| 升温速率对低碳无取向电工钢脱碳退火组织及织构的影响 |
夏冬生, 杨平( ), 谢利, 毛卫民 |
| 北京科技大学材料科学与工程学院, 北京 100083 |
|
| INFLUENCE OF HEATING RATE ON THE DECARBU- RIZED ANNEALING MICROSTRUCTURE AND TEXTURE IN LOW-CARBON NON-ORIENTED ELECTRICAL STEEL |
XIA Dongsheng, YANG Ping( ), XIE Li, MAO Weimin |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083 |
引用本文:
夏冬生, 杨平, 谢利, 毛卫民. 升温速率对低碳无取向电工钢脱碳退火组织及织构的影响[J]. 金属学报, 2014, 50(12): 1437-1445.
Dongsheng XIA,
Ping YANG,
Li XIE,
Weimin MAO.
INFLUENCE OF HEATING RATE ON THE DECARBU- RIZED ANNEALING MICROSTRUCTURE AND TEXTURE IN LOW-CARBON NON-ORIENTED ELECTRICAL STEEL[J]. Acta Metall Sin, 2014, 50(12): 1437-1445.
| [1] |
He Z Z,Zhao Y,Luo H W. Electrical Steels. Beijing: Metallurgical Industry Press, 2012: 187
|
| [1] |
(何忠治,赵 宇,罗海文. 电工钢. 北京: 冶金工业出版社, 2012: 187)
|
| [2] |
Park J T, Szpunar J A, Cha S Y. ISIJ Int, 2003; 43: 1611
|
| [3] |
Tomida T, Tanaka T. ISIJ Int, 1995; 35: 548
|
| [4] |
Tomida T. J Appl Phys, 1996; 79: 5443
|
| [5] |
Tomida T. J Mater Eng Perform, 1996; 5: 316
|
| [6] |
Tomida T, Uenoya S. IEEE Trans Magn, 2001; 37: 2318
|
| [7] |
Tomida T, Sano N, Ueda K, Fujiwarab K, Takahashi N. J Magn Magn Mater, 2003; 254-255: 315
|
| [8] |
Tomida T. Metall Trans, 2003; 44: 1096
|
| [9] |
Kovac F, Dzubinsky M, Sidor Y. J Magn Magn Mater, 2004; 269: 333
|
| [10] |
He L J. Wuhan Iron Steel Corp Technol, 1981; (3): 58
|
| [10] |
(何礼君. 武钢技术, 1981; (3): 58)
|
| [11] |
He L J, Pei D R. Wuhan Iron Steel Corp Technol, 1981; (4): 28
|
| [11] |
(何礼君, 裴大荣. 武钢技术, 1981; (4): 28)
|
| [12] |
Xie L,Yang P,Zhang N,Mao W M
|
| [13] |
Marder A R. Metall Trans, 1986; 17A: 1227
|
| [14] |
Ashbrook R W J, Marder A R. Metall Trans, 1985; 16A: 897
|
| [15] |
Swisher J H. Trans TMS AIME, 1968; 242: 763
|
| [16] |
Pyyry J, Kettunen E. Scand J Met, 1973; 2: 265
|
| [17] |
Marder A, Perpetua S M, Kowalik J A, Stephenson E T. Metall Trans, 1985; 16A: 1160
|
| [18] |
Sidor Y, Kovac F. Mater Charact, 2005; 55: 1
|
| [19] |
Dzubinsky M, Sidor Y, Kovac F. Mater Sci Eng, 2004; A385: 449
|
| [20] |
Sidor Y, Kovac F, Kvackaj T. Acta Mater, 2007; 55: 1711
|
| [21] |
Mao W M,Zhao X B. Recrystallization and Grain Growth in Metals. Beijing: Metallurgical Industry Press, 1994: 274
|
| [21] |
(毛卫民,赵新兵. 金属的再结晶与晶粒长大. 北京: 冶金工业出版社, 1994: 274)
|
| [22] |
Carlos R O. Scr Mater, 1996; 35: 1253
|
| [23] |
Takashima M, Komatsubara M, Morit N. ISIJ Int, 1997; 37: 1263
|
| [24] |
Park J T, Szpunar J A. Acta Mater, 2003; 51: 3037
|
| [25] |
Xie L, Yang P, Zhang N, Zong C, Xia D S, Mao W M. J Magn Magn Mater, 2014; 356: 1
|
| [26] |
Sung J K, Lee D N, Wang D H. ISIJ Int, 2011; 51: 284
|
| [27] |
Sung J K, Park S M, Shim B Y. Mater Sci Forum, 2012; 702-703: 730
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|