Please wait a minute...
金属学报  2017, Vol. 53 Issue (11): 1504-1510    DOI: 10.11900/0412.1961.2017.00093
  研究论文 本期目录 | 过刊浏览 |
镍基合金表面Pt改性铝化物涂层的初期Al2O3微观结构分析
宋鹏(), 陈榕, 冯晶, 吕建国, 陆建生
昆明理工大学材料科学与工程学院 昆明 650093
Microstructure Analysis of Initial Alumina of Pt-Modified Aluminide Coatings on Ni-Based Alloy
Peng SONG(), Rong CHEN, Jing FENG, Jianguo Lü, Jiansheng LU
Faculty of Materials Science and Engineering, Kunming University of Science and Technology, Kunming 650093, China
引用本文:

宋鹏, 陈榕, 冯晶, 吕建国, 陆建生. 镍基合金表面Pt改性铝化物涂层的初期Al2O3微观结构分析[J]. 金属学报, 2017, 53(11): 1504-1510.
Peng SONG, Rong CHEN, Jing FENG, Jianguo Lü, Jiansheng LU. Microstructure Analysis of Initial Alumina of Pt-Modified Aluminide Coatings on Ni-Based Alloy[J]. Acta Metall Sin, 2017, 53(11): 1504-1510.

全文: PDF(4344 KB)   HTML
摘要: 

对CMSX-4合金表面Pt改性铝化物(NiPtAl)高温涂层进行了短期高温氧化实验,研究了NiPtAl在1150 ℃形成表面氧化膜的微观结构。结果表明,氧化1 h后形成的氧化膜包含亚稳态和稳态Al2O3区域,同时部分区域发生氧化膜脱落,并在氧化膜内部观察到空洞和Pt颗粒。分析表明,在涂层初期氧化过程中,NiPtAl涂层表面亚稳态θ-Al2O3向稳态α-Al2O3转变,导致氧化膜中α-Al2O3与θ-Al2O3呈区域层状分布,氧化1 h后NiPtAl涂层表面会形成约0.5 μm厚的θ-Al2O3层。随着θ-Al2O3的快速生长,NiPtAl中β-NiAl向γ'-Ni3Al转变,由于Pt在γ'相比β相中溶解度小而发生偏析,从而导致在氧化膜α-Al2O3与θ-Al2O3层界面处含有Pt颗粒。另外,初期Al2O3层的快速生长导致氧化膜内部形成空洞,氧化膜的生长和相变导致的内应力和内部空洞等缺陷降低了表面θ-Al2O3层的黏结性能,最终导致氧化层脱落。

关键词 : NiPtAl,  高温涂层,  初期氧化,  Al2O3,  生长特征    
Abstract:

NiPtAl coatings are widely used as overlaying coatings besides bondcoats for thermal barrier coating (TBC) systems within high temperature environment. Oxidaiton behavior of NiPtAl coatings is mainly contribution for the failure of TBC systems or overlaying coatings. An initial oxide layer growth characteristics play a key role in extending lifetime of TBC system or overlaying coatings. In this work, the oxidation experiments of the Pt modified aluminide coating on CMSX-4 Ni-based alloy were carried out at 1150 ℃ for 1 h in 80%Ar+20%O2. The microstructures of oxide on the NiPtAl coatings are studied by OM, SEM, TEM and Raman spectroscopy. The results indicated that the oxide layer on the NiPtAl coatings included stable and met-stable Al2O3 after 1 h oxidation, and part of spalled oxide layer as well as pores within the oxide layer. The 0.5 μm thickness whisker-like θ-Al2O3 could form on NiPtAl coating during the initially oxidation stage. At the initial oxidation stage θ-Al2O3 fastly grew which resulted β-NiAl to γ'-Ni3Al transformation. The Pt particles formed on the inter-surface between α-Al2O3 and θ-Al2O3 layer due to a less Pt solid solubility in γ'-Ni3Al compared to β-NiAl in the coating. Fast growth of initial Al2O3 could induce pores formation within the alumina layer. The pores and stress due to oxidation and phase transformation could decrease the alumina adherence, and at last result in the oxide spallation.

