					引用本文:
						|  |  
    					|  |  
    					| 籽晶制备及Ti-47Al合金PST晶体取向控制 |  
						| 金浩1,2,贾清1,刘荣华1,线全刚1,崔玉友1,徐东生1,杨锐1(  ) |  
					| 1. 中国科学院金属研究所 沈阳 110016 2. 中国科学院大学 北京 100049
 |  
						|  |  
    					| Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy |  
						| JIN Hao1,2,JIA Qing1,LIU Ronghua1,XIAN Quangang1,CUI Yuyou1,XU Dongsheng1,YANG Rui1(  ) |  
						| 1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2. University of Chinese Academy of Sciences, Beijing 100049, China
 |  
								金浩, 贾清, 刘荣华, 线全刚, 崔玉友, 徐东生, 杨锐. 籽晶制备及Ti-47Al合金PST晶体取向控制[J]. 金属学报, 2019, 55(12): 1519-1526.	
																												JIN Hao,
																								JIA Qing,
																								LIU Ronghua,
																								XIAN Quangang,
																								CUI Yuyou,
																								XU Dongsheng,
																												YANG Rui. 
				Seed Preparation and Orientation Control of PST Crystals of Ti-47Al Alloy[J]. Acta Metall Sin, 2019, 55(12): 1519-1526.
 
					
						| 
								
									|  
          
          
            
             
			              
            
									            
									                
																														  
