Please wait a minute...
金属学报  2016, Vol. 52 Issue (12): 1497-1502    DOI: 10.11900/0412.1961.2016.00207
  本期目录 | 过刊浏览 |
淬火后预拉伸对自然时效状态Al-Li合金组织和性能的影响*
张显峰,李国爱(),陆政,于娟,郝敏
北京航空材料研究院北京市先进铝合金材料及应用工程技术研究中心, 北京 100095
EFFECT OF PREAGED STRETCH AFTER QUENCHED ON THE PROPERTIES AND MICROSTRUCTURE OF A NATURALLY AGED Al-Li ALLOY
Xianfeng ZHANG,Guoai LI(),Zheng LU,Juan YU,Min HAO
Beijing Engineering Research Center of Advanced Aluminum Alloys and Applications, Beijing Institute of Aeronautical Material, Beijing 100095, China
引用本文:

张显峰,李国爱,陆政,于娟,郝敏. 淬火后预拉伸对自然时效状态Al-Li合金组织和性能的影响*[J]. 金属学报, 2016, 52(12): 1497-1502.
Xianfeng ZHANG, Guoai LI, Zheng LU, Juan YU, Min HAO. EFFECT OF PREAGED STRETCH AFTER QUENCHED ON THE PROPERTIES AND MICROSTRUCTURE OF A NATURALLY AGED Al-Li ALLOY[J]. Acta Metall Sin, 2016, 52(12): 1497-1502.

全文: PDF(3362 KB)   HTML
摘要: 

通过拉伸试验机、腐蚀试验箱、DSC以及TEM等手段对淬火后预拉伸处理并自然时效至稳定状态的铝锂合金薄板的拉伸性能、腐蚀性能、时效响应特征以及微观组织进行了研究. 结果表明, 在0~6%范围内, 合金的屈服强度随预拉伸量的增加而逐渐提高; 预拉伸量低于3%时, 合金的抗拉强度随拉伸量增加逐渐降低, 在3%~6%范围内, 抗拉强度趋于平稳; 随预拉伸量增加, 合金由明显的晶间腐蚀转为点蚀, T34状态点蚀深度最小, 约为0.03 mm; 预拉伸改变了合金的时效响应特征, 使合金在100 ℃附近的吸热峰向高温移动, 180 ℃及260 ℃附近的放热峰向低温区移动. 淬火后的预拉伸在增加晶内位错密度的同时, 抑制了δ’相在晶内和晶界的析出, 预拉伸量越大, 晶内及晶界δ’相的数量越少. 位错及析出相的共同作用影响了合金的拉伸及腐蚀性能.

关键词 : 铝锂合金,  预拉伸处理,  拉伸性能,  晶间腐蚀,,  δ;'析出相    
Abstract:

Al-Cu-Li-X alloy has attractive applications in the aerospace and aeronautic industry due to its excellent combination of mechanical properties and corrosion resisting properties. However, the microstructural complexity, especially the type and distribution of precipitates have effects on the properties. Besides changing the chemical compositions of alloy, the preaged stretch after quenched and aging process is the main method to control the type and distribution of precipitates. In this work, the effect of preaged stretch after quenched on tensile properties, corrosion property, aging response and microstructure of a naturally aged Al-Li alloy were studied by DSC, TEM, tensile test and corrosion test. The results show that the yield strength increases gradually at the stretch range from 0 to 6%, ultimate tensile strength decreases with the increase of stretch from 0 to 3%, and then become stable when stretch over 3%. Accompany with the increasing stretch, the corrosion type of alloy changes from intergranular corrosion to point corrosion. The T34 state of alloy has the least corrosion depth, about 0.03 mm. The aging response character of alloy is changed by preaged stretch. Compared with T4 state, the endothermic peak near 100 ℃ move to higher temperature, and two exothermic peaks near 180 ℃ and 260 ℃ move to lower temperature in T3x state, respectively. Preaged stretch after quenched restrains the precipitation of δ’ phase in grain and grain boundary with increasing the density of dislocation in grains. The variations of δ’ phase and dislocation affect the tensile and corrosion properties of alloy.

