金属学报  2014, Vol. 50 Issue (12): 1437-1445    DOI: 10.11900/0412.1961.2014.00311
  本期目录 | 过刊浏览 |
升温速率对低碳无取向电工钢脱碳退火组织及织构的影响
夏冬生, 杨平(), 谢利, 毛卫民
北京科技大学材料科学与工程学院, 北京 100083
INFLUENCE OF HEATING RATE ON THE DECARBU- RIZED ANNEALING MICROSTRUCTURE AND TEXTURE IN LOW-CARBON NON-ORIENTED ELECTRICAL STEEL
XIA Dongsheng, YANG Ping(), XIE Li, MAO Weimin
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
引用本文:

夏冬生, 杨平, 谢利, 毛卫民. 升温速率对低碳无取向电工钢脱碳退火组织及织构的影响[J]. 金属学报, 2014, 50(12): 1437-1445.
Dongsheng XIA, Ping YANG, Li XIE, Weimin MAO. INFLUENCE OF HEATING RATE ON THE DECARBU- RIZED ANNEALING MICROSTRUCTURE AND TEXTURE IN LOW-CARBON NON-ORIENTED ELECTRICAL STEEL[J]. Acta Metall Sin, 2014, 50(12): 1437-1445.

全文: PDF(8100 KB)   HTML
摘要: 

研究了不同升温速率下低碳电工钢两相区脱碳退火组织与织构的演变规律. 结果表明, 脱碳退火升温速率对最终组织和织构均有显著影响: 升温速率决定了柱状晶的“形核”位置, 慢速升温时, 柱状晶“晶核”在表层向里的一定范围内形成, 最终在样品表面附近形成小尺寸晶粒层, 而快速升温则形成完整的柱状晶组织; 慢速升温时获得强g线织构及相对较弱的a线织构, 而快速升温则使g线织构大幅度减弱, a线组分有所增强, 并产生了一定强度的{001}<120>织构. 实验结果证明, 最终的脱碳退火织构主要取决于“形核”处再结晶晶粒的织构成分.

关键词 : 电工钢,  柱状晶,  组织,  织构,  升温速率    
Abstract:

The present work investigates the effect of heating rate on the evolution of decarburized microstructures and textures in low-carbon electrical steels within the inter-critical temperature region. The results show that heating rate has a significant effect on both the final microstructures and textures during the process of decarburization annealing. The ''nucleation'' sites of columnar grains are determined by the heating rate. Slow heating rate would have the ''nuclei'' formed within a certain range of the surface layer, and finally leading to a fine-grained layer near the sample surface. By comparison, a complete columnar microstructure is acquired under the rapid heating condition. Strong g-fiber and relatively weak a-fiber components were obtained at the slow heating rate. In contrast, g-fiber texture is greatly weakened and a-fiber component slightly strengthened under the rapid heating condition, and a relatively strong {001}<120> texture is formed at the same time. The experimental results prove that the final decarburized textures are mainly dependent upon the texture component of recrystallized grains in the ''nucleation'' sites.

Key words: electrical steel    columnar grain    microstructure    texture    heating rate
    
