Grain-size effects on the high-temperature oxidation behaviour of chromium Steels [J]. Oxid. Met., 2010, 73: 551
|
| 24 |
Chen S H, Jin X J, Rong L J. Improvement in high temperature oxidation resistance of 9%Cr ferritic-martensitic steel by enhanced diffusion of Mn [J]. Oxid. Met., 2016, 85: 189
|
| 25 |
Chen S H, Rong L J. Roles of Mn in the high-temperature air oxidation of 9Cr ferritic-martensitic steel after severe plastic deformation [J]. Oxid. Met., 2018, 89: 415
|
| 26 |
Lu Y H, Wang Z B, Song Y Y, et al. Effects of pre-formed nanostructured surface layer on oxidation behaviour of 9Cr2WVTa steel in air and liquid Pb-Bi eutectic alloy [J]. Corros. Sci., 2016, 102: 301
|
| 27 |
Ungár T. Dislocation densities, arrangements and character from X-ray diffraction experiments [J]. Mater. Sci. Eng., 2001, A309-310: 14
|
| 28 |
Chen S H, Jin X J, Rong L J. Improving the strength and ductility of reduced activation ferritic/martensitic steel by cold-swaging and post-annealing [J]. Mater. Sci. Eng., 2015, A631: 139
|
| 29 |
Jin X J, Chen S H, Rong L J. Microstructure modification and mechanical property improvement of reduced activation ferritic/martensitic steel by severe plastic deformation [J]. Mater. Sci. Eng., 2018, A712: 97
|
| 30 |
Gupta R K, Birbilis N. The influence of nanocrystalline structure and processing route on corrosion of stainless steel: A review [J]. Corros. Sci., 2015, 92: 1
|
| 31 |
Mehrer H. Diffusion in Solids: Fundamentals, Methods, Materials, Diffusion-Controlled Processes [M]. Berlin Heidelberg: Springer, 2007: 117
|
| 32 |
Bakaev A, Terentyev D, He X, et al. Interaction of carbon-vacancy complex with minor alloying elements of ferritic steels [J]. J. Nucl. Mater., 2014, 451: 82
|
| 33 |
Feltham P. On the formation of point defects in metals by plastic deformation [J]. Phys. Stat. Sol., 1964, 6: 235
|
| 34 |
Young D J. High Temperature Oxidation and Corrosion of Metals [M]. Amsterdam: Elsevier, 2008: 37
|
| 35 |
Jin X J, Chen S H, Rong L J. Effects of Mn on the mechanical properties and high temperature oxidation of 9Cr2WVTa steel [J]. J. Nucl. Mater., 2017, 494: 103
|
| 36 |
International Atomic Energy Agency. Comparative Assessment of Thermophysical and Thermohydraulic Characteristics of Lead, Lead-Bismuth and Sodium Coolants for Fast Reactors [M]. Vienna: IAEA, 2002: 24
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|