| 近共晶成分Ni-P非晶合金微结构特征的原子模拟分析 |
彭超, 李媛, 邓永和, 彭平( ) |
| 湖南大学材料科学与工程学院 长沙 410082 |
|
| Atomistic Simulation for Local Atomic Structures of Amorphous Ni-P Alloys with Near-Eutectic Compositions |
Chao PENG, Yuan LI, Yonghe DENG, Ping PENG( ) |
| School of Materials Science & Engineering, Hunan Universuty, Changsha 410082, China |
引用本文:
彭超, 李媛, 邓永和, 彭平. 近共晶成分Ni-P非晶合金微结构特征的原子模拟分析[J]. 金属学报, 2017, 53(12): 1659-1668.
Chao PENG,
Yuan LI,
Yonghe DENG,
Ping PENG.
Atomistic Simulation for Local Atomic Structures of Amorphous Ni-P Alloys with Near-Eutectic Compositions[J]. Acta Metall Sin, 2017, 53(12): 1659-1668.
| [1] | Brenner A, Riddell G.Deposition of nickel and cobalt by chemical reduction[J]. J. Res. Nat. Bur. Stand., 1947, 39: 385 | | [2] | Sui M L, Lu K.Microstructures of crystallites in nanocrystalline Ni-P alloys[J]. Acta Metall. Sin., 1994, 30: 413(隋曼龄, 卢柯. 纳米晶体Ni-P合金晶粒微观结构的研究[J]. 金属学报, 1994, 30: 413) | | [3] | Sui M L.An investigation on the recovery behaviors of the lattice distortions in an Ni3P/Ni nanophase material[J] Acta Metall. Sin., 1998, 34: 650(隋曼龄. Ni3P/Ni复相纳米材料晶格畸变的热回复行为研究[J]. 金属学报, 1998, 34: 650) | | [4] | Budurov S, Fotty V, Toncheva S, et al.The glass-forming ability in the ternary Ni-Co-P and Ni-Cu-P systems[J]. Mater. Sci. Eng., 1991, A133: 455 | | [5] | Paseka I.Hydrogen evolution reaction on Ni-P alloys: The internal stress and the activities of electrodes[J]. Electrochim. Acta, 2008, 53: 4537 | | [6] | Hameed R M A, Fekry A M. Electrochemical impedance studies of modified Ni-P and Ni-Cu-P deposits in alkaline medium[J]. Electrochim. Acta, 2010, 55: 5922 | | [7] | Nash P.Phase Diagrams of Binary Nickel Alloys[M]. Ohio: ASM International, 1991: 2833 | | [8] | Schmetterer C, Vizdal J, Ipser H.A new investigation of the system Ni-P[J]. Intermetallics, 2009, 17: 826 | | [9] | Huang Q S, Liu L, Li J F, et al.Redetermination of the eutectic composition of the Ni-P binary alloy[J]. J. Phase Equilib. Diff., 2010, 31: 532 | | [10] | Huang Q S, Lu B F, Kong L T, et al.On the glass-forming ability of Ni-P binary alloys[J]. Mater. Res. Bull., 2012, 47: 1973 | | [11] | Kraus L, Ha?lar V, Duhaj P, et al. The structure and magnetic properties of nanocrystalline Co21Fe64-xNbxB15 alloys [J]. Mater. Sci. Eng., 1997, A226-228: 626 | | [12] | Cheng Y Q, Ma E.Atomic-level structure-property relationship in metallic glasses[J]. Prog. Mater. Sci., 2011, 56: 379 | | [13] | Ding J, Cheng Y Q, Sheng H W, et al.Short-range structural signature of excess specific heat and fragility of metallic glass-forming supercooled liquids[J]. Phys. Rev., 2012, 85B: 060201 | | [14] | Laws K J, Miracle D B, Ferry M.A predictive structural model for bulk metallic glasses[J]. Nat. Commun., 2015, 6: 8123 | | [15] | Bennett M R, Wright J G.Amorphous films of the transition elements[J]. Phys. Stat. Sol., 1972, 13: 135 | | [16] | Lu K, Wang J T.A micromechanism for crystallization of amorphous alloys I. An in situ TEM observation[J]. J. Cryst. Growth, 1991, 112: 525 | | [17] | Lu K, Sui M L, Wang J T.A micromechanism for crystallization of amorphous alloys II. Bulk crystallization process[J]. J. Cryst. Growth, 1991, 113: 242 | | [18] | Luo W K, Ma E.EXAFS measurements and reverse Monte Carlo modeling of atomic structure in amorphous Ni80P20 alloys[J]. J. Non-Cryst. Solids, 2008, 354: 945 | | [19] | Plimpton S.Fast parallel algorithms