Key words: NiPtAl    high temperature coating    initially oxidation    Al2O3    growth characteristics
收稿日期: 2017-03-21     
ZTFLH:  TG172.82  
基金资助:国家自然科学基金项目No.51401097
作者简介:

作者简介 宋 鹏,男,1979年生,副教授,博士

图1  原始NiPtAl涂层截面的SEM像及表面XRD分析
图2  1150 ℃等温氧化1 h后NiPtAl涂层表面Al2O3的OM像和SEM像及图2a中区域I、II和III的Raman光谱
图3  1150 ℃等温氧化1 h后NiPtAl表面形成Al2O3的截面TEM像
图4  图3b中圆圈所示内层和外层氧化膜的SAED花样
图5  图3b中方框区域氧化膜的TEM像和图3c中方框区域氧化膜的HRTEM像
图6  1150 ℃等温氧化1 h后NiPtAl表面形成的Al2O3的截面SEM像
[1] Goward G W. Progress in coatings for gas turbine airfoils [J]. Surf. Coat. Technol., 1998, 108-109: 73
[2] Padture N P, Gell M, Jordan E H.Thermal barrier coatings for gas-turbine engine applications[J]. Science, 2002, 296: 280
[3] Vassen R, Stuke A, St?ver D.Recent developments in the field of thermal barrier coatings[J]. J. Thermal Spray Technol., 2009, 18: 181
[4] Schulz U, Leyens C, Fritscher K, et al.Some recent trends in research and technology of advanced thermal barrier coatings[J]. Aerosp. Sci. Technol., 2003, 7: 73
[5] Gleeson B, Mu N, Hayashi S.Compositional factors affecting the establishment and maintenance of Al2O3 scales on Ni-Al-Pt systems[J]. J. Mater. Sci., 2009, 44: 1704
[6] Tawancy H M, UI-Hamid A, Abbas N M, et al.Effect of platinum on the oxide-to-metal adhesion in thermal barrier coating systems[J]. J. Mater. Sci., 2008, 43: 2978
[7] Vialas N, Monceau D.Effect of Pt and Al content on the long-term, high temperature oxidation behavior and interdiffusion of a Pt-modified aluminide coating deposited on Ni-base superalloys[J]. Surf. Coat. Technol., 2006, 201: 3846
[8] Haynes J A, Pint B A, More K L, et al.Influence of sulfur, platinum, and hafnium on the oxidation behavior of CVD NiAl bond coatings[J]. Oxid. Met., 2002, 58: 513
[9] Hou P Y, Tolpygo V K.Examination of the platinum effect on the oxidation behavior of nickel-aluminide coatings[J]. Surf. Coat. Technol., 2007, 202: 623
[10] Svensson H, Christensen M, Knutsson P, et al.Influence of Pt on the metal-oxide interface during high temperature oxidation of NiAl bulk materials[J]. Corros. Sci., 2009, 51: 539
[11] Qin F, Anderegg J W, Jenks C J, et al.The effect of Pt on Ni3Al surface oxidation at low-pressures[J]. Surf. Sci., 2007, 601: 146
[12] Chieux M C, Molins R, Rémy L, et al. Effect of material and environmental parameters on the microstructure evolution and oxidation behavior of a Ni-based superalloy coated with a Pt-modified Ni-aluminide [J]. Mater. Sci. Forum, 2008, 595-598: 33
[13] Tawancy H M, Abbas N M, Rhys-Jones T N. Role of platinum in aluminide coatings[J]. Surf. Coat. Technol., 1991, 49: 1
[14] Tolpygo V K, Clarke D R.Microstructural study of the theta-alpha transformation in alumina scales formed on nickel-aluminides[J]. Mater. High Temp., 2000, 17: 59
[15] Song P, Lu J S, Lü J G, et al.Influence factors of high temperature oxidation for Pt-modified-aluminide bond coatings[J]. Rare Met. Mater. Eng., 2010, 39: 304(宋鹏, 陆建生, 吕建国等. 铂铝涂层高温氧化的影响因素研究[J]. 稀有金属材料与工程, 2010, 39: 304)
