| 高Fe含量Fe-B-Si-Hf块体非晶合金的结构-性能关联 |
耿遥祥1( ),张志杰1,王英敏2,羌建兵2,董闯2,汪海斌1,特古斯3 |
1 江苏科技大学材料科学与工程学院 镇江 212003 2 大连理工大学三束材料改性教育部重点实验室 大连 116024 3 内蒙古师范大学内蒙古自治区功能材料物理与化学重点实验室 呼和浩特 010022 |
|
| Structure-Property Correlation of High Fe-ContentFe-B-Si-Hf Bulk Glassy Alloys |
Yaoxiang GENG1( ),Zhijie ZHANG1,Yingmin WANG2,Jianbing QIANG2,Chuang DONG2,Haibin WANG1,Ojied TEGUS3 |
1 School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China 2 Key Lab of Materials Modification by Laser, Ion and Electron Beams, Ministry of Education, Dalian University of Technology, Dalian 116024, China 3 Inner Mongolia Key Laboratory for Physics and Chemistry of Functional Materials, Inner Mongolia Normal University, Hohhot 010022, China |
引用本文:
耿遥祥,张志杰,王英敏,羌建兵,董闯,汪海斌,特古斯. 高Fe含量Fe-B-Si-Hf块体非晶合金的结构-性能关联[J]. 金属学报, 2017, 53(3): 369-375.
Yaoxiang GENG,
Zhijie ZHANG,
Yingmin WANG,
Jianbing QIANG,
Chuang DONG,
Haibin WANG,
Ojied TEGUS.
Structure-Property Correlation of High Fe-ContentFe-B-Si-Hf Bulk Glassy Alloys[J]. Acta Metall Sin, 2017, 53(3): 369-375.
| [1] | Egami T.Magnetic amorphous alloys: Physics and technological applications[J]. Rep. Prog. Phys., 1984, 47: 1601 | | [2] | McHenry M E, Willard M A, Laughlin D E. Amorphous and nanocrystalline materials for applications as soft magnets[J]. Prog. Mater. Sci., 1999, 44: 291 | | [3] | Hasegawa R.Amorphous magnetic materials——A history[J]. J. Magn. Magn. Mater., 1991, 100: 1 | | [4] | Inoue A, Shinohara Y, Gook J S.Thermal and magnetic properties of bulk Fe-based glassy alloys prepared by copper mold casting[J]. Mater. Trans. JIM, 1995, 36: 1427 | | [5] | Makino A, Kubota T, Chang C T, et al.Fe-metalloids bulk glassy alloys with high Fe content and high glass-forming ability[J]. J. Mater. Res., 2008, 23: 1339 | | [6] | Liu F J, Yao K F, Ding H Y.Fe-based glassy alloys with high iron content and high saturation magnetization[J]. Intermetallics, 2011, 19: 1674 | | [7] | Meng S Y, Ling H B, Li Q, et al.Development of Fe-based bulk metallic glasses with high saturation magnetization[J]. Scr. Mater., 2014, 81: 24 | | [8] | Suryanarayana C, Inoue A.Bulk Metallic Glasses [M]. Boca Raton, FL: CRC Press, 2011: 460 | | [9] | Miracle D B.A structural model for metallic glasses[J]. Nat. Mater., 2004, 3: 697 | | [10] | Han G, Qiang J B, Li F W, et al.The e/a values of ideal metallic glasses in relation to cluster formulae[J]. Acta Mater., 2011, 59: 5917 | | [11] | Luo L J, Chen H, Wang Y M, et al.24 electron cluster formulas as the 'molecular' units of ideal metallic glasses[J]. Philos. Mag., 2014, 94: 2520 | | [12] | Geng Y X, Wang Y M, Qiang J B, et al.Composition formulas of Fe-B binary amorphous alloys[J]. J. Non-Cryst. Solids, 2016, 432: 453 | | [13] | Geng Y X, Wang Y M, Qiang J B, et al.Fe-B-Si-Zr soft magnetic bulk glassy alloys[J]. Intermetallics, 2015, 67: 138 | | [14] | Geng Y X, Wang Y M, Wang Z R, et al.Formation and structure-property correlation of new bulk Fe-B-Si-Hf metallic glasses[J]. | | [14] | Mater. Des., 2016, 106: 69 | | [15] | Geng Y X, Han K M, Wang Y M, Q et al. Composition design of Fe-B-Si-Ta bulk amorphous alloys based on cluster+glue atom model[J]. Acta Metall. Sin., 2015, 51: 1017 | | [15] | (耿遥祥, 韩凯明, 王英敏等. 基于团簇+连接原子模型的Fe-B-Si-Ta块体非晶合金的成分设计[J]. 金属学报, 2015, 51: 1017) | | [16] | Geng Y X, Wang Y M, Qiang J B, et al.Composition design and optimization of Fe-B-Si-Nb bulk amorphous alloys[J]. Acta Metall. Sin., 2016, 52: 1459 | | [16] | (耿遥祥, 王英敏, 羌建兵等. Fe-B-Si-Nb块体非晶合金的成分设计与优化[J]. 金属学报, 2016, 52: 1459) | | [17] | Inoue A, Shen B L.Soft magnetic bulk glassy Fe-B-Si-Nb alloys with high saturation magnetization above 1.5 T[J]. Mater. Trans., 2002, 43: 766 | | [18] | Inoue A, Shen B L.Formation and soft magnetic properties of Fe-B-Si-Zr bulk glassy alloys with high saturation magnetization above 1.5 T[J]. Mater. Trans., 2002, 43: 2350 | | [19] | Miracle D B.The density and packing fraction of binary metallic glasses[J]. Acta Mater., 2013, 61: 3157 | | [20] | Takeuchi A, Inoue A.Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element[J]. Mater. Trans., 2005, 46: 2817 | | [21] | Stillinger F H.Relaxation and flow mechanisms in "fragile" glass-forming liquids[J]. J. Chem. Phys., 1988, 89: 6461 | | [22] | Ediger M D.Spatially heterogeneous dynamics in supercooled liquids[J]. Annu. Rev. Phys. Chem., 2000, 51: 99 | | [23] | Tanaka H.Two-order-parameter model of the liquid-glass transition. II. Structural relaxation and dynamic heterogeneity[J]. J. Non-Cryst. Solids, 2005, 351: 3385 | | [24] | Bakonyi I.Relevance of Fe atomic volumes for the magnetic properties of Fe-rich metallic glasses[J]. J. Magn. Magn. Mater., 2012, 324: 3961 | | [25] | Durand J.Magnetic properties of metallic glasses [A]. Glassy Metals II[M]. Berlin, Heidelberg: Springer-Verlag, 1983: 343 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|