| β-(Nb, Zr)第二相合金在360 ℃去离子水中的腐蚀行为 |
陈兵1,2,高长源1,2,黄娇1,2,毛亚婧1,2,姚美意1,2( ),张金龙1,2,周邦新1,2,李强1,2 |
1 上海大学材料研究所 上海 200072 2 上海大学微结构重点实验室 上海200444 |
|
| Corrosion Behavior of Second Phase Alloys of β-(Nb, Zr) in Deionized Water at 360 ℃ |
Bing CHEN1,2,Changyuan GAO1,2,Jiao HUANG1,2,Yajing MAO1,2,Meiyi YAO1,2( ),Jinlong ZHANG1,2,Bangxin ZHOU1,2,Qiang LI1,2 |
1 Institute of Materials, Shanghai University, Shanghai 200072, China 2 Laboratory for Microstructures, Shanghai University, Shanghai 200444, China |
引用本文:
陈兵,高长源,黄娇,毛亚婧,姚美意,张金龙,周邦新,李强. β-(Nb, Zr)第二相合金在360 ℃去离子水中的腐蚀行为[J]. 金属学报, 2017, 53(4): 447-454.
Bing CHEN,
Changyuan GAO,
Jiao HUANG,
Yajing MAO,
Meiyi YAO,
Jinlong ZHANG,
Bangxin ZHOU,
Qiang LI.
Corrosion Behavior of Second Phase Alloys of β-(Nb, Zr) in Deionized Water at 360 ℃[J]. Acta Metall Sin, 2017, 53(4): 447-454.
| [1] | Zhou W J, Zhou B X, Miao Z, et al.Development of Chinese advanced zirconium alloys[J]. At. Energy Sci. Technol., 2005, 39(Suppl.): 2 | | [1] | (赵文金, 周邦新, 苗志等. 我国高性能锆合金的发展[J]. 原子能科学技术, 2005, 39(增刊): 2) | | [2] | Bojinov M, Karastoyanov V, Kinnunen P, et al.Influence of water chemistry on the corrosion mechanism of a zirconium-niobium alloy in simulated light water reactor coolant conditions[J]. Corros. Sci., 2010, 52: 54 | | [3] | Nikulina A V, Markelov V A, Peregud M M.Zirconium alloy E635 as a material for fuel rod cladding and other components of VVER and RBMK cores [A]. Zirconium in the Nuclear Industry: Eleventh International Symposium, ASTM STP 1295[C]. West Conshohocken, Philadelphia: American Society for Testing and Materials, 1996: 785 | | [4] | Müller S, Lanzani L.Corrosion of zirconium alloys in concentrated lithium hydroxide solutions[J]. J. Nucl. Mater., 2013, 439: 251 | | [5] | Anada H, Takeda K.Microstructure of oxides on zircaloy-4, 1.0 Nb zircaloy-4, and zircaloy-2 formed in 10.3-MPa steam at 673 K [A]. Zirconium in the Nuclear Industry: Eleventh International Symposium, ASTM STP 1295[C]. West Conshohocken, Philadelphia: American Society for Testing and Materials, 1996: 35 | | [6] | Perkins R A, Busch R A.Corrosion of zircaloy in the presence of LiOH [A]. Zirconium in the Nuclear Industry: Ninth International Symposium, ASTM STP 1132[C]. Philadelphia: American Society for Testing and Materials, 1991: 595 | | [7] | Shebaldov P V, Peregud M M, Nikulina A V, et al.E110 alloy cladding tube properties and their interrelation with alloy structure-phase condition and impurity content [A]. Zirconium in the Nuclear Industry: Twelfth International Symposium, ASTM STP 1354[C]. Philadelphia: American Society for Testing and Materials, 2000: 545 | | [8] | Sun F T, Yao M Y, Xu L, et al.Effect of adding dilute Si on corrosion resistance of zirconium alloys[J]. J. Shanghai Univ.(Nat. Sci.), 2015, 21: 182 | | [8] | (孙风涛, 姚美意, 徐龙等. 添加微量Si对锆合金耐腐蚀性能的影响[J]. 上海大学学报(自然科学版), 2015, 21: 182) | | [9] | Kim H G, Choi B K, Park J Y, et al.Analysis of oxidation behavior of the β-Nb phase formed in Zr-1.5Nb alloy by using the HVEM[J]. J. Alloys Compd., 2009, 481: 867 | | [10] | Yang W D.Reactor Materials Science [M]. Beijing: Atomic Energy Press, 2000: 19 | | [10] | (杨文斗. 