| 激光冲击诱导的航空铝合金表层高熵结构及其抗蚀性 |
罗新民1, 王翔1( ), 陈康敏1,2, 鲁金忠3, 王兰1, 张永康4 |
1 江苏大学材料科学与工程学院, 镇江 212013 2 江苏大学分析中心, 镇江 212013 3 江苏大学机械工程学院, 镇江 212013 4 东南大学机械工程学院, 南京 210089 |
|
| SURFACE LAYER HIGH-ENTROPY STRUCTURE AND ANTI-CORROSION PERFORMANCE OF AERO-ALUMINUM ALLOY INDUCED BY LASER SHOCK PROCESSING |
LUO Xinmin1( ), WANG Xiang1, CHEN Kangmin1,2, LU Jinzhong3, WANG Lan1, ZHANG Yongkang4 |
1 School of Materials Science and Engineering, Jiangsu University, Zhenjiang 212013 2 Analysis and Test Center, Jiangsu University, Zhenjiang 212013 3 School of Mechanical Engineering, Jiangsu University, Zhenjiang 212013 4 School of Mechanical Engineering, Southeast University, Nanjing 210089 |
引用本文:
罗新民, 王翔, 陈康敏, 鲁金忠, 王兰, 张永康. 激光冲击诱导的航空铝合金表层高熵结构及其抗蚀性[J]. 金属学报, 2015, 51(1): 57-66.
Xinmin LUO,
Xiang WANG,
Kangmin CHEN,
Jinzhong LU,
Lan WANG,
Yongkang ZHANG.
SURFACE LAYER HIGH-ENTROPY STRUCTURE AND ANTI-CORROSION PERFORMANCE OF AERO-ALUMINUM ALLOY INDUCED BY LASER SHOCK PROCESSING[J]. Acta Metall Sin, 2015, 51(1): 57-66.
| [1] |
Fairand B P, Wilcox B A, Gallagher W J. Appl Phys, 1972; 43: 3893
|
| [2] |
Gomez R G, Rubio G C, Ocaña J L. Appl Surf Sci, 2010; 256: 5828
|
| [3] |
Hatamleh O, Lyons J, Forman R. Int J Fatigue, 2007; 29: 421
|
| [4] |
Lu J Z, Luo K Y, Zhang Y K, Cui C Y, Sun G F, Zhou J Z, Zhang L, You J, Chen K M, Zhong J W. Acta Mater, 2010; 58: 3984
|
| [5] |
Wu B, Wang S B, Guo D H, Wu H X. Acta Opt Sin, 2005; 25: 1352
|
| [5] |
(吴 边, 王声波, 郭大浩, 吴鸿兴. 光学学报, 2005; 25: 1352)
|
| [6] |
Yeh J W, Chen S K, Lin S J, Gan J Y, Chin T S, Shun T T, Tsau C H, Chang S Y. Adv Eng Mater, 2004; 6: 299
|
| [7] |
Zhang Y, Zuo T T, Tang Z, Gao M C, Dahmen K A, Liaw P K, Zhao P L. Prog Mater Sci, 2014; 61(4): 1
|
| [8] |
Daniel B, Miracle J D, Miller O N, Senkov C W, Michael D U, Tiley J. Entropy, 2014; 16: 494
|
| [9] |
Ren M X, Li B S, Fu H Z. Trans Nonferrous Met Soc China, 2013; 23: 991
|
| [10] |
Sun H F. Master Thesis, Shandong University of Science and Technology, Jinan, 2009
|
| [10] |
(孙宏飞. 山东科技大学硕士学位论文, 济南, 2009)
|
| [11] |
Zhang H, Pan Y, He Y Z. Acta Metall Sin, 2011; 47: 1075
|
| [11] |
(张 晖, 潘 冶, 何宜柱. 金属学报, 2011; 47: 1075)
|
| [12] |
Chen M, Liu Y, Li Y X, Chen X. Acta Metall Sin, 2007; 43: 1020
|
| [12] |
(陈 敏, 刘 源, 李言祥, 陈 祥. 金属学报, 2007; 43: 1020)
|
| [13] |
Song C H, Gan Z H, Lu Z H, Chen H J, Huang F. J Mater Sci Eng, 2011; 29: 747
|
| [13] |
(宋春晖, 甘章华, 卢志红, 陈汉杰, 黄 峰. 材料科学与工程学报, 2011; 29: 747)
|
| [14] |
Zhou Y J, Zhang Y, Wang Y L, Chen G L. Rare Met Mater Eng, 2007; 36: 2136
|
| [14] |
(周云军, 张 勇, 王艳丽, 陈国良. 稀有金属材料与工程, 2007; 36: 2136)
|
| [15] |
Yu Y, Xie F Q, Zhang T B, Kou H C, Hu R, Li J S. Rare Met Mater Eng, 2012; 41: 862
|
| [15] |
(于 源, 谢发勤, 张铁邦, 寇宏超, 胡 锐, 李金山. 稀有金属材料与工程, 2012; 41: 862)
|
| [16] |
