| 过热温度和冷却速率对过冷Ti熔体凝固过程的影响 |
樊丹丹, 许军锋, 钟亚男, 坚增运( ) |
| 西安工业大学材料与化工学院 西安 710021 |
|
| Effect of Superheated Temperature and Cooling Rate on the Solidification of Undercooled Ti Melt |
Dandan FAN, Junfeng XU, Yanan ZHONG, Zengyun JIAN( ) |
| School of Materials and Chemical Engineering, Xi'an Technological University, Xi'an 710021, China |
引用本文:
樊丹丹, 许军锋, 钟亚男, 坚增运. 过热温度和冷却速率对过冷Ti熔体凝固过程的影响[J]. 金属学报, 2018, 54(6): 844-850.
Dandan FAN,
Junfeng XU,
Yanan ZHONG,
Zengyun JIAN.
Effect of Superheated Temperature and Cooling Rate on the Solidification of Undercooled Ti Melt[J]. Acta Metall Sin, 2018, 54(6): 844-850.
| [1] | Jian Z Y, Chang F E, Ma W H, et al.Metal nucleation and undercooling[J]. Sci. China, 2000, 30E: 9(坚增运, 常芳娥, 马卫红等. 金属熔体的形核和过冷度[J]. 中国科学, 2000, 30E: 9) | | [2] | Mortensen A, Flemings M C.Solidification of binary hypoeutectic alloy matrix composite castings[J]. Metall. Mater. Trans., 1996, 27A: 595 | | [3] | Jian Z Y, Kuribayashi K, Jie W Q.Critical undercoolings for the transition from the lateral to continuous growth in undercooled silicon and germanium[J]. Acta Mater., 2004, 52: 3323 | | [4] | Xu J F, Xiang M, Dang B, et al.Relation of cooling rate, undercooling and structure for rapid solidification of iron melt[J]. Comput. Mater. Sci., 2017, 128: 98 | | [5] | Feng Y.Study on non-equilibrium solidification mechanism of Al-Si alloys [D]. Chongqing: Chongqing University, 2008(冯毅. Al-Si合金的非平衡凝固机理研究 [D]. 重庆: 重庆大学, 2008) | | [6] | Si N C, Zhao L G, Sun K Q.Influence of melt thermal history on structure of melt Al-Cu alloy[J]. Nonferrous Met., 2008, 60(4): 22(司乃潮, 赵罗根, 孙克庆. 熔体热历史对Al-Cu合金熔体结构的影响[J]. 有色金属, 2008, 60(4): 22) | | [7] | Li J Y, Liu R S, Zhou Z, et al.A simulation study for the effects of initial conditions of liquid metals on solidification microstructures[J]. Chin. J. At. Mol. Phys., 1998, 15(2): 193(李基永, 刘让苏, 周征等. 液态金属的初始状态对凝固微结构影响的模拟研究[J]. 原子与分子物理学报, 1998, 15(2): 193) | | [8] | Hou Z Y, Dong K J, Tian Z A, et al.Cooling rate dependence of solidification for liquid aluminium: A large-scale molecular dynamics simulation study[J]. Phys. Chem. Chem. Phys., 2016, 18: 17461 | | [9] | Hou Z Y, Tian Z A, Liu R S, et al.Formation mechanism of bulk nanocrystalline aluminium with multiply twinned grains by liquid quenching: A molecular dynamics simulation study[J]. Comput. Mater. Sci., 2015, 99: 256 | | [10] | Zhang H T, Liu R S, Hou Z Y, et al.A simulation study for the effects of cooling rate on evolution of microstructures during solidification of liquid metal Ga[J]. Acta Phys. Sin., 2006, 55: 2409(张海涛, 刘让苏, 侯兆阳等. 冷速对液态金属Ga凝固过程中微观结构演变影响的模拟研究[J]. 物理学报, 2006, 55: 2409) | | [11] | Zhang T, Zhang X R, Guan L.Molecular dynamics simulations of the solidification of liquid Au[J]. J. Shandong Univ. Technol., 2002, 32: 57(张弢, 张晓茹, 管立. 贵金属Au冷却过程的分子动力学研究[J]. 山东工业大学学报, 2002, 32: 57) | | [12] | Lin Y, Liu R S, Tian Z A, et al.Effect of cooling rates on microstructures during solidification process of liquid metal Zn[J]. Acta Phys.-Chim. Sin., 2008, 24: 250(林艳, 刘让苏, 田泽安等. 冷却速率对液态金属Zn快速凝固过程中微观结构的影响[J]. 物理化学学报, 2008, 24: 250) | | [13] | Allen M P.Introduction of molecular dynamics simulation [A]. Computational Soft Matter: From Synthetic Polymers to Proteins, Lecture Notes[C]. Julich: John von Neumann Institute for Computing, 2004: 43 | | [14] | Bhat M H, Molinero V, Soignard E, et al.Vitrification of a monatomic metallic liquid[J]. Nature, 2007, 448: 787 | | [15] | Pan S P, Qin J Y, Wang W M, et al.Origin of splitting of the second peak in the pair-distribution function for metallic glasses[J]. Phys. Rev., 2011, 84B: 092201 | | [16] | Alkhateb H, Al-Ostaz A, Cheng A H D. Molecular dynamics