| 拉拔过程中珠光体钢丝心部的织构演化规律及其对力学性能的影响* |
赵天章1, 宋鸿武1, 张光亮2, 程明1, 张士宏1( ) |
1 中国科学院金属研究所, 沈阳 110016 2 台州学院, 台州 318000 |
|
| THE TEXTURE EVOLUTION AT THE CENTER OF PEARLITIC STEEL WIRE DURING DRAWING AND ITS INFLUENCE ON THE MECHANICAL PROPERTIES |
ZHAO Tianzhang1, SONG Hongwu1, ZHANG Guangliang2, CHENG Ming1, ZHANG Shihong1( ) |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 2 Taizhou University, Taizhou 318000 |
引用本文:
赵天章, 宋鸿武, 张光亮, 程明, 张士宏. 拉拔过程中珠光体钢丝心部的织构演化规律及其对力学性能的影响*[J]. 金属学报, 2014, 50(6): 667-673.
Tianzhang ZHAO,
Hongwu SONG,
Guangliang ZHANG,
Ming CHENG,
Shihong ZHANG.
THE TEXTURE EVOLUTION AT THE CENTER OF PEARLITIC STEEL WIRE DURING DRAWING AND ITS INFLUENCE ON THE MECHANICAL PROPERTIES[J]. Acta Metall Sin, 2014, 50(6): 667-673.
| [1] |
Li Y J, Choi P, Goto S, Borchers C, Raabe D, Kirchheim R. Acta Mater, 2012; 60: 4005
|
| [2] |
Embury J D, Fisher R M. Acta Metall, 1966; 14: 147
|
| [3] |
Langford G. Metall Mater Trans, 1977; 8A: 861
|
| [4] |
Dollar M, Bernstein I M, Thompson A W. Acta Metall, 1988; 36: 311
|
| [5] |
Bae C, Lee C, Nam W. Metall Mater Trans, 2000; 31A: 2665
|
| [6] |
Zhang X, Godfrey A, Huang X, Hansen N, Liu Q. Acta Mater, 2011; 59: 3422
|
| [7] |
Zhang X, Godfrey A, Hansen N, Huang X, Liu W, Liu Q. Mater Charact, 2010; 61: 65
|
| [8] |
Zhang X, Godfrey A, Hansen N, Huang X. Acta Mater, 2013; 61: 4898
|
| [9] |
Li Y J, Choi P, Borchers C, Westerkamp S, Goto S, Raabe D, Kirchheim R. Acta Mater, 2011; 59: 3965
|
| [10] |
Atienza J, Elices M. Mater Struct, 2003; 36: 548
|
| [11] |
Yang F, Jiang J Q, Wang Y, Ma C, Fang F, Zhao K L, Li W. Mater Lett, 2008; 62: 2219
|
| [12] |
Zelin M. Acta Mater, 2002; 50: 4431
|
| [13] |
Yang F, Ma C, Jiang J Q, Feng H P, Zhai S Y. Scr Mater, 2008; 59: 850
|
| [14] |
Liu Y D, Jiang Q W, Zhao X, Zuo L, Liang Z D. Acta Metall Sin, 2002; 38: 1215
|
| [14] |
(刘沿东, 蒋奇武, 赵 骧, 左 良, 梁志德. 金属学报, 2002; 38: 1215)
|
| [15] |
Liu Y D, Zhang Y D, Tidu A, Zuo L. J Mater Sci Technol, 2012; 28: 1010
|
| [16] |
Li S, He S, Van Bael A, Van Houtte P. Mater Sci Forum, 2002; 408-412: 439
|
| [17] |
Zidani M, Messaoudi S, Baudin T, Solas D, Mathon M. Int J Mater Form, 2010; 3: 7
|
| [18] |
Zhang X D, Godfrey A, Liu W, Liu Q. Acta Metall Sin, 2010; 46: 141
|
| [18] |
(张晓丹, Godfrey A, 刘 伟, 刘 庆. 金属学报, 2010; 46: 141)
|
| [19] |
Taylor G I. J Inst Met, 1938; 62: 307
|
| [20] |
Molinari A, Canova G R, Ahzi S. Acta Metall, 1987; 35: 2983
|
| [21] |
Lebensohn R A, Tomé C N. Acta Metall Mater, 1993; 41: 2611
|
| [22] |
Hua F A, Di H S, Li J P, Liu X H, Wang G D. Acta Metall Sin, 2009; 45: 657
|
| [22] |
(花福安, 邸洪双, 李建平, 刘相华, 王国栋. 金属学报, 2009; 45: 657)
|
| [23] |
Li S, Gazder A A, Beyerlein I J, Davies C H J, Pereloma E V. Acta Mater, 2007; 55: 1017
|
| [24] |
Li S Y. Trans Nonferrous Met Soc China, 2013; 23: 170
|
| [25] |
Asaro R,Lubarda V. Mechanics of Solids and Materials. New York: Cambridge University Press, 2006: 538
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|