| 异步轧制硅钢的表面纳米化及轧制参数的影响 |
刘刚1( ), 马野1, 张瑞君1, 王小兰2, 沙玉辉3, 左良3 |
1 东北大学研究院, 沈阳 110819 2 中国科学院金属研究所金属腐蚀与防护国家重点实验室, 沈阳 110016 3 东北大学材料电磁过程研究教育部重点实验室, 沈阳 110819 |
|
| SURFACE NANOCRYSTALLIZATION OF SILICON STEEL INDUCED BY ASYMMETRIC ROLLING AND EFFECT OF ROLLING PARAMETERS |
LIU Gang1( ), MA Ye1, ZHANG Ruijun1, WANG Xiaolan2, SHA Yuhui3, ZUO Liang3 |
1 Research Academy, Northeastern University, Shenyang 110819 2 State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Science, Shenyang 110016 3 Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University, Shenyang 110819 |
引用本文:
刘刚, 马野, 张瑞君, 王小兰, 沙玉辉, 左良. 异步轧制硅钢的表面纳米化及轧制参数的影响[J]. 金属学报, 2014, 50(9): 1071-1077.
Gang LIU,
Ye MA,
Ruijun ZHANG,
Xiaolan WANG,
Yuhui SHA,
Liang ZUO.
SURFACE NANOCRYSTALLIZATION OF SILICON STEEL INDUCED BY ASYMMETRIC ROLLING AND EFFECT OF ROLLING PARAMETERS[J]. Acta Metall Sin, 2014, 50(9): 1071-1077.
| [1] |
Lu K, Lu J. J Mater Sci Technol, 1999; 15: 193
|
| [2] |
Lu K, Lu J. Mater Sci Eng, 2004; A375-377: 38
|
| [3] |
Roland T, Retraint D, Lu K, Lu J. Mater Sci Eng, 2007; A445-446: 281
|
| [4] |
Yong X P, Liu G, Lu K, Lu J. J Mater Sci Technol, 2003; 19: 1
|
| [5] |
Li D, Chen H N, Xu H. Appl Surf Sci, 2009; 255: 3811
|
| [6] |
Zhou L, Liu G, Han Z, Lu K. Scr Mater, 2008; 58: 445
|
| [7] |
Wang T S, Yu J K, Dong B F. Surf Coat Technol, 2006; 200: 4777
|
| [8] |
Zhang H W, Wang L, Hei Z K, Liu G, Lu J, Lu K. Z Metallka, 2003; 94: 1143
|
| [9] |
Wang Z B, Lu J, Lu K. Surf Coat Technol, 2006; 201: 2796
|
| [10] |
Balusamy T,Narayanan T S N S, Ravichandran K. Surf Coat Technol, 2012; 213: 221
|
| [11] |
Ge L L, Tian N, Lu Z X, You C Y. Appl Surf Sci, 2013; 286: 412
|
| [12] |
Liu G, Wang S C, Lou X F, Lu J, Lu K. Scr Mater, 2001; 44: 1791
|
| [13] |
Umemoto M, Todaka Y, Tsuchiya K. Mater Trans, 2003; 44: 1488
|
| [14] |
Liu G, Lu J, Lu K. Mater Sci Eng, 2000; A286: 91
|
| [15] |
Xiong T Y, Liu Z W, Li Z C. Mater Rev, 2003; 17: 69
|
| [15] |
(熊天英, 刘志文, 李智超. 材料导报, 2003; 17: 69)
|
| [16] |
Wang T, Wang D P, Liu G, Gong B M, Song N S. Appl Surf Sci, 2008; 255: 1829
|
| [17] |
Mousavi S A A A, Ebrahimi S M, Madoliat R. J Mater Proc Technol, 2007; 187-188: 725
|
| [18] |
Jiang J H, Ding Y, Zuo F Q, Shan A D. Scr Mater, 2009; 60: 905
|
| [19] |
Kim W J, Yoo S J, Jeong H T, Kim D M, Choe B H, Lee J B. Scr Mater, 2011; 64: 49
|
| [20] |
Liu G, Liu J Y, Wang X L, Wang F H, Zhao X, Zuo L. Acta Metall Sin, 2013; 49: 599
|
| [20] |
(刘 刚, 刘金阳, 王小兰, 王福会, 赵 骧, 左 良. 金属学报, 2013; 49: 599)
|
| [21] |
Tao N R, Wang Z B, Tong W P, Sui M L, Lu J, Lu K. Acta Mater, 200; 50: 4603
|
| [22] |
Zhu K Y, Vassel A, Brisset F, Lu K, Lu J. Acta Mater, 2004; 52: 4101
|
| [23] |
Zuo F Q, Jiang J H, Shan A D, Fang J M, Zhang Y X. Trans Nonferrous Met Soc China, 2008; 18: 774
|
| [24] |
Ji Y H, Park J J, Kim W J. Mater Sci Eng, 2007; A454-455: 570
|
| [25] |
Ji Y H, Park J J. Mater Sci Eng, 2008; A485: 299
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|