ZTFLH:  TG111  
基金资助:* 国家自然科学基金资助项目 51071024
作者简介: null

夏冬生, 男, 1989年生, 硕士生

图1  实验工艺路线图
图2  低碳电工钢在不同工艺条件下的脱碳退火组织
图3  不同升温速率下脱碳退火样品的EBSD图及相应的φ2=45°截面取向分布函数(ODF)图
图4  不同升温速率下样品表层的再结晶织构统计
图5  慢速升温下的部分再结晶组织
图6  不同升温速率下样品内部的温度分布曲线示意图
图7  不同升温速率下的相关织构的统计
图8  H2DA2冷轧板部分再结晶及相应脱碳退火后的EBSD图、极图及φ2=45°截面ODF图
[1] He Z Z,Zhao Y,Luo H W. Electrical Steels. Beijing: Metallurgical Industry Press, 2012: 187
[1] (何忠治,赵 宇,罗海文. 电工钢. 北京: 冶金工业出版社, 2012: 187)
[2] Park J T, Szpunar J A, Cha S Y. ISIJ Int, 2003; 43: 1611
[3] Tomida T, Tanaka T. ISIJ Int, 1995; 35: 548
[4] Tomida T. J Appl Phys, 1996; 79: 5443
[5] Tomida T. J Mater Eng Perform, 1996; 5: 316
[6] Tomida T, Uenoya S. IEEE Trans Magn, 2001; 37: 2318
[7] Tomida T, Sano N, Ueda K, Fujiwarab K, Takahashi N. J Magn Magn Mater, 2003; 254-255: 315
[8] Tomida T. Metall Trans, 2003; 44: 1096
[9] Kovac F, Dzubinsky M, Sidor Y. J Magn Magn Mater, 2004; 269: 333
[10] He L J. Wuhan Iron Steel Corp Technol, 1981; (3): 58
[10] (何礼君. 武钢技术, 1981; (3): 58)
[11] He L J, Pei D R. Wuhan Iron Steel Corp Technol, 1981; (4): 28
[11] (何礼君, 裴大荣. 武钢技术, 1981; (4): 28)
[12] Xie L,Yang P,Zhang N,Mao W M
[13] Marder A R. Metall Trans, 1986; 17A: 1227
[14] Ashbrook R W J, Marder A R. Metall Trans, 1985; 16A: 897
[15] Swisher J H. Trans TMS AIME, 1968; 242: 763
[16] Pyyry J, Kettunen E. Scand J Met, 1973; 2: 265
[17] Marder A, Perpetua S M, Kowalik J A, Stephenson E T. Metall Trans, 1985; 16A: 1160
[18] Sidor Y, Kovac F. Mater Charact, 2005; 55: 1
[19] Dzubinsky M, Sidor Y, Kovac F. Mater Sci Eng, 2004; A385: 449
[20] Sidor Y, Kovac F, Kvackaj T. Acta Mater, 2007; 55: 1711
[21] Mao W M,Zhao X B. Recrystallization and Grain Growth in Metals. Beijing: Metallurgical Industry Press, 1994: 274
[21] (毛卫民,赵新兵. 金属的再结晶与晶粒长大. 北京: 冶金工业出版社, 1994: 274)
[22] Carlos R O. Scr Mater, 1996; 35: 1253
[23] Takashima M, Komatsubara M, Morit N. ISIJ Int, 1997; 37: 1263
[24] Park J T, Szpunar J A. Acta Mater, 2003; 51: 3037
[25] Xie L, Yang P, Zhang N, Zong C, Xia D S, Mao W M. J Magn Magn Mater, 2014; 356: 1
[26] Sung J K, Lee D N, Wang D H. ISIJ Int, 2011; 51: 284
[27] Sung J K, Park S M, Shim B Y. Mater Sci Forum, 2012; 702-703: 730
[1] 马德新, 赵运兴, 徐维台, 王富. 重力对高温合金定向凝固组织的影响[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] 宫声凯, 刘原, 耿粒伦, 茹毅, 赵文月, 裴延玲, 李树索. 涂层/高温合金界面行为及调控研究进展[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] 王磊, 刘梦雅, 刘杨, 宋秀, 孟凡强. 镍基高温合金表面冲击强化机制及应用研究进展[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] 张雷雷, 陈晶阳, 汤鑫, 肖程波, 张明军, 杨卿. K439B铸造高温合金800℃长期时效组织与性能演变[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] 卢楠楠, 郭以沫, 杨树林, 梁静静, 周亦胄, 孙晓峰, 李金国. 激光增材修复单晶高温合金的热裂纹形成机制[J]. 金属学报, 2023, 59(9): 1243-1252.
[6] 陈礼清, 李兴, 赵阳, 王帅, 冯阳. 结构功能一体化高锰减振钢研究发展概况[J]. 金属学报, 2023, 59(8): 1015-1026.
[7] 刘兴军, 魏振帮, 卢勇, 韩佳甲, 施荣沛, 王翠萍. 新型钴基与Nb-Si基高温合金扩散动力学研究进展[J]. 金属学报, 2023, 59(8): 969-985.
[8] 常松涛, 张芳, 沙玉辉, 左良. 偏析干预下体心立方金属再结晶织构竞争[J]. 金属学报, 2023, 59(8): 1065-1074.
[9] 李景仁, 谢东升, 张栋栋, 谢红波, 潘虎成, 任玉平, 秦高梧. 新型低合金化高强Mg-0.2Ce-0.2Ca合金挤压过程中的组织演变机理[J]. 金属学报, 2023, 59(8): 1087-1096.
[10] 孙蓉蓉, 姚美意, 王皓瑜, 张文怀, 胡丽娟, 仇云龙, 林晓冬, 谢耀平, 杨健, 董建新, 成国光. Fe22Cr5Al3Mo-xY合金在模拟LOCA下的高温蒸汽氧化行为[J]. 金属学报, 2023, 59(7): 915-925.
[11] 冯艾寒, 陈强, 王剑, 王皞, 曲寿江, 陈道伦. 低密度Ti2AlNb基合金热轧板微观组织的热稳定性[J]. 金属学报, 2023, 59(6): 777-786.
[12] 郭福, 杜逸晖, 籍晓亮, 王乙舒. 微电子互连用锡基合金及复合钎料热-机械可靠性研究进展[J]. 金属学报, 2023, 59(6): 744-756.
[13] 王法, 江河, 董建新. 高合金化GH4151合金复杂析出相演变行为[J]. 金属学报, 2023, 59(6): 787-796.
[14] 吴东江, 刘德华, 张子傲, 张逸伦, 牛方勇, 马广义. 电弧增材制造2024铝合金的微观组织与力学性能[J]. 金属学报, 2023, 59(6): 767-776.
[15] 张东阳, 张钧, 李述军, 任德春, 马英杰, 杨锐. 热处理对选区激光熔化Ti55531合金多孔材料力学性能的影响[J]. 金属学报, 2023, 59(5): 647-656.