| 退火时间对超快速加热下热镀锌用TRIP钢组织性能的影响 |
| 侯晓英1),王业勤1),陈蓬2) |
| 1) 山东莱芜钢铁集团有限公司, 莱芜 271104
2) 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819 |
|
| EFFECT OF ANNEALING TIME ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF HOT-DIP GALVANIZED TRIP-AIDED SHEET STEELS UNDER ULTRA RAPID HEATING |
| HOU Xiaoying1), WANG Yeqin1), CHEN Peng2) |
1) Laiwu Iron and Steel Corp., Laiwu 271104
2) State Key Laboratory of Rolling Technology & Automation, Northeast University, Shenyang 110819 |
引用本文:
侯晓英,王业勤,陈蓬. 退火时间对超快速加热下热镀锌用TRIP钢组织性能的影响[J]. 金属学报, 2013, 49(10): 1169-1176.
HOU Xiaoying,
WANG Yeqin,
CHEN Peng.
EFFECT OF ANNEALING TIME ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF HOT-DIP GALVANIZED TRIP-AIDED SHEET STEELS UNDER ULTRA RAPID HEATING[J]. Acta Metall Sin, 2013, 49(10): 1169-1176.
| [1] Yi H L, Lee K Y, Bhadeshia H K D H. Mater Sci Eng, 2011; A528: 5900
[2] Mazzoni-Leduc L, Pardoen T, Massart T J. Eur J Mechanics, 2010; 29A: 132
[3] Ding H, Ding H, Song D, Tang Z Y, Yang P. Mater Sci Eng, 2011; A528: 868
[4] Jimenez-Melero E, Dijk N H, Zhao L, Sietsma J, Offerman S E, Wright J P, Zwaag S.Acta Mater, 2009; 57: 533
[5] Herrera C, Ponge D, Raabe D. Acta Mater, 2011; 59: 4653
[6] Jacques P J, Girault E, Mertens A, Verlinden B, van Humbeeck J, Delannay F.ISIJ Int, 2001; 41: 1068
[7] Hojo T, Sugimoto K I, Mukai Y, Ikeda S. ISIJ Int, 2008; 48: 824
[8] Mahieu J, Maki J, De Cooman B C, Claessens S. Metall Mater Trans, 2002; 33A: 2573
[9] De Cooman B C. Current Opinion Solid State Mater Sci, 2004; 8: 285
[10] Sakuma Y, Matsumura O, Akisue O. ISIJ Int, 1991; 31: 1348
[11] Basuki A, Aernoudt E. Scr Mater, 1999; 40: 1003
[12] Balk S C, Kim S, Jin Y S, Kwon O. ISIJ Int, 2001; 41: 290
[13] Kim S J, Lee C G, Lee T H, Oh C S. ISIJ Int, 2002; 42: 1452
[14] Pereloma E V, Russell K F, Miller M K, Timokhina I B. Scr Mater, 2008; 58: 1078
[15] Pereloma E V, Timokhina I B, Hodgson P D. Mater Sci Eng, 1999; A273-275: 448
[16] Jiao S, Hassani F, Donaberger R L, Essadiqi E, Yue S. ISIJ Int, 2002; 42: 299
[17] Chen H C, Era H, Shimizu M. Metall Trans, 1989; 20A: 437
[18] Lesch C, Alvarez P, Bleck W, Gil Sevillano J. Metall Mater Trans, 2007; 38A: 1882
[19] Salvatori I, Moore W B R. ISIJ Int, 2000; 40(suppl 1): 179
[20] Muljono D, Ferry M, Dunne D P. Mater Sci Eng, 2001; A303: 90
[21] Ray R K, Jonas J J, Hook R E. Int Mater Rev, 1994; 39: 129
[22] Chowdhury S G, Pereloma E V, Santos D B. Mater Sci Eng, 2008; A480: 540
[23] Funakawa Y,Shiozaki T, Tomita K, Yamamoto T, Maeda E. ISIJ Int, 2004; 44: 1945 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|