| 超塑变形晶粒长大模型的修正与实验验证 |
| 曹富荣 雷方 崔建忠 温景林 |
| 东北大学材料与冶金学院; 沈阳 110006 |
|
引用本文:
曹富荣; 雷方; 崔建忠; 温景林 . 超塑变形晶粒长大模型的修正与实验验证[J]. 金属学报, 1999, 35(7): 770-772 .
[1]Clark M A,Alden T H.Acta Metall,1973;21:1195 [2]Wilkinson D S,Caceres C H.Acta Metall 1984;32:1335 [3]Sato E, Kuribsyashi K, Horiuchi R. Iron Steel Inst Jpn,1992 78:1414 [4]Hamilton C H. Metall Trans, 1989; 20A: 2783 [5]Campenni V D,Caceres C H.Scr Metall,1987;22:359 [6] Ashby M F, Verral R A. Acta Metall, 1973; 21: 149 [7]Herriot G,Suery M,Baudelet B.Scr Metall,1972;6:657 [8]Moles M D C,Davies G J.Scr Metall,1976;6:455 [9]Sagat S, Taplin D M R. Acta Metall, 1976; 24: 307 [10]Samuelsson L C A.Melton K N,Edington J W.Acta Metall,1976; 24:1017 [11]Rabinovich K,Trifonov V G.Acta Mater,1996 44:2073 [12] Kim W-Y, Hanada S, Takasugi T. Scr Mater, 1997; 37:1053 [13] Suery M, Baudelet B J Mater Sci, 1973 8: 363 [14] Naziri H, Pearce R. Acta Metall, 1974; 22: 1321 [15] Liu Q PhD Thesis,Harbin Institute of Technology, 1991 [16]Kaibyshev O A,Vaiev R Z,Astanin V V.Phys Status Solidi, 1976;35a:403 [17]Caceres C H,Wilkinson D S.J Mater Sci Lett,1984 3:395 [18]Valiev R Z, Kaibvshev O A. Fiz Met Metalloved,1976; 41: 382 [19]Cao F R,Cui J Z,Wen J L,Lei F Scr Mater,1999,to be published [20]Borisov Y V,Grunzin P L,Paulinov L V.Met Metalloved Christykh Met,1959;1:213 [21]Metenier P,Gonzalez-Doncel G,Ruano O A,Wolfenstine J, Sherby O D.Mater Sci Eng; 1990; A125: 195 [22]Taleff E M, Sherby O D.J Mater Res, 1992 7: 2131 [23]Chen I W. In: Baudelet B, Suery M eds, Proc Int Conf on Superplasticity,Paris:CNRS,1985:5.1 [24]Sato E, Kuribnyashi K,Horiuchi R.J Jpn Inst Met, 1991: 55:839 (佐藤英一,栗林一彦,倔内良日本金属学会志,1991;55: 839) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|