Key words: Al-Li alloy    preaged stretch    tensile property    intergranular corrosion    δ;' precipitate
收稿日期: 2016-05-27     
基金资助:* 国家自然科学基金资助项目51474195
图1  不同状态板材的DSC曲线
图2  淬火后预拉伸变形量对自然时效后合金拉伸性能的影响
图3  不同状态合金晶间腐蚀性能
图4  不同状态合金析出相及位错组态
[1] Meric C.Mater Res Bull, 2000; 35: 1479
[2] Rioja R J, Liu J.Metall Mater Trans, 2012; 43A: 3325
[3] Tsivoulas D, Prangnell P B.Metall Mater Trans, 2014; 45A: 1338
[4] Lequeu P, Smith K P, Daniélou A.J Mater Eng Perform, 2010; 19: 841
[5] Acosta E, Garcia O, Dakessian A, Aung Ra K, Torroledo J, Tsang A. Mater Sci Forum#/magtechI#, 2002; 396-402: 1157
[6] Lequeu P, Lassince P, Warner T.Adv Mater Processes, 2007; 165(7): 41
[7] Lequeu P.Adv Mater Processes, 2008; 166(2): 47
[8] Kertz J E, Gouma P I, Buchheit R G.Metall Mater Trans, 2001; 32A: 2561
[9] Li H Y, Tang Y, Zeng Z D, Zheng Z Q, Zheng F.Mater Sci Eng, 2008; A498: 314
[10] Wang S C, Starink M J.Int Mater Rev, 2005; 50: 193
[11] Decreus B, Deschamps A, De Geuser F, Donnadieu P, Sigli C, Weyland M.Acta Mater, 2013; 61: 2207
[12] Ovri H, J?gle E A, Stark A, Lilleodden E T.Mater Sci Eng, 2015; A637: 162
[13] Thomas D, Frédéric D G, Williams L, Christophe S, Alexis D.Mater Sci Eng, 2014; A605: 119
[14] Huang B P, Zheng Z Q.Scr Mater, 1998; 38: 357
[15] Cassada W A, Shiflet G J, Jr Starke E A.Metall Mater Trans, 1991; 22A: 299
[16] Gable B M, Zhu A W, Csontos A A, Jr Starke E A.J Light Met, 2001; 1: 1
[17] Buchheit R G, Moran J P, Stoner G E.Corrosion, 1994; 50: 120
[18] Proton V, Alexis J, Andrieu E, Delfosse J, Deschamps A, Geuser F D, Lafont M C, Blanc C.Corros Sci, 2014; 80: 494
[19] Decreus B B, Deschamps A, Geuser F D, Sigli C.Adv Eng Mater, 2013; 15: 1082
[20] Li H Y, Tang Y, Z Z D, Zheng F.Trans Nonferrous Met Soc China, 2008; 18: 778
[21] Noble B, Thompson G E.Met Sci J, 1972; 6: 167
[22] Sinyavskii V S, Semenov A M.Prot Met, 2002; 38: 132