反应堆材料学 [M]. 北京: 原子能出版社, 2000: 19) | | [11] | Sabol G P, Comstock R J, Nayak U P.Effect of dilute alloy additions of molybdenum, niobium, and vanadium on zirconium corrosion [A]. Zirconium in the Nuclear Industry: Twelfth International Symposium, ASTM STP 1354[C]. Philadelphia: American Society for Testing and Materials, 2000: 525 | | [12] | Li Q, Liang X, Peng J C, et al.Oxidation behavior of the β-Nb phase precipitated in Zr-2.5Nb alloy[J]. Acta Metall. Sin., 2011, 47: 893 | | [12] | (李强, 梁雪, 彭剑超等. Zr-2.5Nb合金中β-Nb相的氧化过程[J]. 金属学报, 2011, 47: 893) | | [13] | Gong W J, Zhang H L, Wu C F, et al.The role of alloying elements in the initiation of nanoscale porosity in oxide films formed on zirconium alloys[J]. Corros. Sci., 2013, 77: 391 | | [14] | Proff C, Abolhassani S, Lemaignan C.Oxidation behaviour of binary zirconium alloys containing intermetallic precipitates[J]. J. Nucl. Mater., 2011, 416: 125 | | [15] | Proff C, Abolhassani S, Lemaignan C.Oxidation behaviour of zirconium alloys and their precipitates——A mechanistic study[J]. J. Nucl. Mater., 2013, 432: 222 | | [16] | Pêcheur D, Lefebvre F, Motta A T, et al.Precipitate evolution in the zircaloy-4 oxide layer[J]. J. Nucl. Mater., 1992, 189: 318 | | [17] | Pêcheur D.Oxidation of β-Nb and Zr(Fe, V)2 precipitates in oxide films formed on advanced Zr-based alloys[J]. J. Nucl. Mater., 2000, 278: 195 | | [18] | Yilmazbayhan A, Breval E, Motta A T, et al.Transmission electron microscopy examination of oxide layers formed on Zr alloys[J]. J. Nucl. Mater., 2006, 349: 265 | | [19] | Yao M Y, Gao C Y, Huang J, et al.Oxidation behavior of β-Nb precipitates in Zr-1Nb-0.2Bi alloy corroded in lithiated water at 360 ℃[J]. Corros. Sci., 2015, 100: 169 | | [20] | Cao X X.Study on the corrosion behavior of the second phase particles in zirconium alloy [D]. Shanghai: Shanghai University, 2010 | | [20] | (曹潇潇. 锆合金中第二相腐蚀行为研究 [D]. 上海: 上海大学, 2010) | | [21] | Huang J, Yao M Y, Gao C Y, et al.Analysis of the oxidized surface of 90Nb-10Zr alloy after exposure to lithiated water with 0.01 M LiOH at 360 ℃/18.6 MPa[J]. Corros. Sci., 2016, 104: 269 | | [22] | Shen Y F.Effect of β-quenching and annealing treatments on the corrosion resistance of zircaloy-4 [D]. Shanghai: Shanghai University, 2012 | | [22] | (沈月锋. β相水淬及退火处理对Zr-4合金耐腐蚀性能的影响 [D]. 上海: 上海大学, 2012) | | [23] | Liang P Y, Dupin N, Fries S G, et al.Thermodynamic assessment of the Zr-O binary system[J]. Z. Metallk., 2001, 92: 747 | | [24] | Pérez R J, Massih A R.Thermodynamic evaluation of the Nb-O-Zr system[J]. J. Nucl. Mater., 2007, 360: 242 | | [25] | Ondik H M, McMurdie H F. Phase Diagrams for Zirconium and Zirconia Systems[M]. Ohio: The American Ceramic Society, 1998: 145 | | [26] | Cambridge U O.The Interactive Ellingham Diagram, Dissemination of IT for the Promotion of Materials Science, |
|
|