for short-range molecular dynamics[J]. J. Comput. Phys., 1995, 117: 1 | | [20] | Mendelev M I, Sordelet D J, Kramer M J.Using atomistic computer simulations to analyze X-ray diffraction data from metallic glasses[J]. J. Appl. Phys., 2007, 102: 043501 | | [21] | Martyna G J, Tobias D J, Klein M L.Constant pressure molecular dynamics algorithms[J]. J. Chem. Phys., 1994, 101: 4177 | | [22] | Verlet L.Computer experiments on classical fluids: I. Thermodynamical properties of lennard-jones molecules[J]. Phys. Rev., 1967, 159: 98 | | [23] | Finney J L.Random packings and the structure of simple liquids. II. The molecular geometry of simple liquids[J]. Proc. R. Soc. Lond., 1970, 319A: 495 | | [24] | Wei Y D, Peng P, Yan Z Z, et al.A comparative study on local atomic configurations characterized by cluster-type-index method and Voronoi polyhedron method[J]. Comput. Mater. Sci., 2016, 123: 214 | | [25] | Mo Y F, Liu R S, Liang Y C, et al.Molecular dynamics simulation on the evolution of microstructures of liquid ZnxAl100-x alloys during rapid solidification[J]. Acta Metall. Sin., 2012, 48: 907(莫云飞, 刘让苏, 梁永超等. ZnxAl100-x合金快凝过程中微结构演变特性的分子动力学模拟[J]. 金属学报, 2012, 48: 907) | | [26] | Wigner E, Seitz F.On the constitution of metallic sodium[J]. Phys. Rev., 1933, 43: 804 | | [27] | Lamparter P.Reverse monte carlo simulation of amorphous Ni80P20 and Ni81B19 [J]. Phys. Scr., 1995, 57: 72 | | [28] | Swope W C, Andersen H C.106-particle molecular-dynamics study of homogeneous nucleation of crystals in a supercooled atomic liquid[J]. Phys. Rev., 1990, 41B: 7042 | | [29] | Brostow W, Chybicki M, Laskowski R, et al.Voronoi polyhedra and Delaunay simplexes in the structural analysis of molecular-dynamics-simulated materials[J]. Phys. Rev., 1998, 57B: 13448 | | [30] | Yu D Q, Chen M, Han X J.Structure analysis methods for crystalline solids and supercooled liquids[J]. Phys. Rev., 2005, 72E: 051202 | | [31] | Gao W, Feng S D, Qi L, et al.Local five-fold symmetry and diffusion behavior of Zr64Cu36 amorphous alloy based on molecular dynamics[J]. Chin. Phys. Lett., 2015, 32: 116101 | | [32] | Honeycutt J D, Andersen H C.Molecular dynamics study of melting and freezing of small Lennard-Jones clusters[J]. J. Phys. Chem., 1987, 91: 4950 | | [33] | Deng Y H, Wen D D, Peng C, et al.Heredity of icosahedrons: A kinetic parameter related to glass-forming abilities of rapidly solidified Cu56Zr44 alloys[J]. Acta Phys. Sin., 2016, 65: 066401(邓永和, 文大东, 彭超等. 二十面体团簇的遗传: 一个与快凝Cu56Zr44合金玻璃形成能力有关的动力学参数[J]. 物理学报, 2016, 65: 066401) | | [34] | Wen D D, Peng P, Jiang Y Q, et al.The effect of cooling rates on hereditary characteristics of icosahedral clusters in rapid solidification of liquid Cu56Zr44 alloys[J]. J. Non-Cryst. Solids, 2014, 388: 75 | | [35] | Hou Z Y, Liu L X, Liu R S, et al.Short-range and medium-range order in Ca7Mg3 metallic glass[J]. J. Appl. Phys., 2010, 107: 083511 | | [36] | Wen D D, Peng P, Jiang Y Q, et al.A track study on icosahedral clusters inherited from liquid in the process of rapid solidification of Cu64Zr36 alloy[J]. Acta Phys. Sin., 2013, 62: 196101(文大东, 彭平, 蒋元祺等. 快凝过程中液态Cu64Zr36合金二十面体团簇遗传与演化跟踪[J]. 物理学报, 2013, 62: 196101) | | [37] | Sheng H W, Luo W K, Alamgir F M, et al.Atomic packing and short-to-medium-range order in metallic glasses[J]. Nature, 2006, 439: 419 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|