| Al薄膜对玻璃纤维增强树脂基复合材料电磁性能的影响 |
陈育秋1,2, 祖亚培1, 宫骏1, 孙超1( ), 王晨3 |
1 中国科学院金属研究所 沈阳 110016 2 中国科学院大学 北京 100049 3 澳汰尔工程软件(上海)有限公司 上海 200436 |
|
| Effect of Al Film on the Electromagnetic Properties of Glass Fiber Reinforced Resin Matrix Composite |
Yuqiu CHEN1,2, Yapei ZU1, Jun GONG1, Cao SUN1( ), Chen WANG3 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 University of Chinese Academy of Sciences, Beijing 100049, China 3 Altair Engineering Software (Shanghai) Co., Ltd., Shanghai 200436, China |
引用本文:
陈育秋, 祖亚培, 宫骏, 孙超, 王晨. Al薄膜对玻璃纤维增强树脂基复合材料电磁性能的影响[J]. 金属学报, 2017, 53(11): 1511-1520.
Yuqiu CHEN,
Yapei ZU,
Jun GONG,
Cao SUN,
Chen WANG.
Effect of Al Film on the Electromagnetic Properties of Glass Fiber Reinforced Resin Matrix Composite[J]. Acta Metall Sin, 2017, 53(11): 1511-1520.
| [1] | Zhou H, Qu S B, Peng W D, et al.A novel frequency selective surface loaded with resistance films absobers[J]. Acta Phys. Sin., 2012, 61: 104201(周航, 屈绍波, 彭卫东等. 一种加载电阻膜吸波材料的新型频率选择表面[J]. 物理学报, 2012, 61: 104201) | | [2] | Cheng Y Z, Nie Y, Gong R Z, et al.Design of an ultrathin and wideband metamaterial absorber based on resistance film and fractal frequency selective surface[J]. Acta Phys. Sin., 2013, 62: 044103(程用志, 聂彦, 龚荣洲等. 基于电阻膜与分形频率选择表面的超薄宽频带超材料吸波体的设计[J]. 物理学报, 2013, 62: 044103) | | [3] | Pang Y Q, Cheng H F, Zhou Y J, et al.Ultrathin and broadband high impedance surface absorbers based on metamaterial substrates[J]. Opt. Express, 2012, 20: 12515 | | [4] | Zhao D L, Song Y L, Zhu Y P.New microwave absorber based on resonant high-impedance surface[J]. J. Nanjing Univ. Sci. Technol.(Nat. Sci.), 2010, 34: 136(赵德林, 宋耀良, 朱艳萍. 一种新的基于谐振型高阻抗表面的微波吸波屏[J]. 南京理工大学学报(自然科学版), 2010, 34: 136) | | [5] | Costa F, Monorchio A.Electromagnetic absorbers based on high-impedance surfaces: From ultra-narrowband to ultra-wideband absorption[J]. Adv. Electromagnet., 2012, 1(3): 7 | | [6] | Teng Z P.The study of electromagnetic band-gap structure used in antenna design [D]. Nanchang: East China Jiaotong University, 2016(腾兆朋. 电磁带隙结构研究与在天线设计中的应用 [D]. 南昌: 华东交通大学, 2016) | | [7] | Costa F, Genovesi S, Monorchio A.On the bandwidth of high-impedance frequency selective surfaces[J]. IEEE Antennas Wirel. Propag. Lett., 2010, 8: 1341 | | [8] | Sun L K, Cheng H F, Zhou Y J, et al.Broadband metamaterial absorber based on coupling resistive frequency selective surface[J]. Opt. Express, 2012, 20: 4675 | | [9] | Sun L K, Cheng H F, Zhou Y J, et al.Low-frequency and broad band metamaterial absorber: Design, fabrication, and characterization[J]. Appl. Phys., 2011, 105A: 49 | | [10] | Chen J F, Hu Z Y, Wang G D, et al.High-impedance surface-based broadband absorbers with interference theory[J]. IEEE Trans. Antennas Propag., 2015, 63: 4367 | | [11] | Gu C, Qu S B, Pei Z B, et al.Design of a wide-band metamaterial absorber based on resistance films[J]. Acta Phys. Sin., 2011, 60(8): 087802(顾超, 屈绍波, 裴志斌等. 基于电阻膜的宽频带超材料吸波体的设计[J]. 物理学报, 2011, 60(8): 087802) | | [12] | Yan Z W, Su D L, Yuan X M.FEKO 5.4 Electromagnetic Field Analysis Techniques and Examples [M]. Beijing: China Water Power Press, 2009: 1(阎照文, 苏东林, 袁晓梅. FEKO 5.4电磁场分析技术与实例详解 [M]. 