[23] Feng D. Metal Physics.Vol.1, Beijing: Science Press, 1998: 305
[23] (冯端. 金属物理学. 第1卷, 北京: 科学出版社, 1998: 305)
[24] Kumar K S, Brown S A, Pickens J R.Acta Mater, 1996; 44: 1899
[25] Yoshimura R, Konno T J, Abe E, Hiraga K.Acta Mater, 2003; 51: 4251
[26] Kumar K S, Brown S A, Pickens J R.Scr Metall Mater, 1990; 24: 1245
[27] Gayle F W, Heubaum F H, Pickens J R.Scr Metall Mater, 1990; 24: 79
[28] Zhang L, Chen Q Z, Wang Y Y, Yan W D.J Aeronaut Mater, 2007; 27(4): 31
[28] (张蕾, 陈群志, 王逾涯, 严卫东. 航空材料学报, 2007; 27(4): 31)
[29] Liu B X, Li G A.Heat Treat Met, 2004; 29(5): 32
[29] (刘北兴, 李国爱. 金属热处理, 2004; 29(5): 32)
[1] 王迪, 贺莉丽, 王栋, 王莉, 张思倩, 董加胜, 陈立佳, 张健. Pt-Al涂层对DD413合金高温拉伸性能的影响[J]. 金属学报, 2023, 59(3): 424-434.
[2] 孙腾腾, 王洪泽, 吴一, 汪明亮, 王浩伟. 原位自生2%TiB2 颗粒对2024Al增材制造合金组织和力学性能的影响[J]. 金属学报, 2023, 59(1): 169-179.
[3] 郑椿, 刘嘉斌, 江来珠, 杨成, 姜美雪. 拉伸变形对高氮奥氏体不锈钢显微组织和耐腐蚀性能的影响[J]. 金属学报, 2022, 58(2): 193-205.
[4] 刘先锋, 刘冬, 刘仁慈, 崔玉友, 杨锐. Ti-43.5Al-4Nb-1Mo-0.1B合金的包套热挤压组织与拉伸性能[J]. 金属学报, 2020, 56(7): 979-987.
[5] 余晨帆, 赵聪聪, 张哲峰, 刘伟. 选区激光熔化316L不锈钢的拉伸性能[J]. 金属学报, 2020, 56(5): 683-692.
[6] 李源才, 江五贵, 周宇. 纳米孔洞对单晶/多晶Ni复合体拉伸性能的影响[J]. 金属学报, 2020, 56(5): 776-784.
[7] 王希,刘仁慈,曹如心,贾清,崔玉友,杨锐. 冷却速率对β凝固γ-TiAl合金硼化物和室温拉伸性能的影响[J]. 金属学报, 2020, 56(2): 203-211.
[8] 蔡超,李煬,李劲风,张昭,张鉴清. 2A97 Al-Li合金薄板时效析出与电位及晶间腐蚀的相关性研究[J]. 金属学报, 2019, 55(8): 958-966.
[9] 刘征,刘建荣,赵子博,王磊,王清江,杨锐. 电子束快速成形制备TC4合金的组织和拉伸性能分析[J]. 金属学报, 2019, 55(6): 692-700.
[10] 任德春, 苏虎虎, 张慧博, 王健, 金伟, 杨锐. 冷旋锻变形对TB9钛合金显微组织和拉伸性能的影响[J]. 金属学报, 2019, 55(4): 480-488.
[11] 陈胜虎, 戎利建. Ni-Fe-Cr合金固溶处理后的组织变化及其对性能的影响[J]. 金属学报, 2018, 54(3): 385-392.
[12] 李冬冬, 钱立和, 刘帅, 孟江英, 张福成. Mn含量对Fe-Mn-C孪生诱发塑性钢拉伸变形行为的影响[J]. 金属学报, 2018, 54(12): 1777-1784.
[13] 陈瑞, 许庆彦, 郭会廷, 夏志远, 吴勤芳, 柳百成. Al-7Si-Mg铝合金拉伸过程应变硬化行为及力学性能模拟研究[J]. 金属学报, 2017, 53(9): 1110-1124.
[14] 席明哲, 吕超, 吴贞号, 尚俊英, 周玮, 董荣梅, 高士友. 连续点式锻压激光快速成形TC11钛合金的组织和力学性能[J]. 金属学报, 2017, 53(9): 1065-1074.
[15] 杨金侠,徐福涛,周动林,孙元,侯星宇,崔传勇. 重熔工艺对K452合金高温拉伸性能的影响[J]. 金属学报, 2017, 53(6): 703-708.