| 位错对Ti-6Al-4V合金α相形核及微织构形成的影响* |
张金虎1,徐东生1( ),王云志2,杨锐1 |
1 中国科学院金属研究所, 沈阳 110016. 2 The Ohio State University, Columbus, OH 43210, USA |
|
| INFLUENCES OF DISLOCATIONS ON NUCLEATION AND MICRO-TEXTURE FORMATION OFα PHASE IN Ti-6Al-4V ALLOY |
Jinhu ZHANG1,Dongsheng XU1( ),Yunzhi WANG2,Rui YANG1 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 The Ohio State University, Columbus, OH 43210, USA |
引用本文:
张金虎,徐东生,王云志,杨锐. 位错对Ti-6Al-4V合金α相形核及微织构形成的影响*[J]. 金属学报, 2016, 52(8): 905-915.
Jinhu ZHANG,
Dongsheng XU,
Yunzhi WANG,
Rui YANG.
INFLUENCES OF DISLOCATIONS ON NUCLEATION AND MICRO-TEXTURE FORMATION OFα PHASE IN Ti-6Al-4V ALLOY[J]. Acta Metall Sin, 2016, 52(8): 905-915.
| [1] | Furuhara T, Maki T.Mater Sci Eng, 2001; A312: 145 | | [2] | Gey N, Humbert M, Philippe M J, Combres Y.Mater Sci Eng, 1997; A230: 68 | | [3] | Feng Z Q, Yang Y Q, Huang B, Luo X, Li M H, Han M, Fu M S.Acta Mater, 2011; 59: 2412 | | [4] | van Bohemen S M C, Kamp A, Petrov R H, Kestens L A I, Sietsma J.Acta Mater, 2008; 56: 5907 | | [5] | Bhattacharyya D, Viswanathan G B, Denkenberger R, Furrer D, Fraser H L.Acta Mater, 2003; 51: 4679 | | [6] | Bhattacharyya D, Viswanathan G B, Fraser H L.Acta Mater, 2007; 55: 6765 | | [7] | Shi R, Wang Y.Acta Mater, 2013; 61: 6006 | | [8] | Glavicic M, Goetz R, Barker D, Shen G, Furrer D, Woodfield A, Semiatin S.Metall Mater Trans, 2008; 39A: 887 | | [9] | Bate P, Hutchinson B.Acta Mater, 2000; 48: 3183 | | [10] | Germain L, Gey N, Humbert M, Vo P, Jahazi M, Bocher P.Acta Mater, 2008; 56: 4298 | | [11] | Banerjee D, Williams J C.Acta Mater, 2013; 61: 844 | | [12] | Germain L, Gey N, Humbert M, Bocher P, Jahazi M.Acta Mater, 2005; 53: 3535 | | [13] | Humbert M, Germain L, Gey N, Bocher P, Jahazi M.Mater Sci Eng, 2006; A430: 157 | | [14] | Thomas G, Nutting J.The Mechanism of Phase Transformations in Metals .London: Institute of Metals, 1956: 57 | | [15] | Xu D S, Wang H, Teng C Y, Zhang J H, Wu H N, Bai C G, Yang R.e-Sci Technol Appl, 2015; 6(3): 14 | | [15] | (徐东生, 王皞, 滕春禹, 张金虎, 武鹤楠, 柏春光, 杨锐. 科研信息化技术与应用, 2015; 6(3): 14) | | [16] | Teng C Y, Zhou N, Wang Y, Xu D S, Du A, Wen Y H, Yang R.Acta Mater, 2012; 60: 6372 | | [17] | Teng C Y, Du A, Xu D S, Wang Y, Yang R.Intermetallics, 2015; 65: 1 | | [18] | Yin J, Barnett D M, Cai W.Model Simul Mater Sci Eng, 2010; 18: 045013 | | [19] | Ledbetter H, Ogi H, Kai S, Kim S, Hirao M.J Appl Phys, 2004; 95: 4642 | | [20] | Burgers W G.Physica, 1934; 1: 561 | | [21] | Geng F, Niinomi M, Nakai M.Mater Sci Eng, 2011; A528: 5435 | | [22] | Savage M, Tatalovich J, Mills M.Philos Mag, 2004; 84: 1127 | | [23] | Khachaturyan A G.Theory of Structural Transformations in Solids. New York: John Wiley & Sons, Inc, 1983: 198 | | [24] | Wang Y U, Jin Y M, Cuiti?o A M, Khachaturyan A G.Acta Mater, 2001; 49: 1847 | | [25] | Qiu D, Shi R, Zhang D, Lu W, Wang Y.Acta Mater, 2015; 88: 218 | | [26] | Zhou N, Lv D C, Zhang H L, McAllister D, Zhang F, Mills M J, Wang Y,Acta Mater, 2014; 65: 270 | | [27] | Shi R, Ma N, Wang Y.Acta Mater, 2012; 60: 4172 | | [28] | Yang M, Wang G, Teng C Y, Xu D S, Zhang J, Yang R, Wang Y.Acta Metall Sin, 2012; 48: 148 | | [28] | (杨梅, 王刚, 滕春禹, 徐东生, 张鉴, 杨锐, 王云志. 金属学报, 2012; 48: 148) | | [29] | Wang G, Xu D S, Ma N, Zhou N, Payton E J, Yang R, Mills M J, Wang Y.Acta Mater, 2009; 57: 316 | | [30] | Wang Y, Chen L Q. Simulation of Microstructural Evolution Using the Field Method. New York: John Wiley & Sons, Inc, 2000: 2a3.1 | | [31] | Zhang J H, Teng C Y, Yang M, Xu D S, Wang Y, Yang R.Chin Nonferrous Met, 2013; 23(suppl): s296 | | [31] | (张金虎, 滕春禹, 杨梅, 徐东生, 王云志, 杨锐. 中国有色金属学报, 2013; 23(特刊): s296) | | [32] | Hull D, Bacon D J.Introduction to Dislocations. 5th Ed., Oxford: Elsevier Ltd, 2011: 63 | | [33] | Furuhara T, Nakamori H, Maki T.Mater Trans, 1992; 33: 585 | | [34] | Ba?tecká J.Czech J Phys, 1965; 15B: 595 | | [35] | Wang S C, Aindow M, Starink M J.Acta Mater, 2003; 51: 2485 | | [36] | Heo T W, Bhattacharyya S, Chen L Q.Philos Mag, 2013; 93: 1468 | | [37] | Wang S, Starink M, Ubhi H, Li W.Rev Adv Mater Sci, 2012; 32: 47 |
|
|