simulations of graphite-vinylester nanocomposites and their constituents[J]. Carbon Lett., 2010, 11: 316 | | [17] | Cao A J, Yuan Y T.Atomistic study on the strength of symmetric tilt grain boundaries in graphene[J]. Appl. Phys. Lett., 2012, 100: 211912 | | [18] | Ebrahimi S, Montazeri A, Rafii-Tabar H.Molecular dynamics study of the interfacial mechanical properties of the graphene-collagen biological nanocomposite[J]. Comput. Mater. Sci., 2013, 69: 29 | | [19] | Mortazavi B, Ahzi S.Thermal conductivity and tensile response of defective graphene: A molecular dynamics study[J]. Carbon, 2013, 63: 460 | | [20] | Xia L, Chen S, Lu J S, et al.The development and application of the interatomic potentials of precious metals for molecular dynamics simulation[J]. Preci. Met., 2013, 34(4): 82(夏璐, 陈松, 陆建生等. 分子动力学模拟用贵金属势函数的应用与发展[J]. 贵金属, 2013, 34(4): 82) | | [21] | Okita S, Verestek W, Sakane S, et al.Molecular dynamics simulations investigating consecutive nucleation, solidification and grain growth in a twelve-million-atom Fe-system[J]. J. Cryst. Growth, 2017, 474: 140 | | [22] | Plimpton S.Fast parallel algorithms for short-range molecular dynamics[J]. J. Comput. Phys., 1995, 117: 1 | | [23] | Nosé S.A molecular dynamics method for simulations in the canonical ensemble[J]. Mol. Phys., 1984, 52: 255 | | [24] | Hoover W G.Canonical dynamics: Equilibrium phase-space distributions[J]. Phys. Rev., 1985, 31A: 1695 | | [25] | Daw M S, Baskes M I.Embedded-atom method: Derivation and application to impurities, surfaces, and other defects in metals[J]. Phys. Rev., 1984, 29B: 6443 | | [26] | Daw M S.Model of metallic cohesion: The embedded-atom method[J]. Phys. Rev., 1989, 39B: 7441 | | [27] | Gao A H.Effect of melt thermal history on the solidification behaviors of metals [D]. Xi'an: Xi'an Technological University, 2013(高阿红. 熔体热历史对金属凝固特性影响的研究 [D]. 西安: 西安工业大学, 2013) | | [28] | Zhong Y N.Study on the structure of metal melt and solidification behavior by molecular dynamic simulation method [D]. Xi'an: Xi'an Technological University, 2016(钟亚男. 金属熔体结构及凝固特性的分子动力学模拟 [D]. 西安: 西安工业大学, 2016) | | [29] | Xu J F, Dang B, Fan D D, et al.Effect of melt superheating treatment on the latent heat release of Sn[J]. Metall. Mater. Trans., 2017, 48A: 1133 | | [30] | Sapozhnikov F A, Ionov G V, Dremov V V.An adaptive template method for analyzing crystal structures and defects in molecular dynamics simulations of high-rate deformations[J]. Russ. J. Phys. Chem., 2008, 2B: 238 | | [31] | Jian Z Y, Chen J, Chang F E, et al.Simulation of molecular dynamics of silver subcritical nuclei and crystal clusters during solidification[J]. Sci. China Technol. Sci., 2010, 53: 3203 | | [32] | Jian Z Y, Gao A H, Chang F E, et al.Molecular dynamics simulation of the critical and subcritical nuclei during solidification of nickel melt[J]. Acta Phys. Sin., 2013, 62: 056102(坚增运, 高阿红, 常芳娥等. Ni熔体凝固过程中临界晶核和亚临界晶核的分子动力学模拟[J]. 物理学报, 2013, 62: 056102) | | [33] | Nie Y Z, Xie Y Q, Peng H J, et al.First-principles study of thermal properties of metal Ti[J]. J. Cent. South Univ.(Sci. Technol.), 2007, 38: 1072(聂耀庄, 谢佑卿, 彭红建等. 金属Ti热学性质第一原理研究[J]. 中南大学学报(自然科学版), 2007, 38: 1072) | | [34] | Wang L, Bian X F, Li H.Liquid-solid transition and crystal growth of metal Cu by molecular dynamics simulation[J]. J. Phys. Chem. Sin., 2000, 16: 825(王丽, 边秀房, 李辉. 金属Cu液固转变及晶体生长的分子动力学模拟[J]. 物理化学学报, 2000, 16: 825) | | [35] | Schroers J.Condensed-matter physics: Glasses made from pure metals[J]. Nature, 2014, 512: 142 | | [36] | Zhong L, Wang J W, Sheng H W, et al.Formation of monatomic metallic glasses through ultrafast liquid quenching[J]. Nature, 2014, 512: 177 |
|
|