一种单晶高温合金的弹性性能的各向异性 |
刘金来( ), 叶荔华, 周亦胄, 李金国, 孙晓峰 |
中国科学院金属研究所 沈阳 110016 |
|
Anisotropy of Elasticity of a Ni Base Single Crystal Superalloy |
LIU Jinlai( ), YE Lihua, ZHOU Yizhou, LI Jinguo, SUN Xiaofeng |
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
刘金来, 叶荔华, 周亦胄, 李金国, 孙晓峰. 一种单晶高温合金的弹性性能的各向异性[J]. 金属学报, 2020, 56(6): 855-862.
Jinlai LIU,
Lihua YE,
Yizhou ZHOU,
Jinguo LI,
Xiaofeng SUN.
Anisotropy of Elasticity of a Ni Base Single Crystal Superalloy[J]. Acta Metall Sin, 2020, 56(6): 855-862.
[1] |
Wang L N, Liu Y, Yu J J, et al. Orientation and temperature dependence of yielding and deformation behavior of a nickel-base single crystal superalloy [J]. Mater. Sci. Eng., 2009, A505: 144
|
[2] |
Vattré A, Devincre B, Roos A. Orientation dependence of plastic deformation in nickel-based single crystal superalloys: Discrete-continuous model simulations [J]. Acta Mater., 2010, 58: 1938
doi: 10.1016/j.actamat.2009.11.037
|
[3] |
Liu J L, Jin T, Sun X F, et al. Anisotropy of stress rupture properties of a Ni base single crystal superalloy at two temperatures [J]. Mater. Sci. Eng., 2008, A479: 277
|
[4] |
Hou N X, Gou W X, Wen Z X, et al. The influence of crystal orientations on fatigue life of single crystal cooled turbine blade [J]. Mater. Sci. Eng., 2008, A492: 413
|
[5] |
Gunturi S S K, MacLachlan D W, Knowles D M. Anisotropic creep in CMSX-4 in orientations distant from 〈001〉 [J]. Mater. Sci. Eng., 2000, A289: 289
|
[6] |
Prikhodko S V, Carnes J D, Isaak D G, et al. Elastic constants of a Ni-12.69 at.% Al alloy from 295 to 1300 K [J]. Scr. Mater., 1997, 38: 67
|
[7] |
Prikhodko S V, Yang H, Ardell A J, et al. Temperature and composition dependence of the elastic constants of Ni3Al [J]. Metall. Mater. Trans., 1999, 30A: 2403
|
[8] |
Siebörger D, Knake H, Glatzel U. Temperature dependence of the elastic moduli of the nickel-base superalloy CMSX-4 and its isolated phases [J]. Mater. Sci. Eng., 2001, A298: 26
|
[9] |
Wolf R J, Mansour K A, Lee M W, et al. Temperature dependence of elastic constants of embedded-atom models of palladium [J]. Phys. Rev., 1992, 46B: 8027
|
[10] |
Cheng D Y, Wang S Q, Ye H Q. First-principles calculations of the elastic properties of ZrC and ZrN [J]. J. Alloys Compd., 2004, 377: 221
|
[11] |
Wang S Q, Ye H Q. First-principles study on elastic properties and phase stability of III-V compounds [J]. Phys. Stat. Sol., 2003, 240B: 45
|
[12] |
Wen M, Barnoush A, Yokogawa K. Calculation of all cubic single-crystal elastic constants from single atomistic simulation: Hydrogen effect and elastic constants of nickel [J]. Comput. Phys. Commun., 2011, 182: 1621
|
[13] |
Jamal M, Asadabadi S J, Ahmad I, et al. Elastic constants of cubic crystals [J]. Comput. Mater. Sci., 2014, 95: 592
|
[14] |
Duan L J, Liu Y C. Relationships between elastic constants and EAM/FS potential functions for cubic crystals [J]. Acta Metall. Sin., 2020, 56: 112
|
[14] |
段灵杰, 刘永长. 立方晶体弹性常数和EAM/FS势函数的关系 [J]. 金属学报, 2020, 56: 112
|
[15] |
Huang X Y, Hu B R, Chen X W, et al. Mechanical Behavior of Aeronautical Materials [M]. Beijing: National Defense Industry Press, 2012: 118
|
[15] |
黄新跃, 胡本润, 陈新文等. 航空材料的力学行为 [M]. 北京: 国防工业出版社, 2012: 118
|
[16] |
Aba-Perea P E, Pirling T, Withers P J, et al. Determination of the high temperature elastic properties and diffraction elastic constants of Ni-base superalloys [J]. Mater. Des., 2016, 89: 856
|
[17] |
Ma S, Brown D, Bourke M A M, et al. Microstrain evolution during creep of a high volume fraction superalloy [J]. Mater. Sci. Eng., 2005, A399: 141
|
[18] |
Crimp M A. HREM examination of [101] screw dislocations in Ni3Al [J]. Philos. Mag. Lett., 1989, 60: 45
|
[19] |
Ting T C T. On anisotropic elastic materials for which Young's modulus E(n) is independent of n or the shear modulus G(n, m) is independent of n and m [J]. J. Elasticity, 2005, 81: 271
|
[20] |
Knowles K M, Howie P R. The directional dependence of elastic stiffness and compliance shear coefficients and shear moduli in cubic materials [J]. J. Elasticity, 2015, 120: 87
|
[21] |
Wallow F, Neite G, Schröer W, et al. Stiffness constants, dislocation line energies, and tensions of Ni3Al and of the γ'-phases of NIMONIC 105 and of NIMONIC PE16 [J]. Phys. Status Solidi, 1987, 99A: 483
|
[22] |
Dye D, Coakley J, Vorontsov V A, et al. Elastic moduli and load partitioning in a single-crystal nickel superalloy [J]. Scr. Mater., 2009, 61: 109
|
[23] |
Prikhodko S V, Ma Y, Ardell A J, et al. Elastic constants of face-centered cubic and L12 Ni-Si alloys: Composition and temperature dependence [J]. Metall. Mater. Trans., 2003, 34A: 1863
|
[24] |
Xing L L, Yang H, Zhang G, et al. Temperature and pressure dependence of elastic moduli of MgO and Cu [J]. J. Atom. Mol. Phys., 2017, 34: 547
|
[24] |
邢玲玲, 杨 欢, 张 刚等. MgO和Cu的弹性常数随温度及压强变化关系的研究 [J]. 原子与分子物理学报, 2017, 34: 547
|
[25] |
Wang Z Q, Stoica A D, Ma D, et al. Diffraction and single-crystal elastic constants of Inconel 625 at room and elevated temperatures determined by neutron diffraction [J]. Mater. Sci. Eng., 2016, A674: 406
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|