																| | [1] | Yang R. Advances and challenges of TiAl base alloys [J]. Acta Metall. Sin., 2015, 51: 129 |  | [1] | (杨 锐. 钛铝金属间化合物的进展与挑战 [J]. 金属学报, 2015, 51: 129) |  | [2] | Wu X H. Review of alloy and process development of TiAl alloys [J]. Intermetallics, 2006, 14: 1114 |  | [3] | Kim Y W, Dimiduk D M. Progress in the understanding of gamma titanium aluminides [J]. JOM, 1991, 43(8): 40 |  | [4] | Lin J P, Zhao L L, Li G Y, et al. Effect of Nb on oxidation behavior of high Nb containing TiAl alloys [J]. Intermetallics, 2011, 19: 131 |  | [5] | Liu Z C, Lin J P, Li S J, et al. Effects of Nb and Al on the microstructures and mechanical properties of high Nb containing TiAl base alloys [J]. Intermetallics, 2002, 10: 653 |  | [6] | Inui H, Oh M H, Nakamura A, et al. Room-temperature tensile deformation of polysynthetically twinned (PST) crystals of TiAl [J]. Acta Metall. Mater., 1992, 40: 3095 |  | [7] | Oh M H, Inui H, Misaki M, et al. Environmental-effects on the room-temperature ductility of polysynthetically twinned (PST) crystals of binary and some ternary TiAl compounds [A]. Proceeding of the 5th High-Temperature Ordered Intermetallic Alloys V [C]. Boston, MA: Mater. Res. Soc. Symp. Proc., 1993, 288: 1001 |  | [8] | Johnson D R, Inui H, Yamaguchi M. Directional solidification and microstructural control of the TiAl/Ti3Al lamellar microstructure in TiAl-Si alloys [J]. Acta Mater., 1996, 44: 2523 |  | [9] | Johnson D R, Masuda Y, Inui H, et al. Alignment of the TiAl/Ti3Al lamellar microstructure in TiAl alloys by growth from a seed material [J]. Acta Mater., 1997, 45: 2523 |  | [10] | Umeda H, Kishida K, Inui H, et al. Effects of Al-concentration and lamellar spacing on the room-temperature strength and ductility of PST crystals of TiAl [J]. Mater. Sci. Eng., 1997, A239-240: 336 |  | [11] | Yamanaka T, Johnson D R, Inui H, et al. Directional solidification of TiAl-Re-Si alloys with aligned γ/α2 lamellar microstructures [J]. Intermetallics, 1999, 7: 779 |  | [12] | Johnson D R, Inui H, Muto S, et al. Microstructural development during directional solidification of α-seeded TiAl alloys [J]. Acta Mater., 2006, 54: 1077 |  | [13] | Fu H Z, Su Y Q, Guo J J, et al. The solidification behavior of high temperature intermetallics [J]. Acta Metall. Sin., 2002, 38: 1127 |  | [13] | (傅恒志, 苏彦庆, 郭景杰等. 高温金属间化合物的定向凝固特性 [J]. 金属学报, 2002, 38: 1127) |  | [14] | Yamaguchi M, Inui H, Yokoshima S, et al. Recent progress in our understanding of deformation and fracture of two-phase and single-phase TiAl alloys [J]. Mater. Sci. Eng., 1996, A213: 25 |  | [15] | Lee H N, Johnson D R, Inui H, et al. Microstructural control through seeding and directional solidification of TiAl alloys containing Mo and C [J]. Acta Mater., 2000, 48: 3221 |  | [16] | Lee H N, Johnson D R, Inui H, et al. Directional solidification and creep deformation of a Ti-46Al-1.5Mo-0.2C (at. %) alloy [J]. Intermetallics, 2002, 10: 841 |  | [17] | Lee H N, Johnson D R, Inui H, et al. A composition window in the TiAl-Mo-Si system suitable for lamellar structure control through seeding and directional solidification [J]. Mater. Sci. Eng., 2002, A329-331: 19 |  | [18] | Kim J H, Kim S W, Lee H N, et al. Effects of Si and C additions on the thermal stability of directionally solidified TiAl-Nb alloys [J]. Intermetallics, 2005, 13: 1038 |  | [19] | Luo W Z, Shen J, Li Q L, et al. Microstructural evolution of Ti-47Al alloy during directional solidification by seeding method [J]. Acta Metall. Sin., 2007, 43: 897 |  | [19] | (罗文忠, 沈 军, 李庆林等. Ti-47Al合金籽晶法定向凝固过程中的组织演化 [J]. 金属学报, 2007, 43: 897) |  | [20] | Zheng X Q, Shen J, Ding H S, et al. Preparation of fully lamellar microstructure Ti-43Al-3Si alloy with alignment perpendicular to the growth direction in steel mould [J]. Mater. Rep., 2005, 19(3): 118 |  | [20] | (郑循强, 沈 军, 丁宏升等. 单一取向的Ti-43Al-3Si全片层组织制备 [J]. 材料导报, 2005, 19(3): 118) |  | [21] | Luo W Z, Shen J, Li Q L, et al. Effects of growth rate on microstructure of directionally solidified Ti-43Al-3Si alloy with a seed technique [J]. Acta Metall. Sin., 2006, 42: 1238 |  | [21] | (罗文忠, 沈 军, 李庆林等. 抽拉速率对Ti-43Al-3Si合金籽晶法定向凝固组织的影响 [J]. 金属学报, 2006, 42: 1238) |  | [22] | Fan J L, Li X Z, Guo J J, et al. Structure evolution of directionally solidified Ti-43Al-3Si alloy I. Microstructure evolution in the transition region [J]. Acta Metall. Sin., 2009, 45: 302 |  | [22] | (樊江磊, 李新中, 郭景杰等. 定向凝固Ti-43Al-3Si合金的组织演化规律 Ⅰ. 初始过渡区组织演化规律 [J]. 金属学报, 2009, 45: 302) |  | [23] | Li X Z, Fan J L, Guo J J, et al. Structure evolution of directionally solidified Ti-43Al-3Si alloy II. Microstructure evolution in the steady-state growth region [J]. Acta Metall. Sin., 2009, 45: 308 |  | [23] | (李新中, 樊江磊, 郭景杰等. 定向凝固Ti-43Al-3Si合金的组织演化规律 Ⅱ. 稳态生长区组织演化规律 [J]. 金属学报, 2009, 45: 308) |  | [24] | Liu R H, Cui Y Y, Yang R. Effect of seed shape and size on the seeding of TiAl directional solidification [J]. Rare Met. Mater. Eng., 2008, 37(suppl.3): 141 |  | [24] | (刘荣华, 崔玉友, 杨 锐. 籽晶形状和尺寸对TiAl合金引晶生长的影响 [J]. 稀有金属材料与工程, 2008, 37(增刊3): 141) |  | [25] | Luo W Z, Shen J, Li Q L, et al. Preparation of aligned lamellar microstructure in TiAl alloys by directional solidification with a seed technique [J]. Acta Metall. Sin., 2007, 43: 1287 |  | [25] | (罗文忠, 沈 军, 李庆林等. TiAl合金定向全片层组织的籽晶法制备 [J]. 金属学报, 2007, 43: 1287) |  | [26] | Koohpayeh S M, Fort D, Abell J S. The optical floating zone technique: A review of experimental procedures with special reference to oxides [J]. Prog. Cryst. Growth Charact. Mater., 2008, 54: 121 |  | [27] | Koohpayeh S M, Fort D, Bradshaw A, et al. Thermal characterization of an optical floating zone furnace: A direct link with controllable growth parameters [J]. J. Cryst. Growth, 2009, 311: 2513 | 
 |  
             
												
											    	