Liu S Q, Huang W G. Mater Eng, 2012; (1): 5
|
| [16] |
(刘恕骞, 黄维刚. 材料工程, 2012; (1): 5)
|
| [17] |
Zhang S, Wu C L, Wang C, Yi J Z, Zhang C H. Acta Metall Sin, 2014; 50: 555
|
| [17] |
(张 松, 吴臣亮, 王 超, 伊俊振, 张春华. 金属学报, 2014; 50: 555 )
|
| [18] |
Yue T M, Xie H, Lin X, Yang H O, Meng G H. Entropy, 2013; 15: 2833
|
| [19] |
Zhang Y K, Xu X J, Luo Y, Song T, Wang H Y, Wu G C, Zhang Z Q. Rare Met Mater Eng, 2012; 41(Suppl 2): 612
|
| [19] |
(张允康, 许晓静, 罗 勇, 宋 涛, 王宏宇, 吴桂潮, 张振强. 稀有金属材料与工程, 2012; 41(增刊2): 612)
|
| [20] |
Ning A L, Liu Z Y, Feng C, Zeng S M. Acta Metall Sin, 2006; 42: 1253
|
| [20] |
(宁爱林, 刘志义, 冯 春, 曾苏民. 金属学报, 2006; 42: 1253)
|
| [21] |
Ren N F, Zhang Y K. Appl Laser, 1997; 17: 105
|
| [21] |
(任乃飞, 张永康. 应用激光, 1997; 17: 105)
|
| [22] |
Tian Y Q, Zhang H J, Chen L S, Song J Y, Xu Y, Zhang S H. Acta Metall Sin, 2014; 50: 531
|
| [22] |
(田亚强, 张宏军, 陈连生, 宋进英, 徐 勇, 张士宏. 金属学报, 2014; 50: 531)
|
| [23] |
Inoue A, Takauchi A. Mater Trans, 2002; 43: 1892
|
| [24] |
Liang X B, Zhang Z B, Chen Y X, Xu B S. Acta Metall Sin, 2012; 48: 289
|
| [24] |
(梁秀兵, 张志彬, 陈永雄, 徐滨士. 金属学报, 2012; 48: 289)
|
| [25] |
Wang Z L. Master Thesis, Northeastern University, Shenyang, 2009
|
| [25] |
(王志良. 东北大学硕士学位论文, 沈阳, 2009)
|
| [26] |
Zhang J. J Chin Rare Earth Soc, 2006; 24(10): 40
|
| [26] |
(张 鉴. 中国稀土学报, 2006; 24(10): 40)
|
| [27] |
Lang Y J, Cui H, Cai Y H, Zhang J S. Chin J Mater Res, 2012; 26: 143
|
| [27] |
(郎玉婧, 崔 华, 蔡元华, 张济山. 材料研究学报, 2012; 26: 143)
|
| [28] |
Wang Y, Zhang W L, Sun D B, Li H Q. J Mater Sci Eng, 2006; 24: 292
|
| [28] |
(王 玉, 张文礼, 孙冬柏, 李辉勤. 材料科学与工程学报, 2006; 24: 292)
|
| [29] |
Zhu L F, Li Y C, Hu X Z, Dong J. Acta Mech Solid Sin, 2005; 26: 37
|
| [29] |
(朱林法, 李永池, 胡秀章, 董 杰. 固体力学学报, 2005; 26: 37)
|
| [30] |
Rosakis P, Rosakis A J, Ravichandran G, Hodowany J. J Mech Phys Solids, 2000; 48: 581
|
| [31] |
Luo X M, Zhang J W, Ma H, Zhang Y K, Chen K M, Ren X D, Luo K Y. Acta Opt Sin, 2011; 31: 714002-1
|
| [31] |
(罗新民, 张静文, 马 辉, 张永康, 陈康敏, 任旭东, 罗开玉. 光学学报, 2011; 31: 714002-1)
|
| [32] |
Luo X M, Chen K M, Zhang J W, Lu J Z, Ren X D, Luo K Y, Zhang Y K. Acta Metall Sin, 2013; 49: 667
|
| [32] |
(罗新民, 陈康敏, 张静文, 鲁金忠, 任旭东, 罗开玉, 张永康. 金属学报, 2013; 49: 667)
|
| [33] |
Luo X M, Zhao G Z, Yang K, Chen K M, Zhang X N, Zhang Y K, Luo K Y, Ren X D. Chin J Lasers, 2011; 39: 0603001-1
|
| [33] |
(罗新民, 赵广志, 杨 坤, 陈康敏, 张晓柠, 张永康, 罗开玉, 任旭东. 中国激光, 2011; 39: 0603001-1)
|
| [34] |
Sui M L, Wang Y B, Cui J P, Li B Q. J Chin Electr Microsc Soc, 2010; 29: 219
|
| [34] |
(隋曼龄, 王艳波, 崔静萍, 李白清. 电子显微学报, 2010; 29: 219)
|
| [35] |
Wan C Y, Chen J H, Yang X B, Liu J Z, Wu C L, Zhao X Q. J Chin Electr Microsc Soc, 2010; 29: 455
|
| [35] |
(万彩云, 陈江华, 杨修波, 刘吉梓, 伍翠兰, 赵新奇. 电子显微学报, 2010; 29: 455)
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|