| 片层石墨尺寸对片层石墨/Al复合材料的强度和热导率的影响 |
刘晓云1,2,王文广2,王东2,肖伯律2,倪丁瑞2,陈礼清1,马宗义2( ) |
1 东北大学轧制技术及连轧自动化国家重点实验室 沈阳 110819 2 中国科学院金属研究所沈阳材料科学国家(联合)实验室 沈阳 110016 |
|
| Effect of Graphite Flake Size on the Strength and Thermal Conductivity of Graphite Flakes/Al Composites |
Xiaoyun LIU1,2,Wenguang WANG2,Dong WANG2,Bolv XIAO2,Dingrui NI2,Liqing CHEN1,Zongyi MA2( ) |
1 State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China 2 Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
刘晓云,王文广,王东,肖伯律,倪丁瑞,陈礼清,马宗义. 片层石墨尺寸对片层石墨/Al复合材料的强度和热导率的影响[J]. 金属学报, 2017, 53(7): 869-878.
Xiaoyun LIU,
Wenguang WANG,
Dong WANG,
Bolv XIAO,
Dingrui NI,
Liqing CHEN,
Zongyi MA.
Effect of Graphite Flake Size on the Strength and Thermal Conductivity of Graphite Flakes/Al Composites[J]. Acta Metall Sin, 2017, 53(7): 869-878.
| [1] | Sidhu S S, Kumar S, Batish A.Metal matrix composites for thermal management: A review[J]. Crit. Rev. Solid State Mater. Sci., 2016, 41: 132 | | [2] | Mathias J D, Geffroy P M, Silvain J F.Architectural optimization for microelectronic packaging[J]. Appl. Therm. Eng., 2009, 29: 2391 | | [3] | Rawal S P.Metal-matrix composites for space applications[J]. JOM, 2001, 53(4): 14 | | [4] | Xia Y, Song Y Q, Cui S, et al.Progress in thermal management materials[J]. Mater. Rev., 2008, 22(1): 4 | | [4] | (夏杨, 宋月清, 崔舜等. 热管理材料的研究进展[J]. 材料导报, 2008, 22(1): 4) | | [5] | Xue C, Yu J K.Enhanced thermal transfer and bending strength of SiC/Al composite with controlled interfacial reaction[J]. Mater. Des., 2014, 53: 74 | | [6] | Liu X Y, Wang W G, Wang D, et al.Effect of nanometer TiC coated diamond on the strength and thermal conductivity of diamond/Al composites[J]. Mater. Chem. Phys., 2016, 182: 256 | | [7] | Yoshida K, Morigami H.Thermal properties of diamond/copper composite material[J]. Microelectron. Reliab., 2004, 44: 303 | | [8] | Fu H T, Huang Y, Wu H W, et al.Synthesis by vacuum infiltration, microstructure, and thermo-physical properties of graphite-aluminum composite[J]. ?Adv. Eng. Mater., 2016, 18: 1609 | | [9] | Zhou S X, Chiang S, Xu J Z, et al.Modeling the in-plane thermal conductivity of a graphite/polymer composite sheet with a very high content of natural flake graphite[J]. Carbon, 2012, 50: 5052 | | [10] | Li W J, Liu Y, Wu G H.Preparation of graphite flakes/Al with preferred orientation and high thermal conductivity by squeeze casting[J]. Carbon, 2015, 95: 545 | | [11] | Kurita H, Miyazaki T, Kawasaki A, et al.Interfacial microstructure of graphite flake reinforced aluminum matrix composites fabricated via hot pressing[J]. Composites, 2015, 73A: 125 | | [12] | Prieto R, Molina J M, Narciso J, et al.Thermal conductivity of graphite flakes-SiC particles/metal composites[J]. Composites, 2011, 42A: 1970 | | [13] | Yang Y W, Huang Y, Wu H W, et al.Interfacial characteristic, thermal conductivity, and modeling of graphite flakes/Si/Al composites fabricated by vacuum gas pressure infiltration[J]. J. Mater. Res., 2016, 31: 1723 | | [14] | Prieto R, Molina J M, Narciso J, et al.Fabrication and properties of graphite flakes/metal composites for thermal management applications[J]. Scr. Mater., 2008, 59: 11 | | [15] | Chen J K, Huang I S.Thermal properties of aluminum-graphite composites by powder metallurgy[J]. Composites, 2013, 44B: 698 | | [16] | Wang D, Xiao B L, Wang Q Z, et al.Friction stir welding of SiCp/2009Al composite plate[J]. Mater. Des., 2013, 47: 243 | | [17] | Huang Y, Ouyang Q B, Guo Q, et al.Graphite film/aluminum laminate composites with ultrahigh thermal conductivity for thermal management applications[J]. Mater. Des., 2016, 90: 508 | | [18] | Zhou C, Huang W, Chen Z, et al.In-plane thermal enhancement behaviors of Al matrix composites with oriented graphite flake alignment[J]. Composites, 2015, 70B: 256 | | [19] | Wang D, Xiao B L, Wang Q Z, et al.Evolution of the microstructure and strength in the nugget zone of friction stir welded SiCp/Al-Cu-Mg composite[J]. J. Mater. Sci. Technol., 2014, 30: 54 | | [20] | Xue C, Bai H, Tao P F, et al.Thermal conductivity and mechanical properties of flake graphite/Al composite with a SiC nano-layer on graphite surface[J]. Mater. Des., 2016, 108: 250 | | [21] | Nan C W, Birringer R, Clarke D R, et al.Effective thermal conductivity of particulate composites with interfacial thermal resistance[J]. J. Appl. Phys., 1997, 81: 6692 | | [22] | Wang Z T, Tian R Z.Aluminum Alloy and Its Processing Manual [M]. 3rd Ed., Changsha: Central South University Press, 2005: 314 | | [22] | (王祝堂, 田荣璋. 铝合金机器加工手册 [M]. 长沙: 中南大学出版社, 2005: 314) | | [23] | Molina J M, Louis E.Anisotropy in thermal conductivity of graphite flakes-SiCp/matrix composites: implications in heat sinking design for thermal management applications[J]. Mater. Charact., 2015, 109: 107 | | [24] | Shenogin S, Gengler J, Roy A, et al.Molecular dynamics studies of thermal boundary resistance at carbon-metal interfaces[J]. Scr. Mater., 2013, 69: 100 | | [25] | Chu K, Jia C C, Liang X B, et al.Modeling the thermal conductivity of diamond reinforced aluminium matrix composites with inhomogeneous interfacial conductance[J]. Mater. Des., 2009, 30: 4311 | | [26] | Zhou C, Ji G, Chen Z, et al.Fabrication, interface characterization and modeling of oriented graphite flakes/Si/Al composites for thermal management applications[J]. Mater. Des., 2014, 63: 719 |
|
|