| 22MnB5热成形钢奥氏体化时热镀Al-10%Si镀层组织的演化 |
袁训华( ), 张启富 |
| 新冶高科技集团有限公司先进金属材料涂镀国家工程实验室 北京 100081 |
|
| Microstructure Evolution of Hot-Dip Al-10%Si Coating During the Austenitization of 22MnB5 Hot Stamping Steel |
Xunhua YUAN( ), Qifu ZHANG |
| National Engineering Laboratory of Advanced Coating Technology for Metals, New Metallurgy Hi-Tech Group Co., Ltd., Beijing 100081, China |
引用本文:
袁训华, 张启富. 22MnB5热成形钢奥氏体化时热镀Al-10%Si镀层组织的演化[J]. 金属学报, 2017, 53(11): 1495-1503.
Xunhua YUAN,
Qifu ZHANG.
Microstructure Evolution of Hot-Dip Al-10%Si Coating During the Austenitization of 22MnB5 Hot Stamping Steel[J]. Acta Metall Sin, 2017, 53(11): 1495-1503.
| [1] | Kang Y L.Lightweight vehicle, advanced high strength steel and energy-saving and emission reduction[J]. Iron Steel, 2008, 43(6): 1(康永林. 汽车轻量化先进高强钢与节能减排[J]. 钢铁, 2008, 43(6): 1) | | [2] | Jenner F.Investigation of the intermetallic coating formed during processing of aluminum-coated boron heat-treatable steels [A]. Proceedings of the XIth International Congress and Exposition[C]. Orlando: Society for Experimental Mechanics, 2008: 37 | | [3] | Barcellona A, Palmeri D.Effect of plastic hot deformation on the hardness and continuous cooling transformations of 22MnB5 microalloyed boron steel[J]. Metall. Mater. Trans, 2009, 40A: 1160 | | [4] | Abdulhay B, Bourouga B, Dessain C, et al.Experimental study of heat transfer in hot stamping process[J]. Int. J. Mater. Form., 2009, 2: 255 | | [5] | Ma N, Shen G Z, Zhang Z H, et al.Material performance of hot-forming high strength steel and its application in vehicle body[J]. Chin. J. Mech. Eng., 2011, 47(8): 60(马宁, 申国哲, 张宗华等. 高强度钢板热冲压材料性能研究及在车身设计中的应用[J]. 机械工程学报, 2011, 47(8): 60) | | [6] | Nakagawa K, Nakagaito T, Yokata T, et al.Effect of depth of crack on fatigue property in Zn-Ni coated press hardened steel [A]. 5th International Conference on Proceedings on Hot Sheet Metal Forming of High-Performance Steel[C]. Toronto: Association for Iron & Steel Technology, 2015: 77 | | [7] | Kolleck R, Veit R, Merklein M, et al.Investigation on induction heating for hot stamping of boron alloyed steels[J]. CIRP Ann. Manuf. Technol., 2009, 58(1): 275 | | [8] | Naganathan A.Hot stamping of manganese boron steel [D]. Columbus: Ohio State University, 2010: 31 | | [9] | Han Q H, Bi W Z, Jin X Y, et al.Low temperature hot forming of medium-Mn steel [A]. 5th International Conference on Hot Sheet Metal Forming of High-Performance Steel[C]. Toronto: Association for Iron & Steel Technology, 2015: 381 | | [10] | Xu W L, Guan S R, Ai J, et al.Introduction of sheet metal hot-forming[J]. J. Plast. Eng., 2009, 16(4): 39(徐伟力, 管曙荣, 艾键等. 钢板热冲压新技术介绍[J]. 塑性工程学报, 2009, 16(4): 39) | | [11] | Liu H S, Liu W, Bao J, et al.Numerical and experimental investigation into hot forming of ultra high strength steel sheet[J]. J. Mater. Eng. Perform., 2011, 20: 1 | | [12] | Naderi M, Ketabchi M, Abbasi M, et al.Semi-hot stamping as an improved process of hot stamping[J]. J. Mater. Sci. Technol., 2011, 27: 369 | | [13] | Naderi M, Ketabchi M, Abbasi M, et al.Analysis of microstructure and mechanical properties of different high strength carbon steels after hot stamping[J]. J. Mater. Process. Technol., 2011, 211: 1117 | | [14] | Liu H P, Jin X J, Dong H, et al.Martensitic microstructural transformations from the hot stamping, quenching and partitioning process[J]. Mater. Charact., 2011, 62: 223 | | [15] | Sengoku A, Takebayashi H, Matsumura K.Microstructural and phase evolution of galvannealed coating during hot stamping heating [A]. 