北京: 中国水利水电出版社, 2009: 1) | | [13] | Xing L Y.Study on the microwave-absorbing composite with circuit analogue [D]. Beijing: Beihang University, 2003(邢丽英. 含电路模拟结构吸波复合材料研究 [D]. 北京: 北京航空航天大学, 2003) | | [14] | Zhou Y J, Chen Z H, Cheng H F, et al.Calculating microwave effective permittivity of particle-filling composite materials by FDTD method[J]. J. Mater. Sci. Eng., 2006, 24: 830(周永江, 陈朝辉, 程海峰等. 用FDTD方法研究颗粒型复合材料微波等效介电常数[J]. 材料科学与工程学报, 2006, 24: 830) | | [15] | Wang D, Deng J L, Jiao Y J.The evaluation for the theory calculation methods of composite medium absorbing material equivalent electromagnetic parameters[J]. Mater. Prot., 2014, 47(suppl.1): 46(王丹, 邓京兰, 焦亚军. 复合介质吸波材料等效电磁参数理论计算方法的评价[J]. 材料保护, 2014, 47(增刊1): 46) | | [16] | Wang T G, Gong J, Du H, et al.Study on electromagnetic wave transmission performances of ultra-thin metallic films[J]. Acta Metall. Sin., 2005, 41: 814(王铁钢, 宫骏, 杜昊等. 超薄金属膜电磁波传输性能的研究[J]. 金属学报, 2005, 41: 814) | | [17] | Liu J G, Wang T G, Du H, et al.Permittivity of nano aluminum films in microwave band[J]. Met. Funct. Mater., 2006, 13(1): 24(刘健钢, 王铁钢, 杜昊等. 纳米Al膜的微波介电特性研究[J]. 金属功能材料, 2006, 13(1): 24) | | [18] | Liu Z M, Du H, Shi N L, et al.Influence of conductivity size effect on the microwave absorption properties of aluminium films[J]. Acta Metall. Sin., 2008, 44: 1099(刘志敏, 杜昊, 石南林等. 铝膜电导率尺寸效应对其微波性能的影响[J]. 金属学报, 2008, 44: 1099) | | [19] | Du H, Xiao J Q, Tan M H, et al.Initial analysis of effective medium theory to dielectric function change of nanometal film[J]. Acta Metall. Sin., 2000, 36: 1165(杜昊, 肖金泉, 谭明晖等. 利用有效媒质理论对纳米金属薄膜介电函数的初步分析[J]. 金属学报, 2000, 36: 1165) | | [20] | Du H, Bai X D, Xiao J Q, et al.Size effect of the absorptance of the ultra-thin titanium films[J]. Chin. J. Mater. Res., 2001, 15: 215(杜昊, 白雪冬, 肖金泉等. 超薄Ti膜吸收率的尺寸效应[J]. 材料研究学报, 2001, 15: 215) | | [21] | Bai X D, Huang R F, Wen L S.The size effect of the visible absorptance of the ultrathin aluminum film[J]. Acta Metall. Sin., 1998, 34: 1005(白雪冬, 黄荣芳, 闻立时. 超薄Al膜可见光吸收率的尺寸效应[J]. 金属学报, 1998, 34: 1005) | | [22] | Bai X D, Huang R F, Wen L S.The size effect of the visible optical characteristics for ultrathin Al films[J]. Vac. Sci. Technol.(China), 1999, 19(2): 108(白雪冬, 黄荣芳, 闻立时. 超薄Al膜可见光光学特性与其特征尺寸的关系[J]. 真空科学与技术, 1999, 19(2): 108) | | [23] | Tang W, Deng L J, Xu K W, et al., Relationship between resistivity of metallic film and its surface roughness, residual stress[J]. Rare Met. Mater. Eng., 2008, 37: 617(唐武, 邓龙江, 徐可为等. 金属薄膜电阻率与表面粗糙度、残余应力的关系[J]. 稀有金属材料与工程, 2008, 37: 617) | | [24] | Zhang H B.Design of broadband periodic absorbing structure based on electromagnetic resonances [D]. Chengdu: University of Electronic Science and Technology of China, 2013(张辉彬. 基于电磁谐振的宽频周期吸波结构设计 [D]. 成都: 电子科技大学, 2013) | | [25] | Xu Y Q, Zhang H B, Zhou P H, et al.Design of a low-frequency broadband circuit analog absorbers based on wire media[J]. Acta Phys. Sin., 2013, 62: 058103(徐阳秋, 张辉彬, 周佩珩等. 基于金属线阵列嵌入的低频宽带电路模拟吸波体设计[J]. 物理学报, 2013, 62: 058103) | | [26] | Zhang H B, Zhou P H, Lu H P, et al.Resistance selection of high impedance surface absorbers for perfect and broadband absorption[J]. IEEE Trans. Antennas Propag., 2013, 61: 976 |
|
|