[16] Song P, Lu J S, Zhang D F.High temperature oxidation of surface polished treatment Pt-modified-aluminide bond coats[J]. Chin. J. Nonferrous Met., 2009, 19: 1417(宋鹏, 陆建生, 张德丰. 抛光处理铂铝粘结层的高温氧化[J]. 中国有色金属学报, 2009, 19: 1417)
[17] Xing L L, Zheng Y J, Cui L S, et al.Progress of water vapour effect on growth of alumina forming alloys[J]. J. Chin. Soc. Corros. Prot., 2011, 31: 409(邢琳琳, 郑雁军, 崔立山等. 水蒸汽影响氧化铝膜生长的研究新进展[J]. 中国腐蚀与防护学报, 2011, 31: 409)
[18] Hayashi S, Narita T, Gleeson B. Early-stage oxidation behavior of γ′-Ni3Al-based alloys with and without Pt addition [J]. Mater. Sci. Forum, 2006, 522-523: 229
[19] Hayashi S, Gleeson B.Early-stage oxidation behavior of Pt-modified γ′-Ni3Al-based alloys with and without Hf addition[J]. Oxid. Met., 2009, 71: 5
[20] Pint B A, Haynes J A, Zhang Y, et al.The effect of water vapor on the oxidation behavior of Ni-Pt-Al coatings and alloys[J]. Surf. Coat. Technol., 2006, 201: 3852
[21] Li M S, Zhou Y C.Transient oxidation of Al2O3 forming alloys[J]. Corros. Sci. Prot. Technol., 2005, 17: 409(李美栓, 周延春. Al2O3形成合金过渡态氧化行为[J]. 腐蚀科学与防护技术, 2005, 17: 409)
[22] Grabke H J.Oxidation of NiAl and FeAl[J]. Intermetallics, 1999, 7: 1153
[23] Svensson H, Stiller K, Angenete J. Investigation of oxide formation during short-term oxidation of model NiAl alloys [J]. Mater. Sci. Forum, 2004, 461-464: 231
[24] Svensson H, Knutsson P, Stiller K.Formation and healing of voids at the metal-oxide interface in NiAl alloys[J]. Oxid. Met., 2009, 71: 143
[25] Hou P Y, Izumi T, Gleeson B.Sulfur segregation at Al2O3/γ-Νi + γ'-Ni3Al interfaces: Effects of Pt, Cr and Hf additions[J]. Oxid. Met., 2009, 72: 109
[26] Hayashi S, Ford S I, Young D J, et al.α-NiPt(Al) and phase equilibria in the Ni-Al-Pt system at 1150 ℃[J]. Acta Mater., 2005, 53: 3319
[1] 宋庆忠, 潜坤, 舒磊, 陈波, 马颖澈, 刘奎. 镍基高温合金K417G与氧化物耐火材料的界面反应[J]. 金属学报, 2022, 58(7): 868-882.
[2] 宋芊汀, 徐映坤, 徐坚. (TiZrNbTa)90Mo10高熵合金与Al2O3干摩擦条件下的滑动磨损行为[J]. 金属学报, 2020, 56(11): 1507-1520.
[3] 郭策安, 陈明辉, 廖依敏, 苏北, 谢冬柏, 朱圣龙, 王福会. 模拟燃气热冲击条件下搪瓷基复合涂层的防护机理研究[J]. 金属学报, 2018, 54(12): 1825-1832.
[4] 刘涛,董加胜,谢光,王义胜,李辉,李志军,周兴泰,楼琅洪. GH3535合金在FLiNaK熔盐中的腐蚀行为[J]. 金属学报, 2015, 51(9): 1059-1066.
[5] 吴铭方,刘飞,王凤江,乔岩欣. 陶瓷基复合材料辅助脉冲电流液相扩散连接的界面反应及接头强化机制[J]. 金属学报, 2015, 51(9): 1129-1135.
[6] 崔跃,席文君,王星,李树杰. 纳米Al2O3和NiAl共同强化的铁基ODS合金的铝热合成研究[J]. 金属学报, 2015, 51(7): 791-798.
[7] 刘毅, 江国锋, 许昆, 罗锡明, 陈登权, 李伟. 中间层金属对Al2O3/1Cr18Ni9Ti钎焊接头组织及剪切强度的影响*[J]. 金属学报, 2015, 51(2): 209-215.
[8] 吴铭方, 匡泓锦, 王凤江, 林红香, 胥国祥. Zr/Cu/Zr部分瞬间液相焊扩散连接Ti(C, N)-Al2O3陶瓷基复合材料*[J]. 金属学报, 2014, 50(5): 619-625.
[9] 蔡俊,凌国平,陈长安,张桂凯. 液态Al氧化的环境透射电镜观察[J]. 金属学报, 2013, 49(8): 953-958.
[10] 宋衎 张军 贾晓娇 苏海军 刘林 傅恒志. 激光悬浮区熔定向凝固Al2O3/YAG/ZrO2 三元过共晶合金的微观组织[J]. 金属学报, 2012, 48(2): 220-226.
[11] 张花蕊 高明 唐晓霞 张虎. 定向凝固过程中Ti-47Al-2Cr--Nb合金与Y2O3陶瓷的相互作用[J]. 金属学报, 2010, 46(7): 890-896.
[12] 申坤 汪明朴 郭明星 李树梅. Cu--0.23%Al2O3弥散强化铜合金的高温变形特性研究[J]. 金属学报, 2009, 45(5): 597-604.
[13] 赵丽利; 林均品; 王艳丽; 叶丰; 陈国良 . Ti50Al和Ti45Al8Nb合金高温初期氧化行为[J]. 金属学报, 2008, 44(5): 557-564 .
[14] 何叶青; 熊科北 . Nd-Fe-B铸锭的晶体生长特征[J]. 金属学报, 1999, 35(3): 271-274 .
[15] 马信清;李美栓;彭晓;陈全芳;李铁藩. 弥散CeO_2对高温下α-Al_2O_3氧化膜初期生长的影响[J]. 金属学报, 1995, 31(21): 399-405.