5th International Conference on Proceedings on Hot Sheet Metal Forming of High-Performance Steel[C]. Toronto: Association for Iron & Steel Technology, 2015: 363 | | [16] | Suehiro M, Kusumi K, Miyakoshi T, et al.Properties of aluminum-coated steels for hot-forming[J]. Nippon Steel Tech. Rep., 2003, 88: 16 | | [17] | Maki J, Kurosaki M, Kusumi K, et al.Effect of heating condition and hot forming on corrosion resistance of hot stamped aluminized steels [A]. 3th International Conference on Proceedings on Hot Sheet Metal Forming of High-Performance Steel[C]. Kassel: Association for Iron & Steel Technology, 2011: 449 | | [18] | Dosdat L, Petitjean J, Vietoris T, et al.Corrosion resistance of different metallic coatings on press-hardened steels for automotive[J]. Steel Res. Int., 2011, 82: 726 | | [19] | Fan D W, De Cooman B C. State-of-the-knowledge on coating systems for hot stamped parts[J]. Steel Res. Int., 2012, 83: 412 | | [20] | Grigorieva R, Drillet P, Mataigne J M, et al. Phase transformations in the Al-Si coating during the austenitization step [J]. Solid State Phenom., 2011, 172-174: 784 | | [21] | Luther F, Koll T, Braun M.Laboratory study on the performance of zinc and aluminum based coatings for a direct hot press forming process [A]. 8th International Conference on Zinc and Zinc Alloy Coated Steel Sheet[C]. Genova: Associazione Italiana Di Metallurgia, 2011: 379 | | [22] | Fan D W, Kim H S, Oh J K, et al.Coating degradation in hot press forming[J]. ISIJ Int., 2010, 50: 561 | | [23] | Chang Y Y, Tsaur C C, Rock J C.Microstructure studies of an aluminide coating on 9Cr-1Mo steel during high temperature oxidation[J]. Surf. Coat. Technol., 2006, 200: 6588 | | [24] | Borsetto F, Ghiotti A, Bruschi S. Investigation of the high strength steel Al-Si coating during hot stamping operations [J]. Key Eng. Mater., 2009, 410-411: 289 | | [25] | Young D J.High temperature oxidation and corrosion of metals[M]. Oxford, UK: Elsevier, 2008: 16 | | [26] | Liu B J.Hot Dip Aluminizing Steel [M]. Beijing: Metallurgical Industry Press, 1995: 12(刘邦津. 钢材的热浸镀铝 [M]. 北京: 冶金工业出版社, 1995: 12) | | [27] | Paul A, Van Dal M J H, Kodentsov A A, et al. The kirkendall effect in multiphase diffusion[J]. Acta Mater., 2004, 52: 623 | | [28] | Maitra T, Gupta S P.Intermetallic compound formation in Fe-Al-Si ternary system: Part II[J]. Mater. Charact., 2002, 49: 293 | | [29] | Grigorieva R, Drillet P, Mataigne J M, et al.Study of phase transformations in Al-Si coating during the austenitization step [A]. 8th International Conference on Zinc and Zinc Alloy Coated Steel Sheet[C]. Genova: Associazione Italiana Di Metallurgia, 2011: 331 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|