| 一种超高碳钢的滚动接触疲劳研究 |
刘宏基1, 孙俊杰1, 江涛1, 郭生武1, 柳永宁1( ), 林鑫2 |
1 西安交通大学材料科学与工程学院金属材料强度国家重点实验室, 西安 710049 2 西北工业大学材料科学与工程学院, 西安 710072 |
|
| ROLLING CONTACT FATIGUE BEHAVIOR OF AN ULTRAHIGH CARBON STEEL |
LIU Hongji1, SUN Junjie1, JIANG Tao1, GUO Shengwu1, LIU Yongning1( ), LIN Xin2 |
1 State Key Laboratory for Mechanical Behavior of Materials, School of Materials Science and Engineering,Xi′an Jiaotong University, Xi′an 710049 2 School of Materials Science and Engineering, Northwestern Polytechnical University, Xi′an 710072 |
引用本文:
刘宏基, 孙俊杰, 江涛, 郭生武, 柳永宁, 林鑫. 一种超高碳钢的滚动接触疲劳研究[J]. 金属学报, 2014, 50(12): 1446-1452.
Hongji LIU,
Junjie SUN,
Tao JIANG,
Shengwu GUO,
Yongning LIU,
Xin LIN.
ROLLING CONTACT FATIGUE BEHAVIOR OF AN ULTRAHIGH CARBON STEEL[J]. Acta Metall Sin, 2014, 50(12): 1446-1452.
| [1] |
Sherby O D, Cady J E M, Walser B, Young C M. US Pat, 3951697, 1976
|
| [2] |
Wadsworth J, Sherby O D. Prog Mater Sci, 1980; 25: 35
|
| [3] |
Lesuer D R, Syn C K, Sherby O D. SAE Tech Paper, 960314, 1996, doi:10.4271/960314
|
| [4] |
Wadsworth J, Sherby O D. J Mech Work Technol, 1978; 2: 53
|
| [5] |
Kayali E S, Sunada H, Oyama T, Wadsworth J, Sherby O D. J Mater Sci, 1979; 14: 2688
|
| [6] |
Sunada H, Wadsworth J, Lin J, Sherby O D. Mater Sci Eng, 1979; 38: 35
|
| [7] |
Chen X, Liu Y, Zhu J, Ge L. Tribol Lett, 2010; 38: 79
|
| [8] |
Zhu J W, Yan X, Liu Y N. Mater Sci Eng, 2004; A385: 440
|
| [9] |
Zhang Z L, Liu Y N, Yu G, Zhu J W, He T. Acta Metall Sin, 2009; 45: 280
|
| [9] |
(张占领, 柳永宁, 于 光, 朱洁武, 何 涛. 金属学报, 2009; 45: 280)
|
| [10] |
Hengerer F. Ball Bearing J, 1987; 231: 2
|
| [11] |
Bhadeshia H K D H. Prog Mater Sci, 2012; 57: 268
|
| [12] |
Liu H, Tang B, Wang L, Wang X, Jiang B. Surf Coat Technol, 2007; 201: 5273
|
| [13] |
Liu H X, Wang L P, Wang X F, Huang L, Tang B Y. Acta Metall Sin, 2006; 42: 1197
|
| [13] |
(刘洪喜, 王浪平, 王小峰, 黄 磊, 汤宝寅. 金属学报, 2006; 42: 1197)
|
| [14] |
Liu H X, Jiang Y H, Zhou R, Zhou R F, Jin Q L, Tang B Y. Acta Metall Sin, 2008; 44: 325
|
| [14] |
(刘洪喜, 蒋业华, 周 荣, 周荣峰, 金青林, 汤宝寅. 金属学报, 2008; 44: 325)
|
| [15] |
Kuhn M, Gold P W, Loos J. Surf Coat Technol, 2004; 177-178: 469
|
| [16] |
Nakashima H. NTN Tech Rev, 2008; 76: 10
|
| [17] |
O'Brien M J,Presser N,Robinson E Y. Eng Fail Anal, 2003; 10: 453
|
| [18] |
Szost B A, Vegter R H, Rivera-Díaz-del-Castillo P E J. Mater Des, 2013; 43: 499
|
| [19] |
Lian F L, Liu H J, Sun J J, Sun X J, Guo S W, Liu Y N. J Mater Res, 2013; 28: 757
|
| [20] |
Rivero I V, Ruud C O. Mater Charact, 2004; 53: 381
|
| [21] |
Yoon D J, Lee M H, Jin J K, Kang S H, Nam T H. Met Mater, 2000; 6: 429
|
| [22] |
Kim K H, Lee J S. Mater Sci Technol, 2012; 28: 50
|
| [23] |
Zaretsky E V. NASA Tech Memorandum, 88881, 1986,
|
| [24] |
Ringsberg J W. Int J Fatigue, 2001; 23: 575
|
| [25] |
Kumar S, Curtin W A. Mater Today, 2007; 10: 34
|
| [26] |
Zhai T, Wilkinson A J, Martin J W. Acta Mater, 2000; 48: 4917
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|