| 钢的等离子体基低能离子注入的传质机制 |
| 雷明凯 朱雪梅 袁力江 张仲麟 |
| 大连理工大学材料工程系; 大连 116024 |
|
引用本文:
雷明凯; 朱雪梅; 袁力江; 张仲麟 . 钢的等离子体基低能离子注入的传质机制[J]. 金属学报, 1999, 35(7): 767-769 .
[1]Conrad J R. Mater Sci Eng, 1989; 116A: 197 [2]Collins G A,Hutchings R,Tendys J.Mater,Sci Eng,1991;139A:171 [3]Byeli A V, Shikh S K, Kharko V V Wear, 1992 159: 185 [4]Zhang Z L, Bell T Surf Eng, 1985;1:131 [5]Lei M K, Zhang Z L.J Vac Sci Technol, 1995; 13A: 2986 [6]Lei M K; Zhang Z L.J Vac Sci Technol, 1998; 16A: 524 [7]Collins G A, Tendys J.J Vac Sci Technol, 1994; 13B: 875 [8]Lei M K, Zhans Z L.Surf Coat Technol,1997 91: 25 [9]Zhang Z L,Lei M K,Yu an L J,Kong C J.Heat Treat Met,19962(10): 14(张仲麟,雷明凯,袁力江,孔常静金属热处理,1996;(10): 14) [10]Lei M K,Wang P,Huang Y,Yu W W,Yuan L J,Zhang Z L.Wear,1997;209:301 |
|